Complete Set of CAMPUS® Data, ASTM Data, Biopolymer Database, Application Database, Tradename Database, Literature Database, Toolbox.

Material datasheets available free. Online registration at: www.materialdatacenter.com

Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.

This is the free Material Data Center Datasheet of Delrin® 511P NC010 - POM - DuPont Engineering Polymers

Material Data Center offers the following functions for Delrin® 511P NC010:
unit conversion, PDF datasheet print, comparison with other plastics

Check here, which other Delrin datasheets, application examples or technical articles are available in Material Data Center

Use the following short links to get directly to the properties of interest in this datasheet:
Any use of this information falls under the rules of our disclaimer.
Caractéristiques des transformations/physiquesValeurUnitéNorme du test
ASTM Data
Indice de fluidité, MFI 7 g/10min ASTM D 1238
Température 190 °C -
Charge 1.05 kg -
Retrait au moulage , parallèle 0.0165 mm/mm ASTM D 955
Retrait au moulage, perpendiculaire 0.0175 mm/mm ASTM D 955
Propriétés mécaniquesValeurUnitéNorme du test
ASTM Data
Module en traction 3380 MPa ASTM D 638
Module de traction 72 MPa ASTM D 638
Module de traction d’élasticité 72 MPa ASTM D 638
Allongement d’élasticité 11 % ASTM D 638
Allongement à la rupture 33 % ASTM D 638
Module de flexion 3300 MPa ASTM D 790
Izod choc avec entaille, 1/8 in 73 J/m ASTM D 256
Propriétés thermiquesValeurUnitéNorme du test
ASTM Data
UL 94 inflammabilité HB - UL 94
Épaisseur testée 1.5 mm -
coefficient de dilatation thermique, long. 120 E-6/K ASTM D 696
Coefficient de dilatation thermique, trav. 120 E-6/K ASTM D 696
DTUL à 66 psi 169 °C ASTM D 648
DTUL à 264 psi 114 °C ASTM D 648
Température de fusion 178 °C ASTM D 3418
Propriétés électriquesValeurUnitéNorme du test
ASTM Data
Rigidité diélectrique, peu de temps 18 kV/mm ASTM D 149
Facteur de dissipation diélectrique, 1 MHz 0.005 - ASTM D 150
Constante diélectrique, 1 MHz 3.7 - ASTM D 150
Résistance de la surface 3E14 Ohm ASTM D 257
Résistance volumique 7E14 Ohm*cm ASTM D 257
Propriétés diversesValeurUnitéNorme du test
Absorption d’eau, 24hr 0.3 % ASTM D 570
Densité 1420 kg/m³ ASTM D 792
Caractéristiques
Transformation
Moulage par injection, Extrusion de films, Extrusion de tubes, Extrusion de profilés, Extrusion de plaques, Extrusion de cable, Extrusion (autres), Coulage
Conditionnement
Granulés, Couleurs naturelles
Additifs
Lubrifiant, Agent de démoulage
Caractéristiques
Résistance au fluage, Résistance à la fatigue, Bas gauchissement, Stabilité thermique, Soudable, Homopolymère
Applications
Automobile
Disponibilité régionale
Amérique du nord, Europe, Asia Pacific, South and Central America, Proche-Orient/Afrique
Conditions générales
Copyright Altair Engineering GmbH. Altair Engineering GmbH assumes no liability for the system to be free of errors. The user takes sole responsibility for the use of this data under the exclusion of every liability from Altair Engineering GmbH; this is especially valid for claims of compensation resulting from consequential damages. Altair explicitly points out that any decision about the application of materials must be double checked with the producer of this material. This includes all contents of this system. Copyright laws are applicable for the content of this system.
Created: Source: www.materialdatacenter.com


Material Data Center is provided by M-Base Engineering + Software GmbH. M-Base Engineering + Software GmbH assumes no liability for the system to be free of errors. Any decision about the application of materials must be double checked with the producer of this material.

Additional information about this material, like producer contact address, etc. can be found at www.materialdatacenter.com. For access to this extra information a registration is requested. Free online registration is available.