Complete Set of CAMPUS® Data, ASTM Data, Biopolymer Database, Application Database, Tradename Database, Literature Database, Toolbox.

Material datasheets available free. Online registration at: www.materialdatacenter.com

Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.

This is the free Material Data Center Datasheet of Delrin® 311DP NC010 - POM - DuPont Engineering Polymers

Material Data Center offers the following functions for Delrin® 311DP NC010:
unit conversion, PDF datasheet print, comparison with other plastics, snap fit calculation, beam deflection calculation, parameters for material models, CAE Interfaces

Check here, which other Delrin datasheets, application examples or technical articles are available in Material Data Center

Use the following short links to get directly to the properties of interest in this datasheet:
Any use of this information falls under the rules of our disclaimer.
Informations produit
Common features of Delrin® acetal resins include mechanical and physical properties such as high mechanical strength and rigidity, excellent fatigue and impact resistance, as well as resistance to moisture, gasoline, lubricants, solvents, and many other neutral chemicals. Delrin® acetal resins also have excellent dimensional stability and good electrical insulating characteristics. They are naturally resilient, self-lubricating, and available in a variety of colors and speciality grades.

Delrin® acetal resin typically is used in demanding applications in the automotive, domestic appliances, sports, industrial engineering, electronics, and consumer goods industries.

Delrin® 311DP is a medium-high viscosity acetal homopolymer with enhanced crystallization for faster cycle times and excellent creep and fatigue resistance. It has improved thermal stability, excellent dimensional stability, low warpage and fewer voids.
Caractéristiques des transformations/physiquesValeurUnitéNorme du test
ISO Data
Indice de fluidité à chaud en volume, MVR 6 cm³/10min ISO 1133
Température 190 °C -
Charge 2.16 kg -
Retrait au moulage, parallèle 1.9 % ISO 294-4, 2577
Retrait au moulage, perpendiculaire 1.8 % ISO 294-4, 2577
Propriétés mécaniquesValeurUnitéNorme du test
ISO Data
Module en traction 3300 MPa ISO 527
Contrainte d'écoulement 74 MPa ISO 527
Déformation au seuil d'écoulement 15 % ISO 527
Déformation nominale à la rupture 35 % ISO 527
Module de fluage en traction, 1h 2400 MPa ISO 899-1
Module de fluage en traction, 1000h 1200 MPa ISO 899-1
Résistance au choc Charpy, +23°C 300 kJ/m² ISO 179/1eU
Résistance au choc Charpy, -30°C 250 kJ/m² ISO 179/1eU
Résistance au choc Charpy (entaillé), +23°C 9 kJ/m² ISO 179/1eA
Résistance au choc Charpy (entaillé), -30°C 8 kJ/m² ISO 179/1eA
Propriétés thermiquesValeurUnitéNorme du test
ISO Data
Température de fusion, 10°C/min 178 °C ISO 11357-1/-3
Température de fléchissement s/chrg, 1.80 MPa 103 °C ISO 75-1/-2
Température de fléchissement s/chrg, 0.45 MPa 165 °C ISO 75-1/-2
Température de ramolliss. Vicat, B 160 °C ISO 306
Coeffic. de dilatation therm. linéique, parallèle 110 E-6/K ISO 11359-1/-2
Coeffic. de dilatation therm. linéique, perpend. 110 E-6/K ISO 11359-1/-2
Inflammabilité ep. nom. 1.5 mm HB class IEC 60695-11-10
Epaisseur de l'éprouvette 1.5 mm -
Yellow Card disponible oui - -
Inflammabilité pr. épaisseur h HB class IEC 60695-11-10
Epaisseur de l'éprouvette 0.8 mm -
Yellow Card disponible oui - -
Propriétés électriquesValeurUnitéNorme du test
ISO Data
Permittivité relative, 100Hz 3.8 - IEC 62631-2-1
Permittivité relative, 1MHz 3.8 - IEC 62631-2-1
Facteur de pertes, 1MHz 50 E-4 IEC 62631-2-1
Résistivité transversale 1E13 Ohm*m IEC 62631-3-1
Résistivité superficielle >1E15 Ohm IEC 62631-3-2
Propriétés diversesValeurUnitéNorme du test
Absorption d'eau 0.9 % Sim. to ISO 62
Absorption d'humidité 0.2 % Sim. to ISO 62
Masse volumique 1420 kg/m³ ISO 1183
Fonctions
Viscosité / Vitesse de cisaillement , Delrin® 311DP NC010, POM, DuPont
Contrainte de cisaillement / Vit. de cisaillement , Delrin® 311DP NC010, POM, DuPont
Contrainte / Déformation , Delrin® 311DP NC010, POM, DuPont
Module sécant / Déformation , Delrin® 311DP NC010, POM, DuPont
LTHA-Contrainte à la rupture 4mm, Delrin® 311DP NC010, POM, DuPont
LTHA-Déformation à la rupture 4mm, Delrin® 311DP NC010, POM, DuPont
Caractéristiques
Transformation
Moulage par injection, Extrusion de profilés, Extrusion de plaques, Extrusion (autres)
Conditionnement
Granulés, Couleurs naturelles
Additifs
Lubrifiant, Agent de démoulage
Caractéristiques
Homopolymère
Disponibilité régionale
Autres informations
Moulages par injection
Drying is recommended, but not necessary for newly opened packaging stored in a dry location.
Follow the drying guidelines above in the following cases:

·         If moisture is above the Processing Moisture Content recommendation,

·         When a resin container is damaged,

·         When the material is not properly stored in a dry place at room temperature, or

·         When packaging stays open for a significant time.

Résistance Chimique
Acides
Acide acétique (masse en 5%) (23°C)
Acide citrique (masse en 10%) (23°C)
Acide lactique (masse en 10%) (23°C)
Acide chlorhydrique (masse en 36%) (23°C)
Acide nitrique (masse en 40%) (23°C)
Acide sulfurique (masse en 38%) (23°C)
Acide sulfurique (masse en 5%) (23°C)
Acide chromique (masse en 40%) (23°C)
Bases
Hydroxyde de soude (masse en 35%) (23°C)
Hydroxyde de soude (masse en 1%) (23°C)
Hydroxyde d'ammoniaque (masse en 10%) (23°C)
Alcool
Isopropanol (23°C)
Méthanol (23°C)
Ethanol (23°C)
Hydrocarbures
n-Hexane (23°C)
Toluene (23°C)
iso-Octane (23°C)
Cetones
Acetone (23°C)
Ethers
Diethyl ether (23°C)
Huiles minérales
Huile moteur multigrade SAE 10W40 (23°C)
Huile moteur multigrade SAE 10W40 (130°C)
Huile engrenage hypoide SAE 80/90 (130°C)
Huile d'isolation (23°C)
Carburants standards
ISO 1817 Liquide 1 (60°C)
ISO 1817 Liquide 2 (60°C)
ISO 1817 Liquide 3 (60°C)
ISO 1817 Liquide 4 (60°C)
Carburant stand. sans alcool (de pref. ISO 1817 liquide C) (23°C)
Carburant stand. avec alcool (de pref. ISO 1817 Liquid 4) (23°C)
Gasoil (pref. ISO 1817 liquide F) (23°C)
Gasoil (pref. ISO 1817 liquide F) (90°C)
Gasoil (pref. ISO 1817 liquide F) (>90°C)
Selts
Chlorure de sodium (masse en 10%) (23°C)
Hypochlorite de soude (masse en 10%) (23°C)
Carbonate de soude (masse en 20%) (23°C)
Carbonate de soude (masse en 2%) (23°C)
Chlorure de zinc (masse en 50%) (23°C)
Autres
Acétate d'éthyle (23°C)
Peroxyde d'hydrogene (23°C)
Liquide de frein DOT N° 4 (130°C)
Ethylene glycol (108°C)
1% nonylphenoxy-polyethyleneoxy dans l'eau (23°C)
50% Acide oléique + 50% d'huile d'olive (23°C)
L'eau (23°C)
L'eau déionisée (90°C)
Phénol (masse en 5%) (23°C)
Conditions générales
Copyright Altair Engineering GmbH. Altair Engineering GmbH assumes no liability for the system to be free of errors. The user takes sole responsibility for the use of this data under the exclusion of every liability from Altair Engineering GmbH; this is especially valid for claims of compensation resulting from consequential damages. Altair explicitly points out that any decision about the application of materials must be double checked with the producer of this material. This includes all contents of this system. Copyright laws are applicable for the content of this system.
Created: Source: www.materialdatacenter.com


Material Data Center is provided by M-Base Engineering + Software GmbH. M-Base Engineering + Software GmbH assumes no liability for the system to be free of errors. Any decision about the application of materials must be double checked with the producer of this material.

Additional information about this material, like producer contact address, etc. can be found at www.materialdatacenter.com. For access to this extra information a registration is requested. Free online registration is available.