Complete Set of CAMPUS® Data, ASTM Data, Biopolymer Database, Application Database, Tradename Database, Literature Database, Toolbox.

Material datasheets available free. Online registration at: www.materialdatacenter.com

Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.

This is the free Material Data Center Datasheet of ALFATER XL D40I 4GP0000 - TPV - MOCOM Compounds GmbH & Co. KG

Material Data Center offers the following functions for ALFATER XL D40I 4GP0000:
unit conversion, PDF datasheet print, comparison with other plastics

Check here, which other Alfater datasheets, application examples or technical articles are available in Material Data Center

Use the following short links to get directly to the properties of interest in this datasheet:
Any use of this information falls under the rules of our disclaimer.
Informations produit
Base PolymerThermoplastic Vulcanisate (PP+EPDM)
Colournatural color,bright inherent color,black
Service Temperaturemax. range (depending on load, geometry, etc.) -40-125 °C
Special Featureslow emission,good colorability,easy flow,good weathering resistance,good chemical resistance,good ozone reistance,good hot air resistance,good hydrolysis resistant
Market SegmentAutomotive,building and construction,do-it-yourself,electrical and electronic,sport and leisure,Furniture
Application Areainjection moulded parts
Typical Applicationsseals,sealing lip,handles,racking / shelving,impact protection / shock absorber,protection caps,thin walled parts,profile,cable ducts,casters,2K components
Adhesion toPolypropylene Homopolymer,Polypropylene Copolymer,Polyethylene,Thermoplastic Vulcanisate (PP+EPDM),Thermoplastic Olefin Elastomer,Thermoplastic Elastomer general
Propriétés mécaniquesValeurUnitéNorme du test
ISO Data
Résistance à la déchirure 70 kN/m ISO 34-1
Dureté Shore D 40 - ISO 7619-1
Propriétés diversesValeurUnitéNorme du test
Masse volumique 940 kg/m³ ISO 1183
Caractéristiques
Transformation
Moulage par injection
Propriétés spéciales
Stabilisé à la chaleur
Disponibilité régionale
Autres informations
Moulages par injection
Pre-Drying Conditionsin a dry air (dessiccant) dryer 70-80 °C
for 2-4 h
max. moisture content <0,10 %
Processing Injection Mouldingmelt temperature 195-230 °C
mould temperature 10-70 °C
injection speed middle - high
back pressure (hydraulic) >3 bar
holding pressure 50-70% of injection pressure
Storagedry, protected from light
tightly sealed
Conditions générales
Copyright Altair Engineering GmbH. Altair Engineering GmbH assumes no liability for the system to be free of errors. The user takes sole responsibility for the use of this data under the exclusion of every liability from Altair Engineering GmbH; this is especially valid for claims of compensation resulting from consequential damages. Altair explicitly points out that any decision about the application of materials must be double checked with the producer of this material. This includes all contents of this system. Copyright laws are applicable for the content of this system.
Created: Source: www.materialdatacenter.com


Material Data Center is provided by M-Base Engineering + Software GmbH. M-Base Engineering + Software GmbH assumes no liability for the system to be free of errors. Any decision about the application of materials must be double checked with the producer of this material.

Additional information about this material, like producer contact address, etc. can be found at www.materialdatacenter.com. For access to this extra information a registration is requested. Free online registration is available.