Complete Set of CAMPUS® Data, ASTM Data, Biopolymer Database, Application Database, Tradename Database, Literature Database, Toolbox.

Material datasheets available free. Online registration at: www.materialdatacenter.com

Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.

This is the free Material Data Center Datasheet of VESTORAN® 1900 GF20 BK 2.7026 - PPE-GF20 - Evonik Operations GmbH

Material Data Center offers the following functions for VESTORAN® 1900 GF20 BK 2.7026:
unit conversion, PDF datasheet print, comparison with other plastics, snap fit calculation, beam deflection calculation, CAE Interfaces

Check here, which other Vestoran datasheets, application examples or technical articles are available in Material Data Center

Use the following short links to get directly to the properties of interest in this datasheet:
Any use of this information falls under the rules of our disclaimer.
Informations produit
Modified polyphenylene ether (PPE), heat resistant, glass fiber-reinforced, suitable for plastic/rubber composites manufactured by the K K process

VESTORAN® 1900GF20 BK 2.7206  is the registered trademark of Evonik Degussa GmbH for molding compounds containing poly-2,6-dimethyl-1,4-phenylene ether as polymeric constituent (polyphenylene ether, PPE, also referred to as PPO).
As a material of amorphous structure VESTORAN® 1900GF20 shows very small mold shrinkage. Therefore molded parts have a very low tendency to warp.
 
Moldings of VESTORAN® 1900GF20 are dimensionally stable and hydrolysis resistant even in hot water, but are more sensitive to organic solvents than semi-crystalline plastics. VESTORAN® 1900GF20 is resistant to aqueous alkalines and acides, certain alcohols, and glycol solutions.
 
Glass fiber reinforcement of this molding material combines outstanding heat deflection temperature under load with high strength and rigidity.

The even smaller shrinkage compared to non-reinforced VESTORAN® depends on the orientation of the glass fibers in the molded parts.
 
VESTORAN® 1900GF20 is particularly suitable for the adhesion promoter-free manufacturing of plastic/rubber composites by the Evonik Degussa GmbH-patented K&K process ("direct-bonding to rubber").

Compared to VESTORAN® 1900, VESTORAN® 1900GF20 offers higher rigidity and strength.
 
Colored material contains only cadmium-free pigments.
 
VESTORAN® 1900GF20 is supplied as cylindrical granules in polyethylene packaging.
 
Processing advice is given in a separate product information.

Pigmentation may affect values.
 
FOR FURTHER INFORMATION PLEASE CONTACT US AT EVONIK-HP@EVONIK.COM
Caractéristiques des transformations/physiquesValeurUnitéNorme du test
ISO Data
Indice de fluidité à chaud en volume, MVR 24 cm³/10min ISO 1133
Température 300 °C -
Charge 21.6 kg -
Retrait au moulage, parallèle 0.5 % ISO 294-4, 2577
Retrait au moulage, perpendiculaire 0.6 % ISO 294-4, 2577
Propriétés mécaniquesValeurUnitéNorme du test
ISO Data
Module en traction 5800 MPa ISO 527
Contrainte d'écoulement 110 MPa ISO 527
Déformation au seuil d'écoulement 2.8 % ISO 527
Déformation nominale à la rupture 3 % ISO 527
Module de fluage en traction, 1h 5100 MPa ISO 899-1
Module de fluage en traction, 1000h 2300 MPa ISO 899-1
Résistance au choc Charpy, +23°C 50 kJ/m² ISO 179/1eU
Type de défaillance C - -
Résistance au choc Charpy (entaillé), +23°C 12 kJ/m² ISO 179/1eA
Type de défaillance C - -
Résistance au choc en traction, +23°C 260 kJ/m² ISO 8256/1
Propriétés thermiquesValeurUnitéNorme du test
ISO Data
Température de transition vitreuse, 10°C/min 190 °C ISO 11357-1/-2
Température de fléchissement s/chrg, 1.80 MPa 185 °C ISO 75-1/-2
Température de fléchissement s/chrg, 0.45 MPa 190 °C ISO 75-1/-2
Température de ramolliss. Vicat, B 193 °C ISO 306
Coeffic. de dilatation therm. linéique, parallèle 40 E-6/K ISO 11359-1/-2
Coeffic. de dilatation therm. linéique, perpend. 50 E-6/K ISO 11359-1/-2
Inflammabilité ep. nom. 1.5 mm HB class IEC 60695-11-10
Epaisseur de l'éprouvette 1.6 mm -
Inflammabilité pr. épaisseur h HB class IEC 60695-11-10
Epaisseur de l'éprouvette 0.8 mm -
Aptitude à l'allumage 29 % ISO 4589-1/-2
Propriétés électriquesValeurUnitéNorme du test
ISO Data
Permittivité relative, 100Hz 2.9 - IEC 62631-2-1
Permittivité relative, 1MHz 2.7 - IEC 62631-2-1
Facteur de pertes, 100Hz 8 E-4 IEC 62631-2-1
Facteur de pertes, 1MHz 180 E-4 IEC 62631-2-1
Résistivité transversale 1E11 Ohm*m IEC 62631-3-1
Résistivité superficielle 1E13 Ohm IEC 62631-3-2
Indice de résistance au cheminement 175 - IEC 60112
Propriétés diversesValeurUnitéNorme du test
Absorption d'eau 0.35 % Sim. to ISO 62
Masse volumique 1190 kg/m³ ISO 1183
Caractéristiques
Transformation
Moulage par injection, Extrusion de profilés, Extrusion de plaques
Conditionnement
Granulés, Noir
Propriétés spéciales
Stabilisé à la chaleur
Caractéristiques
Amorphe, Bonne adhérence, Bas gauchissement
Résistance Chimique
Résistance aux acides, Résistance aux alcalis , Stabilité hydrolytique
Disponibilité régionale
Conditions générales
Copyright Altair Engineering GmbH. Altair Engineering GmbH assumes no liability for the system to be free of errors. The user takes sole responsibility for the use of this data under the exclusion of every liability from Altair Engineering GmbH; this is especially valid for claims of compensation resulting from consequential damages. Altair explicitly points out that any decision about the application of materials must be double checked with the producer of this material. This includes all contents of this system. Copyright laws are applicable for the content of this system.
Created: Source: www.materialdatacenter.com


Material Data Center is provided by M-Base Engineering + Software GmbH. M-Base Engineering + Software GmbH assumes no liability for the system to be free of errors. Any decision about the application of materials must be double checked with the producer of this material.

Additional information about this material, like producer contact address, etc. can be found at www.materialdatacenter.com. For access to this extra information a registration is requested. Free online registration is available.