Complete Set of CAMPUS® Data, ASTM Data, Biopolymer Database, Application Database, Tradename Database, Literature Database, Toolbox.

Material datasheets available free. Online registration at: www.materialdatacenter.com

Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.

This is the free Material Data Center Datasheet of VESTAMID® DX9321 BK E70164 - PA612-I-GF20 - Evonik Operations GmbH

Material Data Center offers the following functions for VESTAMID® DX9321 BK E70164:
unit conversion, PDF datasheet print, comparison with other plastics, snap fit calculation, beam deflection calculation, CAE Interfaces

Check here, which other Vestamid datasheets, application examples or technical articles are available in Material Data Center

Use the following short links to get directly to the properties of interest in this datasheet:
Any use of this information falls under the rules of our disclaimer.
Informations produit

Molding compound based on nylon 612 specially suitable for plastic and rubber composites

VESTAMID® DX9321 BK E70164 is a heat-stabilized, glass fiber-reinforced and impact-modified PA 612 compound.

The material contains about 20 % glass fibers, an ageing protective agent and processing aid for a fast and even form filling. VESTAMID® DX9321 BK E70164 is especially suitable for the production of plastic and rubber composites.

 

Parts of VESTAMID® DX9321 BK E70164 can be directly bonded to rubber,e.g., XNBR, HNBR, AEM or FPM, without using any adhesives or adhesion promoters ("direct-bonding to rubber").

 

Because of its semi-crystallinemorphology VESTAMID® DX9321 BK E70164 provides an excellent chemical resistance. e.g., against greases, oils, fuels and hydraulic fluids.

Pigmentation may affect values

Inside the original and undamaged packaging, the product has a shelf life of at least 2 years when stored in dry rooms at temperatures not exceeding 30°C.

For information about processing of VESTAMID®, please follow the general commendations about “Processing of VESTAMID® compounds”. 

FOR FURTHER INFORMATION PLEASE CONTACT US AT EVONIK-HP@EVONIK.COM OR VISIT OUR PRODUCT AT  WWW.VESTAMID.COM

Caractéristiques des transformations/physiquessec / condUnitéNorme du test
ISO Data
Indice de fluidité à chaud en volume, MVR 7 / * cm³/10min ISO 1133
Température 230 / * °C -
Charge 5 / * kg -
Retrait au moulage, parallèle 0.7 / * % ISO 294-4, 2577
Retrait au moulage, perpendiculaire 0.9 / * % ISO 294-4, 2577
Propriétés mécaniquessec / condUnitéNorme du test
ISO Data
Module en traction 5700 / 4700 MPa ISO 527
Contrainte d'écoulement * / 90 MPa ISO 527
Déformation au seuil d'écoulement * / 5 % ISO 527
Déformation nominale à la rupture * / 10 % ISO 527
Contrainte à la rupture 115 / * MPa ISO 527
Déformation à la rupture 4.6 / * % ISO 527
Résistance au choc Charpy, +23°C 93 / 93 kJ/m² ISO 179/1eU
Type de défaillance C / C - -
Résistance au choc Charpy, -30°C 106 / 102 kJ/m² ISO 179/1eU
Type de défaillance C / C - -
Résistance au choc Charpy (entaillé), +23°C 18 / 19 kJ/m² ISO 179/1eA
Type de défaillance C / C - -
Résistance au choc Charpy (entaillé), -30°C 11 / 11 kJ/m² ISO 179/1eA
Type de défaillance C / C - -
Propriétés thermiquessec / condUnitéNorme du test
ISO Data
Température de fusion, 10°C/min 215 / * °C ISO 11357-1/-3
Température de fléchissement s/chrg, 1.80 MPa 189 / * °C ISO 75-1/-2
Température de fléchissement s/chrg, 0.45 MPa 208 / * °C ISO 75-1/-2
Température de ramolliss. Vicat, B 207 / * °C ISO 306
Inflammabilité ep. nom. 1.5 mm HB / * class IEC 60695-11-10
Epaisseur de l'éprouvette 1.6 / * mm -
Propriétés électriquessec / condUnitéNorme du test
ISO Data
Permittivité relative, 100Hz 4.4 / - - IEC 62631-2-1
Permittivité relative, 1MHz 3.1 / - - IEC 62631-2-1
Facteur de pertes, 100Hz 500 / - E-4 IEC 62631-2-1
Facteur de pertes, 1MHz 470 / - E-4 IEC 62631-2-1
Résistivité transversale 1E12 / - Ohm*m IEC 62631-3-1
Indice de résistance au cheminement 600 / - - IEC 60112
Propriétés diversessec / condUnitéNorme du test
Absorption d'eau 2 / * % Sim. to ISO 62
Absorption d'humidité 0.8 / * % Sim. to ISO 62
Masse volumique 1190 / 1190 kg/m³ ISO 1183
Caractéristiques
Transformation
Moulage par injection
Conditionnement
Granulés, Noir
Additifs
Agent de démoulage
Propriétés spéciales
Modifié choc, Stabilisé à la lumière, Stabilisé à la chaleur
Caractéristiques
Bonne adhérence
Résistance Chimique
Résistance chimique générale, Résistance aux graisses, Résistance aux huiles
Disponibilité régionale
Conditions générales
Copyright Altair Engineering GmbH. Altair Engineering GmbH assumes no liability for the system to be free of errors. The user takes sole responsibility for the use of this data under the exclusion of every liability from Altair Engineering GmbH; this is especially valid for claims of compensation resulting from consequential damages. Altair explicitly points out that any decision about the application of materials must be double checked with the producer of this material. This includes all contents of this system. Copyright laws are applicable for the content of this system.
Created: Source: www.materialdatacenter.com


Material Data Center is provided by M-Base Engineering + Software GmbH. M-Base Engineering + Software GmbH assumes no liability for the system to be free of errors. Any decision about the application of materials must be double checked with the producer of this material.

Additional information about this material, like producer contact address, etc. can be found at www.materialdatacenter.com. For access to this extra information a registration is requested. Free online registration is available.