Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.

This is the free Material Data Center Datasheet of THERMOLAST® M TM6MED - TPE - KRAIBURG TPE GmbH & Co. KG

Material Data Center offers the following functions for THERMOLAST® M TM6MED:
unit conversion, PDF datasheet print, comparison with other plastics

Check here, which other Thermolast datasheets, application examples or technical articles are available in Material Data Center

Use the following short links to get directly to the properties of interest in this datasheet:
Any use of this information falls under the rules of our disclaimer.
Informations produit
Typical Markets/ Application Sectors:
•    Medical application

Application Examples:
•    Seals
•    Mouthpieces
•    Valves
•    Soft touch
•    Flexible connections
•    Medical tubes

Material Advantage:
•    Applicaton up to indirect blood contact
•    Tested acord. USP Class IV and ISO 10993-5
•    Tested according to ISO 10993-11, ISO 10993- 10, USP 6.6.1
•    Adhesion to PP und HDPE
•    Adapted for injection moulding and extrusion
•    Very good compression set
•    sterilizable (autoclave 134°C, gammaradiation 2x35 kGy, EtO)
Propriétés mécaniquesValeurUnitéNorme du test
ISO Data
Résistance à la traction 11 MPa ISO 37
Déformation à la rupture 750 % ISO 37
Déformation rémanente en compression à 70 °C, 24h 33 % ISO 815
Déformation rémanente en compression à 100 °C, 24h 51 % ISO 815
Résistance à la déchirure 17 kN/m ISO 34-1
Dureté Shore A 56 - ISO 7619-1
Propriétés diversesValeurUnitéNorme du test
Masse volumique 880 kg/m³ ISO 1183
Recommandations pour la transformation Moulage par injectionValeurUnitéNorme du test
Pré-séchage - température 60 - 80 °C -
Pré-séchage - temps 2 - 4 h -
Température de la matière fondue 200 - 250 °C -
Température du moule 25 - 40 °C -
Zone 1 180 - 200 °C -
Zone 2 200 - 220 °C -
Zone 3 220 - 250 °C -
Pressions d'injection 20 - 100 MPa -
Contre-pression 2 - 10 MPa -
Pression de maintien 8 - 60 MPa -
Temps de sejour maximum 10 min -
Caractéristiques
Transformation
Moulage par injection, Extrusion (autres)
Propriétés spéciales
Translucent, Stérilisable, Stérilisation par oxyde d'éthylène (EtO), Stérilisation à la vapeur, Stérilisation par rayonnement gamma
Caractéristiques
Bonne adhérence, Soft Feel, Soudable
Résistance Chimique
Résistance au rayonnement
Certifications
Grade médical, Biocompatibility ISO 10993, USP Class VI approbation, Drug Master File, Long term supply assurance, RoHS, REACH
Applications
Médical
Disponibilité régionale
Amérique du nord, Europe, Asia Pacific
Conditions générales
Copyright Altair Engineering GmbH. Altair Engineering GmbH assumes no liability for the system to be free of errors. The user takes sole responsibility for the use of this data under the exclusion of every liability from Altair Engineering GmbH; this is especially valid for claims of compensation resulting from consequential damages. Altair explicitly points out that any decision about the application of materials must be double checked with the producer of this material. This includes all contents of this system. Copyright laws are applicable for the content of this system.
Created: Source: www.materialdatacenter.com


Material Data Center is provided by M-Base Engineering + Software GmbH. M-Base Engineering + Software GmbH assumes no liability for the system to be free of errors. Any decision about the application of materials must be double checked with the producer of this material.

Additional information about this material, like producer contact address, etc. can be found at www.materialdatacenter.com. For access to this extra information a registration is requested. Free online registration is available.