Caractéristiques des transformations/physiques | Valeur | Unité | Norme du test |
Other Standards[S] |
Indice de fluidité, MFI |
3 |
g/10min |
ASTM D 3307 |
Température |
372 |
°C |
- |
Charge |
5 |
kg |
- |
S: | These properties are reported by the producer according standards that are different to our defaults. |
Propriétés mécaniques | Valeur | Unité | Norme du test |
Other Standards[S] |
Module de traction |
36 |
MPa |
ASTM D 3307 |
S: | These properties are reported by the producer according standards that are different to our defaults. |
Propriétés thermiques | Valeur | Unité | Norme du test |
Other Standards[S] |
Température de fusion |
284 |
°C |
ASTM D 4591 |
S: | These properties are reported by the producer according standards that are different to our defaults. |
Propriétés électriques | Valeur | Unité | Norme du test |
Other Standards[S] |
Résistivité transversale |
0.1 |
Ohm*m |
ISO 3915 |
S: | These properties are reported by the producer according standards that are different to our defaults. |
Propriétés diverses | Valeur | Unité | Norme du test |
Densité |
2150 |
kg/m³ |
ASTM D 792 |
Caractéristiques
Transformation
Extrusion (autres), Soufflage, Moulage par transfert, Moulage par compression
Conditionnement
Granulés
Propriétés spéciales
Antistatique, Stabilisé aux intempéries
Caractéristiques
Résistance au fluage, Tenue de la matière à l’état fondu, Stabilité thermique, Grade tribologique
Résistance Chimique
Résistance chimique générale, Résistance aux solvants
Disponibilité régionale
Amérique du nord, Europe, Asia Pacific, South and Central America
Conditions générales
Copyright Altair Engineering GmbH. Altair Engineering GmbH assumes no liability for the system to be free of errors. The user takes sole responsibility for the use of this data under the exclusion of every liability from Altair Engineering GmbH; this is especially valid for claims of compensation resulting from consequential damages. Altair explicitly points out that any decision about the application of materials must be double checked with the producer of this material. This includes all contents of this system. Copyright laws are applicable for the content of this system.
Created: Source: www.materialdatacenter.com