Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.

This is the free Material Data Center Datasheet of Delrin® 500CPE NC010 - POM - DuPont Engineering Polymers

Material Data Center offers the following functions for Delrin® 500CPE NC010:
unit conversion, PDF datasheet print, comparison with other plastics, snap fit calculation, beam deflection calculation, parameters for material models, CAE Interfaces

Check here, which other Delrin datasheets, application examples or technical articles are available in Material Data Center

Use the following short links to get directly to the properties of interest in this datasheet:
Any use of this information falls under the rules of our disclaimer.
Informations produit
Common features of Delrin® acetal resins include mechanical and physical properties such as high mechanical strength and rigidity, excellent fatigue and impact resistance, as well as resistance to moisture, gasoline, lubricants, solvents, and many other neutral chemicals. Delrin® acetal resins also have excellent dimensional stability and good electrical insulating characteristics. They are naturally resilient, self-lubricating, and available in a variety of colors and speciality grades.

Delrin® acetal resin typically is used in demanding applications in the automotive, domestic appliances, sports, industrial engineering, electronics, and consumer goods industries.


Delrin® 500CPE is a medium viscosity acetal homopolymer with very low VOC emissions for applications in automotive interiors. It provides good mechanical performances with improved processing, thermal stability and productivity for injection molding.
Caractéristiques des transformations/physiquesValeurUnitéNorme du test
ISO Data
Indice de fluidité à chaud en volume, MVR 13 cm³/10min ISO 1133
Température 190 °C -
Charge 2.16 kg -
Retrait au moulage, parallèle 2.0 % ISO 294-4, 2577
Retrait au moulage, perpendiculaire 1.9 % ISO 294-4, 2577
Propriétés mécaniquesValeurUnitéNorme du test
ISO Data
Module en traction 3100 MPa ISO 527
Contrainte d'écoulement 72 MPa ISO 527
Déformation au seuil d'écoulement 16 % ISO 527
Déformation nominale à la rupture 33 % ISO 527
Résistance au choc Charpy, +23°C 250 kJ/m² ISO 179/1eU
Résistance au choc Charpy, -30°C 340 kJ/m² ISO 179/1eU
Résistance au choc Charpy (entaillé), +23°C 10 kJ/m² ISO 179/1eA
Résistance au choc Charpy (entaillé), -30°C 8 kJ/m² ISO 179/1eA
Propriétés thermiquesValeurUnitéNorme du test
ISO Data
Température de fusion, 10°C/min 178 °C ISO 11357-1/-3
Température de fléchissement s/chrg, 1.80 MPa 97 °C ISO 75-1/-2
Inflammabilité ep. nom. 1.5 mm HB class IEC 60695-11-10
Epaisseur de l'éprouvette 1.5 mm -
Yellow Card disponible oui - -
Inflammabilité pr. épaisseur h HB class IEC 60695-11-10
Epaisseur de l'éprouvette 0.8 mm -
Yellow Card disponible oui - -
Propriétés diversesValeurUnitéNorme du test
Masse volumique 1420 kg/m³ ISO 1183
Fonctions
Viscosité / Vitesse de cisaillement , Delrin® 500CPE NC010, POM, DuPont
Contrainte de cisaillement / Vit. de cisaillement , Delrin® 500CPE NC010, POM, DuPont
Contrainte / Déformation , Delrin® 500CPE NC010, POM, DuPont
Module sécant / Déformation , Delrin® 500CPE NC010, POM, DuPont
LTHA-Contrainte à la rupture mm, Delrin® 500CPE NC010, POM, DuPont
LTHA-Déformation à la rupture mm, Delrin® 500CPE NC010, POM, DuPont
Caractéristiques
Transformation
Moulage par injection
Conditionnement
Granulés, Couleurs naturelles
Additifs
Agent de démoulage
Caractéristiques
Low Emission, Stabilité thermique, Homopolymère
Applications
Automobile
Disponibilité régionale
Autres informations
Moulages par injection
Drying is recommended, but not necessary for newly opened packaging stored in a dry location.
Follow the drying guidelines above in the following cases:

·         If moisture is above the Processing Moisture Content recommendation,

·         When a resin container is damaged,

·         When the material is not properly stored in a dry place at room temperature, or

·         When packaging stays open for a significant time.

Conditions générales
Copyright Altair Engineering GmbH. Altair Engineering GmbH assumes no liability for the system to be free of errors. The user takes sole responsibility for the use of this data under the exclusion of every liability from Altair Engineering GmbH; this is especially valid for claims of compensation resulting from consequential damages. Altair explicitly points out that any decision about the application of materials must be double checked with the producer of this material. This includes all contents of this system. Copyright laws are applicable for the content of this system.
Created: Source: www.materialdatacenter.com