Complete Set of CAMPUS® Data, ASTM Data, Biopolymer Database, Application Database, Tradename Database, Literature Database, Toolbox.

Material datasheets available free. Online registration at: www.materialdatacenter.com

Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.

This is the free Material Data Center Datasheet of Apec® 1745 - PC - Covestro Deutschland AG

Material Data Center offers the following functions for Apec® 1745:
unit conversion, PDF datasheet print, comparison with other plastics, application examples, snap fit calculation, beam deflection calculation, parameters for material models, CAE Interfaces

Check here, which other Apec datasheets, application examples or technical articles are available in Material Data Center

Use the following short links to get directly to the properties of interest in this datasheet:
Any use of this information falls under the rules of our disclaimer.
Informations produit
  • MVR (330°C/2.16kg) 17 cm³/10 min
  • easy release
  • suitable for superheated steam sterilisation up to 143 °C as well as for pharmaceutical applications according to United States Pharmacopeia (USP) XXII Class VI
  • softening temperature (VST/B 120)=170 °C
  • Films for medical packaging
  • Contact lens holders
  • Medical vessels
  • Safety valve for respiration aids
  • Syringe tops
Caractéristiques des transformations/physiquesValeurUnitéNorme du test
ISO Data
Indice de fluidité à chaud en volume, MVR 17 cm³/10min ISO 1133
Température 330 °C -
Charge 2.16 kg -
Retrait au moulage, parallèle 0.8 % ISO 294-4, 2577
Retrait au moulage, perpendiculaire 0.8 % ISO 294-4, 2577
Propriétés mécaniquesValeurUnitéNorme du test
ISO Data
Module en traction 2400 MPa ISO 527
Contrainte d'écoulement 70 MPa ISO 527
Déformation au seuil d'écoulement 6.8 % ISO 527
Déformation nominale à la rupture >50 % ISO 527
Résistance au choc Charpy, +23°C N kJ/m² ISO 179/1eU
Résistance au choc Charpy, -30°C N kJ/m² ISO 179/1eU
Propriétés thermiquesValeurUnitéNorme du test
ISO Data
Température de fléchissement s/chrg, 1.80 MPa 148 °C ISO 75-1/-2
Température de fléchissement s/chrg, 0.45 MPa 160 °C ISO 75-1/-2
Coeffic. de dilatation therm. linéique, parallèle 65 E-6/K ISO 11359-1/-2
Coeffic. de dilatation therm. linéique, perpend. 65 E-6/K ISO 11359-1/-2
Inflammabilité ep. nom. 1.5 mm HB class IEC 60695-11-10
Epaisseur de l'éprouvette 1.5 mm -
Aptitude à l'allumage 25 % ISO 4589-1/-2
Propriétés électriquesValeurUnitéNorme du test
ISO Data
Permittivité relative, 100Hz 3 - IEC 62631-2-1
Permittivité relative, 1MHz 2.9 - IEC 62631-2-1
Facteur de pertes, 100Hz 10 E-4 IEC 62631-2-1
Facteur de pertes, 1MHz 80 E-4 IEC 62631-2-1
Résistivité transversale >1E13 Ohm*m IEC 62631-3-1
Résistivité superficielle >1E15 Ohm IEC 62631-3-2
Rigidité diélectrique 35 kV/mm IEC 60243-1
Indice de résistance au cheminement 250 - IEC 60112
Propriétés diversesValeurUnitéNorme du test
Absorption d'eau 0.3 % Sim. to ISO 62
Absorption d'humidité 0.12 % Sim. to ISO 62
Masse volumique 1170 kg/m³ ISO 1183
Préparation et conditionnement des éprouvettesValeurUnitéNorme du test
ISO Data
Injection, température de la matière fondue 330 °C ISO 294
Injection, température du moule 100 °C ISO 294
Injection, vitesse d'injection 200 mm/s ISO 294
Fonctions
Viscosité / Vitesse de cisaillement , Apec® 1745, PC, Covestro
Contrainte de cisaillement / Vit. de cisaillement , Apec® 1745, PC, Covestro
Contrainte / Déformation , Apec® 1745, PC, Covestro
Module sécant / Déformation , Apec® 1745, PC, Covestro
Contrainte / Déformation (isochrone) 23°C, Apec® 1745, PC, Covestro
Module de fluage / Temps 23°C, Apec® 1745, PC, Covestro
Courbe de fluage 23°C, Apec® 1745, PC, Covestro
Contrainte / Déformation (isochrone) 40°C, Apec® 1745, PC, Covestro
Module de fluage / Temps 40°C, Apec® 1745, PC, Covestro
Courbe de fluage 40°C, Apec® 1745, PC, Covestro
Contrainte / Déformation (isochrone) 60°C, Apec® 1745, PC, Covestro
Module de fluage / Temps 60°C, Apec® 1745, PC, Covestro
Courbe de fluage 60°C, Apec® 1745, PC, Covestro
Contrainte / Déformation (isochrone) 90°C, Apec® 1745, PC, Covestro
Module de fluage / Temps 90°C, Apec® 1745, PC, Covestro
Courbe de fluage 90°C, Apec® 1745, PC, Covestro
Contrainte / Déformation (isochrone) 120°C, Apec® 1745, PC, Covestro
Module de fluage / Temps 120°C, Apec® 1745, PC, Covestro
Courbe de fluage 120°C, Apec® 1745, PC, Covestro
Caractéristiques
Transformation
Moulage par injection, Extrusion de films, Extrusion de profilés, Extrusion de plaques
Conditionnement
Granulés
Additifs
Agent de démoulage
Propriétés spéciales
Transparent, Stérilisable, Stérilisation par oxyde d'éthylène (EtO), Stérilisation à la vapeur, Stérilisation par rayonnement gamma
Certifications
Grade médical, USP Class VI approbation
Applications
Médical
Disponibilité régionale
Autres informations
Moulages par injection
PREPROCESSING
Max. Water content: 0.02 %
Drying temperature: 130 °C
Drying time:
Circulating air drying oven (50 % fresh air) 4-12 h
Fresh air dryer (high speed dryer) 2-4 h
Dry air dryer 2-3 h

PROCESSING
Melt temperature: 320-340 °C
Mold temperature: 110-130 °C

Use open nozzle.
Conditions générales
Copyright Altair Engineering GmbH. Altair Engineering GmbH assumes no liability for the system to be free of errors. The user takes sole responsibility for the use of this data under the exclusion of every liability from Altair Engineering GmbH; this is especially valid for claims of compensation resulting from consequential damages. Altair explicitly points out that any decision about the application of materials must be double checked with the producer of this material. This includes all contents of this system. Copyright laws are applicable for the content of this system.
Created: Source: www.materialdatacenter.com


Material Data Center is provided by M-Base Engineering + Software GmbH. M-Base Engineering + Software GmbH assumes no liability for the system to be free of errors. Any decision about the application of materials must be double checked with the producer of this material.

Additional information about this material, like producer contact address, etc. can be found at www.materialdatacenter.com. For access to this extra information a registration is requested. Free online registration is available.