Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.
This is the free Material Data Center Datasheet of SABIC® PP QR674K - PP - Saudi Basic Industries Corporation (SABIC)
Material Data Center offers the following functions for SABIC® PP QR674K:
unit conversion, PDF datasheet print, comparison with other plastics, snap fit calculation, beam deflection calculation, CAE Interfaces
Check here, which other Sabic datasheets, application examples or technical articles are available in Material Data Center
Use the following short links to get directly to the properties of interest in this datasheet:
Any use of this information falls under the rules of our
disclaimer.
Texto del producto
SABIC® PP QR674K is a high melt flow index random copolymer with excellent transparency
and good antistatic properties. This grade combines improved aesthetics of the finished articles with low
temperature processability and a very good organoleptic performance. Part aesthetics are not affected by the
lower processing temperatures, providing for a broader operating window. The SABIC®PP QR674K presents excellent
flow behaviour, easy demoulding and good stiffness to impact ratio.
Application: SABIC® PP QR674K is mainly used in injection moulding processes. The SABIC® PP QR674K
aims at transparent applications were higher MFI’s with good flow are required. Its intended applications
include injection moulded housewares, office & home storage boxes, thin wall packaging, lids and caps &
closures.
Health, Safety and Food Contact regulations:
Material Safety Data Sheets (MSDS) and Product Safety
declarations are available on our Internet site
http://www.SABIC.com.
The product mentioned herein is in particular not tested and therefore not validated for use in
pharmaceutical/medical applications.
IMDS 80775790
Propiedades mecánicas | Valor | Unidades | Método de ensayo |
ISO Data |
Módulo de tracción |
1150 |
MPa |
ISO 527 |
Esfuerzo de fluencia |
29 |
MPa |
ISO 527 |
Alarg. en límite elástico |
13 |
% |
ISO 527 |
Resistencia al impacto Charpy c/entalla, +23°C |
4.5 |
kJ/m² |
ISO 179/1eA |
Dureza Shore D |
64 |
- |
ISO 7619-1 |
Propiedades térmicas | Valor | Unidades | Método de ensayo |
ISO Data |
Estabilidad al calor, 1.80 MPa |
52 |
°C |
ISO 75-1/-2 |
Estabilidad al calor, 0.45 MPa |
75 |
°C |
ISO 75-1/-2 |
Temp. reblandecimiento Vicat, A |
125 |
°C |
ISO 306 |
Temp. reblandecimiento Vicat, B |
70 |
°C |
ISO 306 |
Características
Procesamiento y forma de entrega
Moldeo por inyección
Características especiales
Transparente
Características
Copolímero
Certifications
Contacto con alimentos
Disclaimer
Copyright Altair Engineering GmbH. Altair Engineering GmbH assumes no liability for the system to be free of errors. The user takes sole responsibility for the use of this data under the exclusion of every liability from Altair Engineering GmbH; this is especially valid for claims of compensation resulting from consequential damages. Altair explicitly points out that any decision about the application of materials must be double checked with the producer of this material. This includes all contents of this system. Copyright laws are applicable for the content of this system.
Created: Source: www.materialdatacenter.com
Material Data Center is provided by M-Base Engineering + Software GmbH. M-Base Engineering + Software GmbH assumes no liability for the system to be free of errors. Any decision about the application of materials must be double checked with the producer of this material.
Additional information about this material, like producer contact address, etc. can be found at www.materialdatacenter.com. For access to this extra information a registration is requested. Free online registration is available.