Complete Set of CAMPUS® Data, ASTM Data, Biopolymer Database, Application Database, Tradename Database, Literature Database, Toolbox.

Material datasheets available free. Online registration at: www.materialdatacenter.com

Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.

This is the free Material Data Center Datasheet of SABIC® PC Resin PC1000R - Asia - PC - Saudi Basic Industries Corporation (SABIC)

Material Data Center offers the following functions for SABIC® PC Resin PC1000R - Asia:
unit conversion, PDF datasheet print, comparison with other plastics, snap fit calculation, beam deflection calculation, CAE Interfaces

Check here, which other Sabic datasheets, application examples or technical articles are available in Material Data Center

Use the following short links to get directly to the properties of interest in this datasheet:
Any use of this information falls under the rules of our disclaimer.
Texto del producto
PC1000R resin is a medium-low flow (MFR = 10 at 300?C/1.2kg), heat stabilized, polycarbonate product with mold release designed for use in the general purpose molding market. It is available exclusively at www.sabicpc.com
Caracteristicas de procesamiento y fisicasValorUnidadesMétodo de ensayo
ISO Data
Indice de fluidez volumétrico, MVR 9 cm³/10min ISO 1133
Temperatura 300 °C -
Carga 1.2 kg -
ASTM Data
Índice de fluidez, MFI 10 g/10min ASTM D 1238
Temperatura 300 °C -
Carga 1.2 kg -
Propiedades mecánicasValorUnidadesMétodo de ensayo
ISO Data
Módulo de tracción 2350 MPa ISO 527
Esfuerzo de fluencia 63 MPa ISO 527
Alarg. en límite elástico 6 % ISO 527
Alargamiento a rotura 50 % ISO 527
Modulo de Flexión 2300 MPa ISO 178
Dureza Rockwell R 120 - ISO 2039-2
ASTM Data
Módulo de tracción 2350 MPa ASTM D 638
Esfuerzo de fluencia a tracción 63 MPa ASTM D 638
Alargamiento a la fluencia 6 % ASTM D 638
Alargamiento a la rotura 70 % ASTM D 638
Módulo de flexión 2300 MPa ASTM D 790
Dureza Rockwell R 120 - ASTM D 785
Resistencia al impacto Izod con entalla, 1/8 in 800 J/m ASTM D 256
Resistencia al impacto Izod, 1/8 in N J/m ASTM D 256
Propiedades térmicasValorUnidadesMétodo de ensayo
ISO Data
Estabilidad al calor, 1.80 MPa 127 °C ISO 75-1/-2
Estabilidad al calor, 0.45 MPa 138 °C ISO 75-1/-2
Temp. reblandecimiento Vicat, B 143 °C ISO 306
Combustibilidad a 1.5mm esp. nom. V-2 class IEC 60695-11-10
Espesores de probeta 1.6 mm -
Conductibilidad termica 0.2 W/(m K) DIN 52616
ASTM Data
Estabilidad al calor @ 66 psi 138 °C ASTM D 648
Estabilidad al calor @ 264 psi 127 °C ASTM D 648
Temperatura Vicat 143 °C ASTM D 1525
Conductividad térmica, estado sólido 0.0288 W/(m K) ASTM C 177
Propiedades eléctricasValorUnidadesMétodo de ensayo
ISO Data
Constante dieléctrica, 1MHz 3 - IEC 62631-2-1
Factor de pérdidas dieléctricas, 100Hz 10 E-4 IEC 62631-2-1
Factor de pérdidas dieléctricas, 1MHz 100 E-4 IEC 62631-2-1
Resistividad volumétrica específica >1E13 Ohm*m IEC 62631-3-1
Resistencia dieléctrica 27 kV/mm IEC 60243-1
ASTM Data
Resistencia dieléctrica, tiempo corto 27 kV/mm ASTM D 149
Factor de pérdidas dieléctricas, 60 Hz 0.001 - ASTM D 150
Factor de pérdidas dieléctricas, 1 MHz 0.01 - ASTM D 150
Constante dieléctrica, 60 Hz 3 - ASTM D 150
Constante dieléctrica, 1 MHz 3 - ASTM D 150
Resistividad volumétrica 1E15 Ohm*cm ASTM D 257
Propiedades opticasValorUnidadesMétodo de ensayo
ASTM Data
Opacidad 0.8 % ASTM D 1003
Transmitancia luminosa 90 % ASTM D 1003
Índice de refracción 1.59 - ASTM D 542
Otras propiedadesValorUnidadesMétodo de ensayo
Absorción de agua 0.35 % Sim. to ISO 62
Densidad 1200 kg/m³ ISO 1183
Absorción de agua, equilibrio 0.35 % ASTM D 570
Densidad 1200 kg/m³ ASTM D 792
Recomendación para procesamiento Moldeo por inyecciónValorUnidadesMétodo de ensayo
Temperatura de pre-secado ≤120 °C -
Tiempo de pre-secado 2 - 4 h -
Temperatura de la masa 280 - 310 °C -
Temperatura del molde 80 - 110 °C -
Zona 1 260 - 280 °C -
Zona 2 270 - 290 °C -
Zona 3 280 - 310 °C -
Temperatura de boquilla 270 - 290 °C -
Características
Características especiales
Estable contra el calor
Disclaimer
Copyright Altair Engineering GmbH. Altair Engineering GmbH assumes no liability for the system to be free of errors. The user takes sole responsibility for the use of this data under the exclusion of every liability from Altair Engineering GmbH; this is especially valid for claims of compensation resulting from consequential damages. Altair explicitly points out that any decision about the application of materials must be double checked with the producer of this material. This includes all contents of this system. Copyright laws are applicable for the content of this system.
Created: Source: www.materialdatacenter.com


Material Data Center is provided by M-Base Engineering + Software GmbH. M-Base Engineering + Software GmbH assumes no liability for the system to be free of errors. Any decision about the application of materials must be double checked with the producer of this material.

Additional information about this material, like producer contact address, etc. can be found at www.materialdatacenter.com. For access to this extra information a registration is requested. Free online registration is available.