Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.

This is the free Material Data Center Datasheet of SABIC® LLDPE 118NE - (PE-LLD) - Saudi Basic Industries Corporation (SABIC)

Material Data Center offers the following functions for SABIC® LLDPE 118NE:
unit conversion, PDF datasheet print, comparison with other plastics

Check here, which other Sabic datasheets, application examples or technical articles are available in Material Data Center

Use the following short links to get directly to the properties of interest in this datasheet:
Any use of this information falls under the rules of our disclaimer.
Texto del producto
SABIC® LLDPE 118NE is a butene linear low density polyethylene resin typically used for general purposeapplications. Films produced from this resin are tough with good puncture resistance, high tensile strength, good hottack properties and low gel levels. Application Typical applications for SABIC® LLDPE 118NE are shipping sacks, ice bags, frozen food bags, liners, carrier bags, garbage bags, agriculture films, lamination and coextruded films, shrink film (for blending with LDPE), industrial consumer packaging and high clarity film if blended with (10-20%) LDPE. Film properties Film of 50 ?m and BUR=2 has been produced on Kiefel IBC with 140 kg/h. Die size 200 mm, die gap 2,7 mm. This product is not intended for and must not be used in any pharmaceutical/medical applications.
Propiedades térmicasValorUnidadesMétodo de ensayo
ISO Data
Temp. reblandecimiento Vicat, A 103 °C ISO 306
Propiedades opticasValorUnidadesMétodo de ensayo
ASTM Data
Opacidad 13 % ASTM D 1003
Propiedades mecánicas (Film)ValorUnidadesMétodo de ensayo
ISO Data
Módulo de tracción, paralelo 190 MPa ISO 527-3
Módulo de tracción, normal 210 MPa ISO 527-3
Tensión a fluencia, paralelo 11 MPa ISO 527-3
Tensión a fluencia, normal 12 MPa ISO 527-3
Resistencia a la tracción, paralelo 44 MPa ISO 527-3
Resistencia a la tracción, normal 33 MPa ISO 527-3
Resistencia al desgarro Trouser, parallel 40 N/mm ISO 6383-1
Resistencia al desgarro Trouser, normal 140 N/mm ISO 6383-1
Disclaimer
Copyright Altair Engineering GmbH. Altair Engineering GmbH assumes no liability for the system to be free of errors. The user takes sole responsibility for the use of this data under the exclusion of every liability from Altair Engineering GmbH; this is especially valid for claims of compensation resulting from consequential damages. Altair explicitly points out that any decision about the application of materials must be double checked with the producer of this material. This includes all contents of this system. Copyright laws are applicable for the content of this system.
Created: Source: www.materialdatacenter.com