Complete Set of CAMPUS® Data, ASTM Data, Biopolymer Database, Application Database, Tradename Database, Literature Database, Toolbox.

Material datasheets available free. Online registration at: www.materialdatacenter.com

Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.

This is the free Material Data Center Datasheet of Makrolon® FR6005 - PC FR - Covestro Deutschland AG

Material Data Center offers the following functions for Makrolon® FR6005:
unit conversion, PDF datasheet print, comparison with other plastics, snap fit calculation, beam deflection calculation, CAE Interfaces

Check here, which other Makrolon datasheets, application examples or technical articles are available in Material Data Center

Use the following short links to get directly to the properties of interest in this datasheet:
Any use of this information falls under the rules of our disclaimer.
Texto del producto
  • MVR (300 °C/1.2 kg) 9.0 cm³/10 min
  • medium viscosity
  • easy release
  • flame retardant
  • impact modified
  • good surface quality
  • electrical/electronic
  • housing parts
Caracteristicas de procesamiento y fisicasValorUnidadesMétodo de ensayo
ISO Data
Indice de fluidez volumétrico, MVR 9 cm³/10min ISO 1133
Temperatura 300 °C -
Carga 1.2 kg -
Contracción posterior al moldeo, paralelo 0.7 % ISO 294-4, 2577
Contracción posterior al moldeo, normal 0.7 % ISO 294-4, 2577
Propiedades mecánicasValorUnidadesMétodo de ensayo
ISO Data
Módulo de tracción 2300 MPa ISO 527
Esfuerzo de fluencia 62 MPa ISO 527
Alarg. en límite elástico 6 % ISO 527
Alarg. nominal a rotura >50 % ISO 527
Módulo de flexión, 23°C 2400 MPa ISO 178
Resistencia a la flexión 90 MPa ISO 178
Resistencia al impacto Charpy c/entalla, +23°C 68 kJ/m² ISO 179/1eA
Type of failure P - -
Resistencia al impacto Charpy c/entalla, -30°C 20 kJ/m² ISO 179/1eA
Type of failure C - -
Resistencia al impacto Izod con entalla, +23°C 60 kJ/m² ISO 180/1A
Resistencia al impacto Izod con entalla 15 kJ/m² ISO 180/1A
Temperatura -30 °C -
Perforación - máxima fuerza, +23°C 5100 N ISO 6603-2
Perforación - máxima fuerza, -30°C 6100 N ISO 6603-2
Perforación - energía, +23°C 54 J ISO 6603-2
Perforación - energía, -30°C 55 J ISO 6603-2
Propiedades térmicasValorUnidadesMétodo de ensayo
ISO Data
Estabilidad al calor, 1.80 MPa 121 °C ISO 75-1/-2
Estabilidad al calor, 0.45 MPa 136 °C ISO 75-1/-2
Temp. reblandecimiento Vicat, B 142 °C ISO 306
Coef.de expansión térmica lineal, paralelo 70 E-6/K ISO 11359-1/-2
Coef.de expansión térmica lineal, normal 70 E-6/K ISO 11359-1/-2
Combustibilidad a 1.5mm esp. nom. V-0 class IEC 60695-11-10
Espesores de probeta 1.5 mm -
Yellow Card disponible - -
Combustibilidad a espesor h V-0 class IEC 60695-11-10
Espesores de probeta 1.0 mm -
Yellow Card disponible - -
Glow Wire Flammability Index (GWFI) 850 °C IEC 60695-2-12
GWFI - thickness tested (1) 1 mm -
Glow Wire Flammability Index (GWFI) 960 °C IEC 60695-2-12
GWFI - thickness tested (2) 1.5 mm -
Glow Wire Flammability Index (GWFI) 960 °C IEC 60695-2-12
GWFI - thickness tested (3) 3 mm -
Glow Wire Ignition Temperature (GWIT) 875 °C IEC 60695-2-13
GWIT - thickness tested (1) 1 mm -
Glow Wire Ignition Temperature (GWIT) 850 °C IEC 60695-2-13
GWIT - thickness tested (2) 1.5 mm -
Glow Wire Ignition Temperature (GWIT) 900 °C IEC 60695-2-13
GWIT - thickness tested (3) 3 mm -
Propiedades eléctricasValorUnidadesMétodo de ensayo
ISO Data
Resistividad volumétrica específica >1E13 Ohm*m IEC 62631-3-1
Resistividad superficial específica >1E15 Ohm IEC 62631-3-2
Indice comparativo de linea de fuga 200 - IEC 60112
Otras propiedadesValorUnidadesMétodo de ensayo
Densidad 1200 kg/m³ ISO 1183
Condiciones de transformaciónValorUnidadesMétodo de ensayo
ISO Data
Moldeo por inyección, temperatura de la masa 300 °C ISO 294
Moldeo por inyección, temperatura del molde 80 °C ISO 294
Moldeo por inyección, velocidad de inyección 200 mm/s ISO 294
Recomendación para procesamiento Moldeo por inyecciónValorUnidadesMétodo de ensayo
Temperatura de pre-secado 120 °C -
Tiempo de pre-secado 2 - 3 h -
Humedad de procesamiento ≤0.02 % -
Temperatura de la masa 280 - 320 °C -
Temperatura del molde 80 - 120 °C -
Zona 1 250 - 260 °C -
Zona 2 270 - 280 °C -
Zona 3 280 - 290 °C -
Temperatura de boquilla 290 - 300 °C -
Contrapresión 5 - 15 MPa -
Características
Procesamiento y forma de entrega
Moldeo por inyección
Forma de suministro
Negro
Aditivos
Desmoldeante
Características especiales
Resistencia mejorada al fuego, Alto impacto o modificado al impacto, Transparente
Applicaciones
Electrica, Encapsulacion
Disponibilidad regional
Norteamérica, Europa, Asia Pacifico, América del Sur y Centroaméric, Próximo Oriente/Africa
Disclaimer
Copyright Altair Engineering GmbH. Altair Engineering GmbH assumes no liability for the system to be free of errors. The user takes sole responsibility for the use of this data under the exclusion of every liability from Altair Engineering GmbH; this is especially valid for claims of compensation resulting from consequential damages. Altair explicitly points out that any decision about the application of materials must be double checked with the producer of this material. This includes all contents of this system. Copyright laws are applicable for the content of this system.
Created: Source: www.materialdatacenter.com


Material Data Center is provided by M-Base Engineering + Software GmbH. M-Base Engineering + Software GmbH assumes no liability for the system to be free of errors. Any decision about the application of materials must be double checked with the producer of this material.

Additional information about this material, like producer contact address, etc. can be found at www.materialdatacenter.com. For access to this extra information a registration is requested. Free online registration is available.