Complete Set of CAMPUS® Data, ASTM Data, Biopolymer Database, Application Database, Tradename Database, Literature Database, Toolbox.

Material datasheets available free. Online registration at: www.materialdatacenter.com

Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.

This is the free Material Data Center Datasheet of LEXAN™ Copolymer ML6411 - Europe - PC - Saudi Basic Industries Corporation (SABIC)

Material Data Center offers the following functions for LEXAN™ Copolymer ML6411 - Europe:
unit conversion, PDF datasheet print, comparison with other plastics, snap fit calculation, beam deflection calculation, CAE Interfaces

Check here, which other Lexan datasheets, application examples or technical articles are available in Material Data Center

Use the following short links to get directly to the properties of interest in this datasheet:
Any use of this information falls under the rules of our disclaimer.
Texto del producto
LEXAN ML6411 polycarbonate (PC) siloxane resin, is a high flow opaque injection molding (IM) grade with very low temperature ductility characteristics. This grade offers UL94 V0 @ 1.5mm and 5VA @ 3.0mm flame retardancy based on non-chlorine, non-bromine FR systems. LEXAN ML6411 resin offers excellent processing characteristics with opportunity for shorter IM cycle times compared to standard PC. This product is available in a wide range of opaque colors and is an excellent candidate for a wide range of electrical applications.

UL Yellow Card Link E45329-100058759
Caracteristicas de procesamiento y fisicasValorUnidadesMétodo de ensayo
ISO Data
Indice de fluidez volumétrico, MVR 18 cm³/10min ISO 1133
Temperatura 260 °C -
Carga 5 kg -
ASTM Data
Índice de fluidez, MFI 15 g/10min ASTM D 1238
Temperatura 300 °C -
Carga 1.2 kg -
Propiedades mecánicasValorUnidadesMétodo de ensayo
ISO Data
Módulo de tracción 2350 MPa ISO 527
Esfuerzo de fluencia 62 MPa ISO 527
Alarg. en límite elástico 5 % ISO 527
Resistencia a la tracción 58 MPa ISO 527
Alargamiento a rotura 50 % ISO 527
Modulo de Flexión 2350 MPa ISO 178
. impacto Izod c/entalla, +23°C, 3mm 60 kJ/m² ISO 180/1A
Res. impacto Izod c/entalla, -30°C, 3mm 15 kJ/m² ISO 180/1A
ASTM Data
Módulo de tracción 2500 MPa ASTM D 638
Esfuerzo de fluencia a tracción 62 MPa ASTM D 638
Esfuerzo de fractura a tracción 54 MPa ASTM D 638
Alargamiento a la fluencia 5 % ASTM D 638
Alargamiento a la rotura 100 % ASTM D 638
Módulo de flexión 2600 MPa ASTM D 790
Resistencia al impacto Izod con entalla, 1/8 in 900 J/m ASTM D 256
Resistencia al impacto Izod con entalla, baja temperatura 150 J/m ASTM D 256
Temperatura -30 °C -
Propiedades térmicasValorUnidadesMétodo de ensayo
ISO Data
Temp. reblandecimiento Vicat, B 134 °C ISO 306
Temp. reblandecimiento Vicat, 120°C/h 50N 135 °C ISO 306
Combustibilidad a 1.5mm esp. nom. V-0 class IEC 60695-11-10
Espesores de probeta 1.5 mm -
Combustibilidad a espesor h V-2 class IEC 60695-11-10
Espesores de probeta 0.8 mm -
Combustibilidad 5V a espesor h 5VB class IEC 60695-11-20
Espesores de probeta 1.7 mm -
Glow Wire Flammability Index (GWFI) 960 °C IEC 60695-2-12
Glow Wire Flammability Index (GWFI) 960 °C IEC 60695-2-12
Glow Wire Flammability Index (GWFI) 960 °C IEC 60695-2-12
Glow Wire Ignition Temperature (GWIT) 800 °C IEC 60695-2-13
GWIT - thickness tested (1) 1 mm -
Glow Wire Ignition Temperature (GWIT) 800 °C IEC 60695-2-13
GWIT - thickness tested (2) 2 mm -
Glow Wire Ignition Temperature (GWIT) 800 °C IEC 60695-2-13
GWIT - thickness tested (3) 3 mm -
ASTM Data
Estabilidad al calor @ 264 psi 114 °C ASTM D 648
Temperatura Vicat 134 °C ASTM D 1525
Propiedades eléctricasValorUnidadesMétodo de ensayo
ISO Data
Resistividad volumétrica específica >1E13 Ohm*m IEC 62631-3-1
Indice comparativo de linea de fuga 250 - IEC 60112
ASTM Data
Resistencia dieléctrica, tiempo corto 26.5 kV/mm ASTM D 149
Otras propiedadesValorUnidadesMétodo de ensayo
Absorción de agua 0.3 % Sim. to ISO 62
Absorción de humedad 0.1 % Sim. to ISO 62
Densidad 1200 kg/m³ ISO 1183
Densidad 1190 kg/m³ ASTM D 792
Recomendación para procesamiento Moldeo por inyecciónValorUnidadesMétodo de ensayo
Temperatura de pre-secado 90 - 100 °C -
Tiempo de pre-secado 2 - 4 h -
Humedad de procesamiento ≤0.02 % -
Temperatura de la masa 270 - 300 °C -
Temperatura del molde 60 - 90 °C -
Temperatura - zona de alimentación 60 - 80 °C -
Zona 1 230 - 260 °C -
Zona 2 250 - 290 °C -
Zona 3 260 - 300 °C -
Características
Procesamiento y forma de entrega
Moldeo por inyección
Aditivos
Ignifugante
Características especiales
Resistencia mejorada al fuego
Disponibilidad regional
Europa
Disclaimer
Copyright Altair Engineering GmbH. Altair Engineering GmbH assumes no liability for the system to be free of errors. The user takes sole responsibility for the use of this data under the exclusion of every liability from Altair Engineering GmbH; this is especially valid for claims of compensation resulting from consequential damages. Altair explicitly points out that any decision about the application of materials must be double checked with the producer of this material. This includes all contents of this system. Copyright laws are applicable for the content of this system.
Created: Source: www.materialdatacenter.com


Material Data Center is provided by M-Base Engineering + Software GmbH. M-Base Engineering + Software GmbH assumes no liability for the system to be free of errors. Any decision about the application of materials must be double checked with the producer of this material.