Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.

This is the free Material Data Center Datasheet of LEXAN™ Copolymer EXL9414T - Europe - PC - Saudi Basic Industries Corporation (SABIC)

Material Data Center offers the following functions for LEXAN™ Copolymer EXL9414T - Europe:
unit conversion, PDF datasheet print, comparison with other plastics, snap fit calculation, beam deflection calculation, CAE Interfaces

Check here, which other Lexan datasheets, application examples or technical articles are available in Material Data Center

Use the following short links to get directly to the properties of interest in this datasheet:
Any use of this information falls under the rules of our disclaimer.
Texto del producto
LEXAN EXL9414T resin grade is a halogen-free flame retardant polycarbonate featuring transparency, -40 degree C ductility and UL-94 V0 rating for injection molding applications. Excellent impact combined with good flow, all transparent colorability for aesthetics and thin wall flame retradancy makes this product an excellent candidate for thin wall applications.

UL Yellow Card Link E207780-100120434
Caracteristicas de procesamiento y fisicasValorUnidadesMétodo de ensayo
ISO Data
Indice de fluidez volumétrico, MVR 12 cm³/10min ISO 1133
Temperatura 300 °C -
Carga 1.2 kg -
ASTM Data
Índice de fluidez, MFI 13 g/10min ASTM D 1238
Temperatura 300 °C -
Carga 1.2 kg -
Propiedades mecánicasValorUnidadesMétodo de ensayo
ISO Data
Módulo de tracción 2300 MPa ISO 527
Esfuerzo de fluencia 56 MPa ISO 527
Alarg. en límite elástico 5.4 % ISO 527
Resistencia a la tracción 55 MPa ISO 527
Alargamiento a rotura 50 % ISO 527
Modulo de Flexión 2120 MPa ISO 178
Resistencia al impacto Charpy, +23°C, 3mm N kJ/m² ISO 179/1eU
Resistencia al impacto Charpy, -30°C, 3mm N kJ/m² ISO 179/1eU
Resistencia al impacto Charpy c/entalla, +23°C, 3mm 70 kJ/m² ISO 179/1eA
Resistencia al impacto Charpy c/entalla, -30°C, 3mm 60 kJ/m² ISO 179/1eA
Resistencia al impacto Izod, +23°C N kJ/m² ISO 180/1U
. impacto Izod c/entalla, +23°C, 3mm 65 kJ/m² ISO 180/1A
Res. impacto Izod c/entalla, -30°C, 3mm 55 kJ/m² ISO 180/1A
ASTM Data
Módulo de tracción 2180 MPa ASTM D 638
Esfuerzo de fluencia a tracción 57 MPa ASTM D 638
Esfuerzo de fractura a tracción 59 MPa ASTM D 638
Alargamiento a la fluencia 5.6 % ASTM D 638
Alargamiento a la rotura 124 % ASTM D 638
Módulo de flexión 2180 MPa ASTM D 790
Resistencia al impacto Izod con entalla, 1/8 in 824 J/m ASTM D 256
Resistencia al impacto Izod con entalla, baja temperatura 712 J/m ASTM D 256
Temperatura -30 °C -
Propiedades térmicasValorUnidadesMétodo de ensayo
ISO Data
Estabilidad al calor, 1.80 MPa 116 °C ISO 75-1/-2
Temp. reblandecimiento Vicat, B 138 °C ISO 306
Temp. reblandecimiento Vicat, 120°C/h 50N 139 °C ISO 306
Combustibilidad a 1.5mm esp. nom. V-1 class IEC 60695-11-10
Espesores de probeta 1.5 mm -
Combustibilidad a espesor h V-2 class IEC 60695-11-10
Espesores de probeta 1.2 mm -
Glow Wire Flammability Index (GWFI) 930 °C IEC 60695-2-12
Glow Wire Flammability Index (GWFI) 960 °C IEC 60695-2-12
Glow Wire Flammability Index (GWFI) 960 °C IEC 60695-2-12
Glow Wire Ignition Temperature (GWIT) 875 °C IEC 60695-2-13
GWIT - thickness tested (1) 1 mm -
Glow Wire Ignition Temperature (GWIT) 850 °C IEC 60695-2-13
GWIT - thickness tested (2) 2 mm -
Glow Wire Ignition Temperature (GWIT) 850 °C IEC 60695-2-13
GWIT - thickness tested (3) 3 mm -
ASTM Data
Estabilidad al calor @ 264 psi 120 °C ASTM D 648
Temperatura Vicat 138 °C ASTM D 1525
Otras propiedadesValorUnidadesMétodo de ensayo
Absorción de agua 0.12 % Sim. to ISO 62
Absorción de humedad 0.09 % Sim. to ISO 62
Densidad 1190 kg/m³ ISO 1183
Densidad 1190 kg/m³ ASTM D 792
Recomendación para procesamiento Moldeo por inyecciónValorUnidadesMétodo de ensayo
Temperatura de pre-secado 120 °C -
Tiempo de pre-secado 3 - 4 h -
Humedad de procesamiento ≤0.02 % -
Temperatura de la masa 295 - 315 °C -
Temperatura del molde 70 - 95 °C -
Zona 1 270 - 295 °C -
Zona 2 280 - 305 °C -
Zona 3 295 - 315 °C -
Velocidad de giro de husillo 40 - 70 rpm -
Contrapresión 0.3 - 0.7 MPa -
Características
Procesamiento y forma de entrega
Moldeo por inyección
Aditivos
Ignifugante
Características especiales
Resistencia mejorada al fuego, Transparente
Disponibilidad regional
Europa
Disclaimer
Copyright Altair Engineering GmbH. Altair Engineering GmbH assumes no liability for the system to be free of errors. The user takes sole responsibility for the use of this data under the exclusion of every liability from Altair Engineering GmbH; this is especially valid for claims of compensation resulting from consequential damages. Altair explicitly points out that any decision about the application of materials must be double checked with the producer of this material. This includes all contents of this system. Copyright laws are applicable for the content of this system.
Created: Source: www.materialdatacenter.com