Complete Set of CAMPUS® Data, ASTM Data, Biopolymer Database, Application Database, Tradename Database, Literature Database, Toolbox.

Material datasheets available free. Online registration at: www.materialdatacenter.com

Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.

This is the free Material Data Center Datasheet of LEXAN™ Copolymer DMX1435 - Asia - PC - Saudi Basic Industries Corporation (SABIC)

Material Data Center offers the following functions for LEXAN™ Copolymer DMX1435 - Asia:
unit conversion, PDF datasheet print, comparison with other plastics, snap fit calculation, beam deflection calculation, CAE Interfaces

Check here, which other Lexan datasheets, application examples or technical articles are available in Material Data Center

Use the following short links to get directly to the properties of interest in this datasheet:
Any use of this information falls under the rules of our disclaimer.
Texto del producto
LEXAN™ DMX1435 is a UV stabilized standard flow polycarbonate copolymer resin with improved scratch resistance, improved dielectric performance (lower Df). It is both transparency and colorable available solutions to the applications such as 5G related devices, anti-scratch covers, etc.
Caracteristicas de procesamiento y fisicasValorUnidadesMétodo de ensayo
ISO Data
Indice de fluidez volumétrico, MVR 13 cm³/10min ISO 1133
Temperatura 300 °C -
Carga 1.2 kg -
ASTM Data
Índice de fluidez, MFI 14.5 g/10min ASTM D 1238
Temperatura 300 °C -
Carga 1.2 kg -
Propiedades mecánicasValorUnidadesMétodo de ensayo
ISO Data
Módulo de tracción 2450 MPa ISO 527
Esfuerzo de fluencia 80 MPa ISO 527
Alarg. en límite elástico 7 % ISO 527
Resistencia a la tracción 60 MPa ISO 527
Alargamiento a rotura 40 % ISO 527
Modulo de Flexión 2450 MPa ISO 178
Resistencia al impacto Charpy, +23°C, 3mm N kJ/m² ISO 179/1eU
Resistencia al impacto Charpy, -30°C, 3mm 47 kJ/m² ISO 179/1eU
Resistencia al impacto Charpy c/entalla, +23°C, 3mm 3 kJ/m² ISO 179/1eA
Resistencia al impacto Charpy c/entalla, -30°C, 3mm 3 kJ/m² ISO 179/1eA
Resistencia al impacto Izod, +23°C N kJ/m² ISO 180/1U
. impacto Izod c/entalla, +23°C, 3mm 5 kJ/m² ISO 180/1A
Res. impacto Izod c/entalla, -30°C, 3mm 4 kJ/m² ISO 180/1A
Ball indentation hardness 128 MPa ISO 2039-1
ASTM Data
Módulo de tracción 2563 MPa ASTM D 638
Esfuerzo de fluencia a tracción 80 MPa ASTM D 638
Esfuerzo de fractura a tracción 65 MPa ASTM D 638
Alargamiento a la fluencia 7 % ASTM D 638
Alargamiento a la rotura 70 % ASTM D 638
Módulo de flexión 2469 MPa ASTM D 790
Dureza Rockwell M 93 - ASTM D 785
Resistencia a la abrasión (Taber) 10 mg/1000 cycles ASTM D 1044
Resistencia al impacto Izod con entalla, 1/8 in 30 J/m ASTM D 256
Resistencia al impacto Izod con entalla, baja temperatura 30 J/m ASTM D 256
Temperatura -30 °C -
Resistencia al impacto Izod, 1/8 in N J/m ASTM D 256
Propiedades térmicasValorUnidadesMétodo de ensayo
ISO Data
Estabilidad al calor, 1.80 MPa 118 °C ISO 75-1/-2
Estabilidad al calor, 0.45 MPa 131 °C ISO 75-1/-2
Temp. reblandecimiento Vicat, B 138 °C ISO 306
Temp. reblandecimiento Vicat, 120°C/h 50N 140 °C ISO 306
Combustibilidad a espesor h HB class IEC 60695-11-10
Espesores de probeta 0.6 mm -
Conductibilidad termica 0.2 W/(m K) DIN 52616
Glow Wire Flammability Index (GWFI) 900 °C IEC 60695-2-12
Glow Wire Flammability Index (GWFI) 960 °C IEC 60695-2-12
Glow Wire Flammability Index (GWFI) 960 °C IEC 60695-2-12
Glow Wire Ignition Temperature (GWIT) 850 °C IEC 60695-2-13
GWIT - thickness tested (1) 1 mm -
Glow Wire Ignition Temperature (GWIT) 825 °C IEC 60695-2-13
GWIT - thickness tested (2) 2 mm -
Glow Wire Ignition Temperature (GWIT) 825 °C IEC 60695-2-13
GWIT - thickness tested (3) 3 mm -
ASTM Data
Estabilidad al calor @ 66 psi 133 °C ASTM D 648
Estabilidad al calor @ 264 psi 119 °C ASTM D 648
Temperatura Vicat 139 °C ASTM D 1525
Conductividad térmica, estado sólido 0.0288 W/(m K) ASTM C 177
Calor específico 1400 J/(kg K) ASTM C 351
Otras propiedadesValorUnidadesMétodo de ensayo
Absorción de agua 0.27 % Sim. to ISO 62
Absorción de humedad 0.13 % Sim. to ISO 62
Densidad 1170 kg/m³ ISO 1183
Absorción de agua, 24hr 0.04 % ASTM D 570
Densidad 1200 kg/m³ ASTM D 792
Recomendación para procesamiento Moldeo por inyecciónValorUnidadesMétodo de ensayo
Temperatura de pre-secado 120 °C -
Tiempo de pre-secado 3 - 4 h -
Humedad de procesamiento ≤0.02 % -
Temperatura de la masa 295 - 315 °C -
Temperatura del molde 70 - 95 °C -
Temperatura - zona de alimentación 60 - 80 °C -
Zona 1 260 - 280 °C -
Zona 2 280 - 305 °C -
Zona 3 295 - 315 °C -
Características
Procesamiento y forma de entrega
Moldeo por inyección
Applicaciones
Automotriz
Disponibilidad regional
Asia Pacifico
Disclaimer
Copyright Altair Engineering GmbH. Altair Engineering GmbH assumes no liability for the system to be free of errors. The user takes sole responsibility for the use of this data under the exclusion of every liability from Altair Engineering GmbH; this is especially valid for claims of compensation resulting from consequential damages. Altair explicitly points out that any decision about the application of materials must be double checked with the producer of this material. This includes all contents of this system. Copyright laws are applicable for the content of this system.
Created: Source: www.materialdatacenter.com


Material Data Center is provided by M-Base Engineering + Software GmbH. M-Base Engineering + Software GmbH assumes no liability for the system to be free of errors. Any decision about the application of materials must be double checked with the producer of this material.

Additional information about this material, like producer contact address, etc. can be found at www.materialdatacenter.com. For access to this extra information a registration is requested. Free online registration is available.