Complete Set of CAMPUS® Data, ASTM Data, Biopolymer Database, Application Database, Tradename Database, Literature Database, Toolbox.

Material datasheets available free. Online registration at: www.materialdatacenter.com

Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.

This is the free Material Data Center Datasheet of Genestar™ GN2330-1 - PA9T-GF33 FR... - Kuraray Co., Ltd.

Material Data Center offers the following functions for Genestar™ GN2330-1:
unit conversion, PDF datasheet print, comparison with other plastics

Check here, which other Genestar datasheets, application examples or technical articles are available in Material Data Center

Use the following short links to get directly to the properties of interest in this datasheet:
Any use of this information falls under the rules of our disclaimer.
Texto del producto
Genestar GN2330-1 is one of standard grades.

Main feature of GN2300-1 is:
 -Good balance of mechanical strength, mold ability, and dimensional stability

Examples of applications are:
 -FPC Connectors
 -Board to Board / Wire to Board Connectors
Caracteristicas de procesamiento y fisicasValorUnidadesMétodo de ensayo
ISO Data
Contracción posterior al moldeo, paralelo 0.2 % ISO 294-4, 2577
Contracción posterior al moldeo, normal 0.8 % ISO 294-4, 2577
ASTM Data
Índice de fluidez, MFI 21 g/10min ASTM D 1238
Temperatura 320 °C -
Carga 2.16 kg -
Propiedades mecánicasValorUnidadesMétodo de ensayo
ISO Data
Resistencia a la tracción 184 MPa ISO 527
Alargamiento a rotura 1.8 % ISO 527
Resistencia al impacto Charpy c/entalla, +23°C 11 kJ/m² ISO 179/1eA
ASTM Data
Esfuerzo de tracción 185 MPa ASTM D 638
Módulo de flexión 11000 MPa ASTM D 790
Resistencia a la flexión 240 MPa ASTM D 790
Resistencia al impacto Izod con entalla, 1/8 in 100 J/m ASTM D 256
Propiedades térmicasValorUnidadesMétodo de ensayo
ISO Data
Temperatura de fusión, 10°C/min 306 °C ISO 11357-1/-3
Temp. de transición vítrea, 10°C/min 125 °C ISO 11357-1/-2
Estabilidad al calor, 1.80 MPa 285 °C ISO 75-1/-2
Combustibilidad a 1.5mm esp. nom. V-0 class IEC 60695-11-10
Combustibilidad a espesor h V-0 class IEC 60695-11-10
Espesores de probeta 0.8 mm -
ASTM Data
Combustibilidad UL 94 V-0 - UL 94
Estabilidad al calor @ 264 psi 285 °C ASTM D 648
Temperatura de fusión 306 °C ASTM D 3418
Temperatura de transición vítrea 125 °C ASTM E 1356
Propiedades eléctricasValorUnidadesMétodo de ensayo
ISO Data
Resistencia dieléctrica 30 kV/mm IEC 60243-1
ASTM Data
Resistencia dieléctrica, tiempo corto 30 kV/mm ASTM D 149
Resistividad volumétrica >1E15 Ohm*cm ASTM D 257
Otras propiedadesValorUnidadesMétodo de ensayo
Absorción de agua 0.13 % Sim. to ISO 62
Densidad 1620 kg/m³ ASTM D 792
Funciones
Esfuerzo-alargamiento , Genestar™ GN2330-1, PA9T-GF33 FR..., Kuraray
Módulo secante-alargamiento , Genestar™ GN2330-1, PA9T-GF33 FR..., Kuraray
Características
Procesamiento y forma de entrega
Moldeo por inyección
Forma de suministro
Sémola
Características especiales
Resistencia mejorada al fuego, Estable contra el calor
Características
Soldable
Disponibilidad regional
Disclaimer
Copyright Altair Engineering GmbH. Altair Engineering GmbH assumes no liability for the system to be free of errors. The user takes sole responsibility for the use of this data under the exclusion of every liability from Altair Engineering GmbH; this is especially valid for claims of compensation resulting from consequential damages. Altair explicitly points out that any decision about the application of materials must be double checked with the producer of this material. This includes all contents of this system. Copyright laws are applicable for the content of this system.
Created: Source: www.materialdatacenter.com


Material Data Center is provided by M-Base Engineering + Software GmbH. M-Base Engineering + Software GmbH assumes no liability for the system to be free of errors. Any decision about the application of materials must be double checked with the producer of this material.

Additional information about this material, like producer contact address, etc. can be found at www.materialdatacenter.com. For access to this extra information a registration is requested. Free online registration is available.