Complete Set of CAMPUS® Data, ASTM Data, Biopolymer Database, Application Database, Tradename Database, Literature Database, Toolbox.

Material datasheets available free. Online registration at: www.materialdatacenter.com

Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.

This is the free Material Data Center Datasheet of Tritan™ EX401 - Copolyester - Eastman Chemical Co.

Material Data Center offers the following functions for Tritan™ EX401:
unit conversion, PDF datasheet print, comparison with other plastics, snap fit calculation, beam deflection calculation, CAE Interfaces

Check here, which other Tritan datasheets, application examples or technical articles are available in Material Data Center

Use the following short links to get directly to the properties of interest in this datasheet:
Any use of this information falls under the rules of our disclaimer.
Texto del producto

Tritan EX401, specifically developed for the Infant Care market, is an amorphous copolyester with excellent appearance and clarity. Tritan EX401 contains a mold release derived from vegetable based sources. Its most outstanding features are clarity, excellent toughness, hydrolytic stability, and heat and chemical resistance. Tritan EX401 meets infant care sterilization requirements via boiling water or microwave steam sterilization. This newgeneration copolyester can also be molded into various applications without incorporating high levels of residual stress. Combined with Tritan's outstanding chemical resistance and hydrolytic stability, these features give molded products enhanced durability in the dishwasher environment, which can expose products to high heat, humidity, and aggressive cleaning agents.

Tritan EX401 can be converted into parts using injection molding, injection stretch blow molding (ISBM), and extrusion blow molding techniques.

Tritan EX401 may be used in repeated use food contact articles under United States Food and Drug Administration (FDA) regulations. Contact Eastman representative for details on global food contact regulatory clearances.




Caracteristicas de procesamiento y fisicasValorUnidadesMétodo de ensayo
ASTM Data
Contracción posterior al moldeo, paralelo 0.006 mm/mm ASTM D 955
Propiedades mecánicasValorUnidadesMétodo de ensayo
ISO Data
Módulo de tracción 1620 MPa ISO 527
Esfuerzo de fluencia 45 MPa ISO 527
Alarg. en límite elástico 7 % ISO 527
Resistencia a la tracción 49 MPa ISO 527
Alargamiento a rotura 130 % ISO 527
Módulo de flexión, 23°C 1530 MPa ISO 178
Resistencia al impacto Izod con entalla, +23°C 66 kJ/m² ISO 180/1A
Resistencia al impacto Izod con entalla 14 kJ/m² ISO 180/1A
Temperatura -40 °C -
ASTM Data
Módulo de tracción 1585 MPa ASTM D 638
Esfuerzo de fluencia a tracción 44 MPa ASTM D 638
Esfuerzo de fractura a tracción 53.1 MPa ASTM D 638
Alargamiento a la fluencia 7 % ASTM D 638
Alargamiento a la rotura 140 % ASTM D 638
Módulo de flexión 1585 MPa ASTM D 790
Dureza Rockwell R 115 - ASTM D 785
Resistencia al impacto Izod con entalla, 1/8 in 650 J/m ASTM D 256
Resistencia al impacto Izod con entalla, baja temperatura 126 J/m ASTM D 256
Temperatura -40 °C -
Resistencia al impacto Izod, 1/8 in N J/m ASTM D 256
Propiedades térmicasValorUnidadesMétodo de ensayo
ASTM Data
Estabilidad al calor @ 66 psi 109 °C ASTM D 648
Estabilidad al calor @ 264 psi 92 °C ASTM D 648
Propiedades opticasValorUnidadesMétodo de ensayo
ASTM Data
Opacidad 1 % ASTM D 1003
Transmitancia luminosa 92 % ASTM D 1003
Otras propiedadesValorUnidadesMétodo de ensayo
Densidad 1170 kg/m³ ASTM D 792
Recomendación para procesamiento Moldeo por inyecciónValorUnidadesMétodo de ensayo
Temperatura de pre-secado 88 °C -
Tiempo de pre-secado 4 - 6 h -
Temperatura de la masa 260 - 282 °C -
Temperatura del molde 38 - 66 °C -
Recomendación para procesamiento ExtrusiónValorUnidadesMétodo de ensayo
Temperatura de pre-secado 88 °C -
Tiempo de pre-secado 4 - 6 h -
Temperatura de la masa 240 - 250 °C -
Temperatura del molde 25 - 45 °C -
Características
Procesamiento y forma de entrega
Moldeo por inyección, Moldeo por soplado
Aditivos
Desmoldeante
Características especiales
Alto impacto o modificado al impacto, Estable contra el calor, Transparente, Esterilizable, Esterilización por vapor
Características
Amorfo, Copolímero
Resistencia quimica
Resistencia química general, Estabilidad hidrolitica
Certifications
Contacto con alimentos, Aprobado por el FDA 21 CFR
Disponibilidad regional
Norteamérica, Europa, Asia Pacifico, América del Sur y Centroaméric, Próximo Oriente/Africa
Disclaimer
Copyright Altair Engineering GmbH. Altair Engineering GmbH assumes no liability for the system to be free of errors. The user takes sole responsibility for the use of this data under the exclusion of every liability from Altair Engineering GmbH; this is especially valid for claims of compensation resulting from consequential damages. Altair explicitly points out that any decision about the application of materials must be double checked with the producer of this material. This includes all contents of this system. Copyright laws are applicable for the content of this system.
Created: Source: www.materialdatacenter.com


Material Data Center is provided by M-Base Engineering + Software GmbH. M-Base Engineering + Software GmbH assumes no liability for the system to be free of errors. Any decision about the application of materials must be double checked with the producer of this material.

Additional information about this material, like producer contact address, etc. can be found at www.materialdatacenter.com. For access to this extra information a registration is requested. Free online registration is available.