Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.

This is the free Material Data Center Datasheet of Repol MI3530 - PP - Reliance Polymers

Material Data Center offers the following functions for Repol MI3530:
unit conversion, PDF datasheet print, comparison with other plastics

Check here, which other Repol datasheets, application examples or technical articles are available in Material Data Center

Use the following short links to get directly to the properties of interest in this datasheet:
Any use of this information falls under the rules of our disclaimer.
Caracteristicas de procesamiento y fisicasValorUnidadesMétodo de ensayo
ASTM Data
Índice de fluidez 3 g/10min ASTM D 1238
Temperatura 230 °C -
Carga 2.16 kg -
Propiedades mecánicasValorUnidadesMétodo de ensayo
ASTM Data
Esfuerzo de fluencia a tracción 26 MPa ASTM D 638
Alargamiento a la fluencia 12 % ASTM D 638
Resistencia al impacto Izod con entalla, 1/8 in 0.115 kJ/m ASTM D 256
Propiedades térmicasValorUnidadesMétodo de ensayo
ASTM Data
Estabilidad al calor @ 66 psi 95 °C ASTM D 648
Características
Procesamiento y forma de entrega
Moldeo por inyección
Características
Copolímero, Copolímero de impacto
Certifications
Contacto con alimentos, Aprobado por el FDA 21 CFR
Applicaciones
Automotriz
Disponibilidad regional
Europa, Asia Pacifico, Próximo Oriente/Africa
Disclaimer
Copyright M-Base Engineering+Software GmbH. M-Base Engineering + Software GmbH assumes no liability for the system to be free of errors. The user takes sole responsibility for the use of this data under the exclusion of every liability from M-Base; this is especially valid for claims of compensation resulting from consequential damages. M-Base explicitly points out that any decision about the application of materials must be double checked with the producer of this material. This includes all contents of this system. Copyright laws are applicable for the content of this system.
Created: 2018-02-25 Source: www.materialdatacenter.com


Material Data Center is provided by M-Base Engineering + Software GmbH. M-Base Engineering + Software GmbH assumes no liability for the system to be free of errors. Any decision about the application of materials must be double checked with the producer of this material.

Additional information about this material, like producer contact address, etc. can be found at www.materialdatacenter.com. For access to this extra information a registration is requested. Free online registration is available.