Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.

This is the free Material Data Center Datasheet of THERMOLAST® K TC8GPZ - TPE - KRAIBURG TPE GmbH & Co. KG

Material Data Center offers the following functions for THERMOLAST® K TC8GPZ:
unit conversion, PDF datasheet print, comparison with other plastics

Check here, which other Thermolast datasheets, application examples or technical articles are available in Material Data Center

Use the following short links to get directly to the properties of interest in this datasheet:
Any use of this information falls under the rules of our disclaimer.
Product Texts
adhesion to PP
excellent mechanical properties
natural compounds easy to colour
meets odour specification for automotive interior
listed according to UL 94 HB
excellent weather resistance for black compounds

Typical Applications:
•    design-functional elements: packaging
•    automotive indoor and under the hood: anti-slip-mats, air-run-channels, air-water-channels
•    soft touch: tracer, push buttons, switches
•    handles: screwdriver, toolbox, ski and hiking sticks

Material Advantages
•    excellent physical properties
•    natural compounds easy to colour
•    meets odour specification for automotive interior
•    good weather resistance for black compounds
•    listed according to UL94HB
•    very good flow characteristics
•    adhesion to PP

Processing
•    like polyolefine
•    processing temperature 180°C to 220 °C (max. 250°C)
•    preferably high injection and pressure
Mechanical propertiesValueUnit
ISO Data
Tensile Strength 10.5 MPa
Strain at break TPE >300 %
Compression set at 23 °C, 24h 30 %
Compression set at 70 °C, 24h 50 %
Compression set at 100 °C, 24h 78 %
Tear strength 29 kN/m
Shore A hardness 80 -
Thermal propertiesValueUnit
ISO Data
Burning behav. at 1.5 mm nom. thickn. HB class
Other propertiesValueUnit
Density 1100 kg/m³
Characteristics
Delivery form
Black
Special Characteristics
Light stabilized or stable to light, U.V. stabilized or stable to weather
Regional Availability
North America, Europe, Asia Pacific
Disclaimer
Copyright M-Base Engineering + Software GmbH. M-Base Engineering + Software GmbH assumes no liability for the system to be free of errors. The user takes sole responsibility for the use of this data under the exclusion of every liability from M-Base; this is especially valid for claims of compensation resulting from consequential damages. M-Base explicitly points out that any decision about the application of materials must be double checked with the producer of this material. This includes all contents of this system. Copyright laws are applicable for the content of this system.
Created: Source: www.materialdatacenter.com


Material Data Center is provided by M-Base Engineering + Software GmbH. M-Base Engineering + Software GmbH assumes no liability for the system to be free of errors. Any decision about the application of materials must be double checked with the producer of this material.

Additional information about this material, like producer contact address, etc. can be found at www.materialdatacenter.com. For access to this extra information a registration is requested. Free online registration is available.