Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.
This is the free Material Data Center Datasheet of TEDUR L PPS 1000 15087 - PPS - MOCOM Compounds GmbH & Co. KG
unit conversion, PDF datasheet print, comparison with other plastics, snap fit calculation, beam deflection calculation, CAE Interfaces
Check here, which other Tedur datasheets, application examples or technical articles are available in Material Data Center
Base Polymer | Polyphenylene Sulphide |
Special Features | elastomer modified,high toughness |
Market Segment | Automotive,Machinery |
Application Area | extrusion grade |
Typical Applications | ducting / piping systems,functional components |
Mechanical properties | Value | Unit | Test Standard | ||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||
ISO Data | |||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||
Tensile Modulus | 2000 | MPa | ISO 527 | ||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||
Yield stress | 45 | MPa | ISO 527 | ||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||
Yield strain | 3.7 | % | ISO 527 | ||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||
Charpy impact strength, +23°C | N | kJ/m² | ISO 179/1eU |
Thermal properties | Value | Unit | Test Standard | ||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||
ISO Data | |||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||
Burning Behav. at 1.5 mm nom. thickn. | V-0 | class | IEC 60695-11-10 | ||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||
Thickness tested | 1.5 | mm | - |
Other properties | Value | Unit | Test Standard |
Density | 1270 | kg/m³ | ISO 1183 |
Pre-Drying Conditions | in a dry air (dessiccant) dryer 100-130 °C for 2-4 h |
Processing Injection Moulding | melt temperature 290-310 °C mould temperature >100 °C |
Processing Extrusion | melt temperature 290-310 °C |
Storage | dry, protected from light |