Complete Set of CAMPUS® Data, ASTM Data, Biopolymer Database, Application Database, Tradename Database, Literature Database, Toolbox. Information about Biopolymers, a project by FH Hannover and M-Base Engineering & Software GmbH sponsored by Fachagentur Nachwachsende Rohstoffe (FNR).

Material datasheets available free. Online registration at: www.materialdatacenter.com

Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.

This is the free Material Data Center Datasheet of Desmopan® CQ33085AUEC DPS300 - TPU - Covestro Deutschland AG

Material Data Center offers the following functions for Desmopan® CQ33085AUEC DPS300:
unit conversion, PDF datasheet print, comparison with other plastics

Check here, which other Desmopan datasheets, application examples or technical articles are available in Material Data Center

Use the following short links to get directly to the properties of interest in this datasheet:
Any use of this information falls under the rules of our disclaimer.
Mechanical propertiesValueUnitTest Standard
ISO Data
Tensile Strength 46 MPa ISO 37
Strain at break 616 % ISO 37
Tear strength 98 kN/m ISO 34-1
Abrasion resistance 47 mm³ ISO 4649
Shore A hardness 83 - ISO 7619-1
Other Standards[S]
Stress at 100% elongation 5.2 MPa DIN 53504
Stress at 300% elongation 10.1 MPa DIN 53504
S: These properties are reported by the producer according standards that are different to our defaults.
Other propertiesValueUnitTest Standard
Density 1270 kg/m³ ISO 1183
Processing Recommendation Injection MoldingValueUnitTest Standard
Pre-drying - Temperature <110 °C -
Melt temperature 165 - 185 °C -
Mold temperature 20 - 40 °C -
Characteristics
Processing
Injection Molding, Other Extrusion
Special Characteristics
U.V. stabilized or stable to weather
Certifications
Contains renewable resources
Regional Availability
North America, Europe, Asia Pacific, South and Central America, Near East/Africa
Disclaimer
Copyright Altair Engineering GmbH. Altair Engineering GmbH assumes no liability for the system to be free of errors. The user takes sole responsibility for the use of this data under the exclusion of every liability from Altair Engineering GmbH; this is especially valid for claims of compensation resulting from consequential damages. Altair explicitly points out that any decision about the application of materials must be double checked with the producer of this material. This includes all contents of this system. Copyright laws are applicable for the content of this system.
Created: Source: www.materialdatacenter.com


Material Data Center is provided by M-Base Engineering + Software GmbH. M-Base Engineering + Software GmbH assumes no liability for the system to be free of errors. Any decision about the application of materials must be double checked with the producer of this material.

Additional information about this material, like producer contact address, etc. can be found at www.materialdatacenter.com. For access to this extra information a registration is requested. Free online registration is available.