Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.
This is the free Material Data Center Datasheet of ALTECH PA66 ECO 2030/510 GF30 IM - PA66-I-GF30 - MOCOM Compounds GmbH & Co. KG
unit conversion, PDF datasheet print, comparison with other plastics, snap fit calculation, beam deflection calculation, CAE Interfaces
Check here, which other Altech datasheets, application examples or technical articles are available in Material Data Center
Base Polymer | Polyamide 66 |
Filler/Additive System | 30 % glass fibres |
Special Features | heat stabilised,injection moulding grade,easy release (demoulding),impact modified |
Market Segment | various |
Application Area | lighting,domestic appliances |
Mechanical properties | Value | Unit | Test Standard | ||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||
ISO Data | |||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||
Tensile Modulus | 8900 | MPa | ISO 527 | ||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||
Stress at break | 135 | MPa | ISO 527 | ||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||
Strain at break | 3.2 | % | ISO 527 | ||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||
Charpy impact strength, +23°C | 65 | kJ/m² | ISO 179/1eU | ||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||
Charpy notched impact strength, +23°C | 9.5 | kJ/m² | ISO 179/1eA |
Thermal properties | Value | Unit | Test Standard | ||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||
ISO Data | |||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||
Temp. of deflection under load, 1.80 MPa | 249 | °C | ISO 75-1/-2 |
Other properties | Value | Unit | Test Standard |
Density | 1400 | kg/m³ | ISO 1183 |
Pre-Drying Conditions | 80 °C in a dry air (dessiccant) dryer for 2-12 h dependant on moisture content |
Processing Injection Moulding | melt temperature 280-300 °C mould temperature 80-90 °C |
Storage | dry, protected from light |