Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.

This is the free Material Data Center Datasheet of Tritan™ TXF1021 - Copolyester - Eastman Chemical Co.

Material Data Center offers the following functions for Tritan™ TXF1021:
unit conversion, PDF datasheet print, comparison with other plastics

Check here, which other Tritan datasheets, application examples or technical articles are available in Material Data Center

Use the following short links to get directly to the properties of interest in this datasheet:
Any use of this information falls under the rules of our disclaimer.
Product Texts

Eastman Tritan™ Copolyester TXF1021 is an amorphous, opaque material offering UL-94 V2 performance with outstanding aesthetics and gloss. Eastman Tritan™ Copolyester TXF1021 has many outstanding features that include excellent toughness, hydrolytic stability, heat resistance, chemical resistance, and melt flowability.

Eastman Tritan™ Copolyester TXF1021 offers improved design flexibility needed in portable consumer electronic devices. Eastman Tritan™ Copolyester TXF1021 has passed FDA/ISO 10993 testing for skin sensitization. Eastman Tritan™ Copolyester TXF1021 contains a non-halogenated flame retardant.

Processing/Physical CharacteristicsValueUnitTest Standard
ASTM Data
Mold Shrinkage, MD 0.006 mm/mm ASTM D 955
Mechanical propertiesValueUnitTest Standard
ASTM Data
Tensile Modulus 1611 MPa ASTM D 638
Tensile Strength at Yield 42 MPa ASTM D 638
Tensile Strength at Break 46 MPa ASTM D 638
Elongation at Yield 6 % ASTM D 638
Elongation at Break 133 % ASTM D 638
Flexural Modulus 1743 MPa ASTM D 790
Rockwell Hardness R 109 - ASTM D 785
Izod Impact notched, 1/8 in 436 J/m ASTM D 256
Izod Impact unnotched, 1/8 in N J/m ASTM D 256
Thermal propertiesValueUnitTest Standard
ASTM Data
UL 94 Flame rating V-2 - UL 94
Thickness tested 1.5 mm -
DTUL @ 66 psi 94 °C ASTM D 648
DTUL @ 264 psi 83 °C ASTM D 648
Other propertiesValueUnitTest Standard
Density 1190 kg/m³ ASTM D 792
Processing Recommendation Injection MoldingValueUnitTest Standard
Pre-drying - Temperature 88 °C -
Pre-drying - Time 4 - 6 h -
Melt temperature 260 - 282 °C -
Mold temperature 38 - 66 °C -
Characteristics
Processing
Injection Molding
Delivery form
Natural Color
Additives
Flame retarding agent
Special Characteristics
Flame retardant, Halogen-free, Heat stabilized or stable to heat, Opaque
Features
Amorphous, High Gloss, Copolymer
Chemical Resistance
General Chemical Resistance, Hydrolytically Stable
Applications
Electrical and Electronical
Regional Availability
North America, Europe, Asia Pacific, South and Central America, Near East/Africa
Disclaimer
Copyright Altair Engineering GmbH. Altair Engineering GmbH assumes no liability for the system to be free of errors. The user takes sole responsibility for the use of this data under the exclusion of every liability from Altair Engineering GmbH; this is especially valid for claims of compensation resulting from consequential damages. Altair explicitly points out that any decision about the application of materials must be double checked with the producer of this material. This includes all contents of this system. Copyright laws are applicable for the content of this system.
Created: Source: www.materialdatacenter.com


Material Data Center is provided by M-Base Engineering + Software GmbH. M-Base Engineering + Software GmbH assumes no liability for the system to be free of errors. Any decision about the application of materials must be double checked with the producer of this material.

Additional information about this material, like producer contact address, etc. can be found at www.materialdatacenter.com. For access to this extra information a registration is requested. Free online registration is available.