Complete Set of CAMPUS® Data, ASTM Data, Biopolymer Database, Application Database, Tradename Database, Literature Database, Toolbox.

Material datasheets available free. Online registration at: www.materialdatacenter.com

Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.

This is the free Material Data Center Datasheet of Tritan™ EX501 - Copolyester - Eastman Chemical Co.

Material Data Center offers the following functions for Tritan™ EX501:
unit conversion, PDF datasheet print, comparison with other plastics, snap fit calculation, beam deflection calculation, CAE Interfaces

Check here, which other Tritan datasheets, application examples or technical articles are available in Material Data Center

Use the following short links to get directly to the properties of interest in this datasheet:
Any use of this information falls under the rules of our disclaimer.
Product Texts

Tritan EX501 is an amorphous copolyester specifically developed for the Infant Care market. Its most outstanding features are consistent glass-like clarity even after multiple dishwasher cycles. Additionally, Tritan EX501 exhibits

low taste and odor retention versus cPP, excellent drop impact resistance, and dishwasher durability. Tritan EX501 contains a mold release derived from vegetable based sources. Tritan EX501 meets infant care sterilization

requirements via boiling water or microwave steam sterilization. This new-generation copolyester can also be molded into various applications without incorporating high levels of residual stress. Combined with Tritan's

outstanding chemical resistance and hydrolytic stability, these features give molded products enhanced durability in the dishwasher environment, which can expose products to high heat, humidity, and aggressive cleaning agents.

Tritan EX501 can be converted into parts using injection molding, injection stretch blow molding (ISBM), and extrusion blow molding techniques.

Tritan EX501 copolyester may be used in repeated-use food contact articles under United States Food and Drug Administration (FDA) regulations. Contact an Eastman representative for details on global food contact regulatory clearances.

Processing/Physical CharacteristicsValueUnitTest Standard
ASTM Data
Mold Shrinkage, MD 0.006 mm/mm ASTM D 955
Mechanical propertiesValueUnitTest Standard
ISO Data
Tensile Modulus 1540 MPa ISO 527
Yield stress 44 MPa ISO 527
Yield strain 6 % ISO 527
Stress at break 55 MPa ISO 527
Strain at break 151 % ISO 527
Izod notched impact strength, +23°C 114 kJ/m² ISO 180/1A
Izod notched impact strength 14 kJ/m² ISO 180/1A
Temperature -40 °C -
ASTM Data
Tensile Modulus 1516 MPa ASTM D 638
Tensile Strength at Yield 45 MPa ASTM D 638
Tensile Strength at Break 56 MPa ASTM D 638
Elongation at Yield 6 % ASTM D 638
Elongation at Break 176 % ASTM D 638
Rockwell Hardness R 109 - ASTM D 785
Izod Impact notched, 1/8 in 1020 J/m ASTM D 256
Izod Impact notched, Low-Temperature 136 J/m ASTM D 256
Temperature -40 °C -
Izod Impact unnotched, 1/8 in N J/m ASTM D 256
Thermal propertiesValueUnitTest Standard
ASTM Data
DTUL @ 66 psi 101 °C ASTM D 648
DTUL @ 264 psi 88 °C ASTM D 648
Optical propertiesValueUnitTest Standard
ASTM Data
Haze 1 % ASTM D 1003
Light Transmittance 91 % ASTM D 1003
Other propertiesValueUnitTest Standard
Density 1180 kg/m³ ASTM D 792
Processing Recommendation Injection MoldingValueUnitTest Standard
Pre-drying - Temperature 88 °C -
Pre-drying - Time 4 - 6 h -
Melt temperature 260 - 282 °C -
Mold temperature 38 - 66 °C -
Characteristics
Processing
Injection Molding, Blow Molding
Additives
Release agent
Special Characteristics
Heat stabilized or stable to heat, Transparent, Sterilizable, Steam sterilization
Features
Amorphous, Copolymer
Chemical Resistance
General Chemical Resistance, Hydrolytically Stable, Stain Resistance
Certifications
Food contact, Food approval FDA 21 CFR
Regional Availability
North America, Europe, Asia Pacific, South and Central America, Near East/Africa
Disclaimer
Copyright Altair Engineering GmbH. Altair Engineering GmbH assumes no liability for the system to be free of errors. The user takes sole responsibility for the use of this data under the exclusion of every liability from Altair Engineering GmbH; this is especially valid for claims of compensation resulting from consequential damages. Altair explicitly points out that any decision about the application of materials must be double checked with the producer of this material. This includes all contents of this system. Copyright laws are applicable for the content of this system.
Created: Source: www.materialdatacenter.com


Material Data Center is provided by M-Base Engineering + Software GmbH. M-Base Engineering + Software GmbH assumes no liability for the system to be free of errors. Any decision about the application of materials must be double checked with the producer of this material.

Additional information about this material, like producer contact address, etc. can be found at www.materialdatacenter.com. For access to this extra information a registration is requested. Free online registration is available.