Complete Set of CAMPUS® Data, ASTM Data, Biopolymer Database, Application Database, Tradename Database, Literature Database, Toolbox.

Material datasheets available free. Online registration at: www.materialdatacenter.com

Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.

This is the free Material Data Center Datasheet of Tritan™ FX200 - Copolyester - Eastman Chemical Co.

Material Data Center offers the following functions for Tritan™ FX200:
unit conversion, PDF datasheet print, comparison with other plastics

Check here, which other Tritan datasheets, application examples or technical articles are available in Material Data Center

Use the following short links to get directly to the properties of interest in this datasheet:
Any use of this information falls under the rules of our disclaimer.
Product Texts

Eastman Tritan™ FX200 is a copolyester resin for calendered and extruded film applications where enhanced heat resistance and toughness are required. It works great in hot fill packaging for food, transaction and identification cards, and protective laminates.

Packaging brands and film converters prefer Tritan™ FX200 for its ability to provide a clear, aesthetically pleasing package that stands up to the strenuous requirements for hot filling, while also providing safety that consumers expect. It’s great for brands looking to replace materials of concern or premiumize their packaging by transitioning from opaque to clear.

Transaction and identification card producers, brands, and governments alike value Tritan™ FX200 for its excellent bend strength and chemical resistance, which provides longer useful life and better security. Compared to PVC and other material alternatives, transaction cards made with Tritan™ have been found to withstand more than 10 times the number of flexural cycles using industry standard fitness for use testing protocols.

Tritan™ FX200 may be used in various food contact applications under the U.S. Food & Drug Administration (FDA) regulations.

Thermal propertiesValueUnitTest Standard
ASTM Data
Coefficient of Thermal Expansion, MD 80 E-6/K ASTM D 696
Glass Transition Temperature 119 °C ASTM E 1356
Optical propertiesValueUnitTest Standard
ASTM Data
Gloss 158 - ASTM D 2457
Haze 0.8 % ASTM D 1003
Light Transmittance 93 % ASTM D 1003
Index of Refraction 1.54 - ASTM D 542
Other propertiesValueUnitTest Standard
Water Absorption, 24hr 0.5 % ASTM D 570
Density 1190 kg/m³ ASTM D 792
Film PropertiesValueUnitTest Standard
ISO Data
Trouser Tear resistance, parallel 10 N/mm ISO 6383-1
Trouser Tear resistance, normal 9 N/mm ISO 6383-1
Thickness of specimen 0.254 mm -
ASTM Data
Tensile Modulus, MD 1500 MPa ASTM D 882
Tensile Modulus, TD 1400 MPa ASTM D 882
Tensile Strength at Yield, MD 43 MPa ASTM D 882
Tensile Strength at Yield, TD 41 MPa ASTM D 882
Tensile Strength at Break, MD 57 MPa ASTM D 882
Tensile Strength at Break, TD 42 MPa ASTM D 882
Elongation at Yield, MD 8 % ASTM D 882
Elongation at Yield, TD 8 % ASTM D 882
Elongation at Break, MD 114 % ASTM D 882
Elongation at Break, TD 115 % ASTM D 882
Thickness of specimen 0.254 mm -
Characteristics
Processing
Other Extrusion
Special Characteristics
Heat stabilized or stable to heat, Transparent
Features
High Gloss, Scratch Resistant, Copolymer
Chemical Resistance
General Chemical Resistance
Certifications
Food contact, Food approval FDA 21 CFR
Applications
Packaging
Regional Availability
North America, Europe, Asia Pacific, South and Central America, Near East/Africa
Disclaimer
Copyright Altair Engineering GmbH. Altair Engineering GmbH assumes no liability for the system to be free of errors. The user takes sole responsibility for the use of this data under the exclusion of every liability from Altair Engineering GmbH; this is especially valid for claims of compensation resulting from consequential damages. Altair explicitly points out that any decision about the application of materials must be double checked with the producer of this material. This includes all contents of this system. Copyright laws are applicable for the content of this system.
Created: Source: www.materialdatacenter.com


Material Data Center is provided by M-Base Engineering + Software GmbH. M-Base Engineering + Software GmbH assumes no liability for the system to be free of errors. Any decision about the application of materials must be double checked with the producer of this material.

Additional information about this material, like producer contact address, etc. can be found at www.materialdatacenter.com. For access to this extra information a registration is requested. Free online registration is available.