Complete Set of CAMPUS® Data, ASTM Data, Biopolymer Database, Application Database, Tradename Database, Literature Database, Toolbox. Information about Biopolymers, a project by FH Hannover and M-Base Engineering & Software GmbH sponsored by Fachagentur Nachwachsende Rohstoffe (FNR).

Material datasheets available free. Online registration at: www.materialdatacenter.com

Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.

This is the free Material Data Center Datasheet of Tenite™ Butyrate 285A2R30020 - CAB - Eastman Chemical Co.

Material Data Center offers the following functions for Tenite™ Butyrate 285A2R30020:
unit conversion, PDF datasheet print, comparison with other plastics

Check here, which other Tenite datasheets, application examples or technical articles are available in Material Data Center

Use the following short links to get directly to the properties of interest in this datasheet:
Any use of this information falls under the rules of our disclaimer.
Product Texts

Tenite™ cellulosic plastics are noted for their excellent balance of properties - toughness, hardness, strength, surface gloss, clarity, and a warm feel. The mechanical properties of Tenite™ cellulosic plastics differ with plasticizer levels. Lower plasticizer content yields a harder surface, higher heat resistance, greater rigidity, higher tensile strength, and better dimensional stability. Higher plasticizer content increases impact strength. Tenite™ cellulose plastics are available in natural, clear, selected ambers, or smoke transparents and black translucents.

Color concentrates are available in let-down ratios from 10:1 to 40:1. Tenite™ Cellulose Acetate Butyrate 285-20 has a plasticizer level of 20% and contains an odor mask.

Mechanical propertiesValueUnitTest Standard
ASTM Data
Tensile Strength at Yield 21.4 MPa ASTM D 638
Tensile Strength at Break 27.6 MPa ASTM D 638
Elongation at Break 50 % ASTM D 638
Flexural Modulus 965 MPa ASTM D 790
Rockwell Hardness R 12 - ASTM D 785
Izod Impact notched, 1/8 in 384 J/m ASTM D 256
Izod Impact notched, Low-Temperature 112 J/m ASTM D 256
Temperature -40 °C -
Thermal propertiesValueUnitTest Standard
ASTM Data
DTUL @ 66 psi 72 °C ASTM D 648
DTUL @ 264 psi 58 °C ASTM D 648
Vicat Temperature 92 °C ASTM D 1525
Other propertiesValueUnitTest Standard
Water Absorption, 24hr 1.2 % ASTM D 570
Density 1170 kg/m³ ASTM D 792
Characteristics
Delivery form
Natural Color
Additives
Plasticizer
Special Characteristics
Transparent
Features
High Gloss, Low Odor
Certifications
Contains renewable resources
Applications
Sports Equipment
Regional Availability
North America, Europe, Asia Pacific, South and Central America, Near East/Africa
Disclaimer
Copyright Altair Engineering GmbH. Altair Engineering GmbH assumes no liability for the system to be free of errors. The user takes sole responsibility for the use of this data under the exclusion of every liability from Altair Engineering GmbH; this is especially valid for claims of compensation resulting from consequential damages. Altair explicitly points out that any decision about the application of materials must be double checked with the producer of this material. This includes all contents of this system. Copyright laws are applicable for the content of this system.
Created: Source: www.materialdatacenter.com


Material Data Center is provided by M-Base Engineering + Software GmbH. M-Base Engineering + Software GmbH assumes no liability for the system to be free of errors. Any decision about the application of materials must be double checked with the producer of this material.

Additional information about this material, like producer contact address, etc. can be found at www.materialdatacenter.com. For access to this extra information a registration is requested. Free online registration is available.