Processing/Physical Characteristics | Value | Unit | Test Standard |
Other Standards[S] |
Melt Flow Index, MFI |
8 |
g/10min |
ASTM D 3307 |
Temperature |
372 |
°C |
- |
Load |
5 |
kg |
- |
S: | These properties are reported by the producer according standards that are different to our defaults. |
Mechanical properties | Value | Unit | Test Standard |
Other Standards[S] |
Tensile Strength |
28 |
MPa |
ASTM D 3307 |
S: | These properties are reported by the producer according standards that are different to our defaults. |
Thermal properties | Value | Unit | Test Standard |
Other Standards[S] |
Melting Temperature |
285 |
°C |
ASTM D 4591 |
S: | These properties are reported by the producer according standards that are different to our defaults. |
Electrical properties | Value | Unit | Test Standard |
Other Standards[S] |
Volume resistivity |
0.11 |
Ohm*m |
ISO 3915 |
S: | These properties are reported by the producer according standards that are different to our defaults. |
Other properties | Value | Unit | Test Standard |
Density |
2150 |
kg/m³ |
ASTM D 792 |
Characteristics
Processing
Other Extrusion, Blow Molding, Transfer Molding, Compression Molding
Delivery form
Pellets
Special Characteristics
Anti-static, U.V. stabilized or stable to weather
Features
Creep Resistance, Melt Strength, Thermal Stability, Tribologic Grade
Chemical Resistance
General Chemical Resistance, Solvent Resistance
Regional Availability
North America, Europe, Asia Pacific, South and Central America
Disclaimer
Copyright Altair Engineering GmbH. Altair Engineering GmbH assumes no liability for the system to be free of errors. The user takes sole responsibility for the use of this data under the exclusion of every liability from Altair Engineering GmbH; this is especially valid for claims of compensation resulting from consequential damages. Altair explicitly points out that any decision about the application of materials must be double checked with the producer of this material. This includes all contents of this system. Copyright laws are applicable for the content of this system.
Created: Source: www.materialdatacenter.com