Complete Set of CAMPUS® Data, ASTM Data, Biopolymer Database, Application Database, Tradename Database, Literature Database, Toolbox.

Material datasheets available free. Online registration at: www.materialdatacenter.com

Tecoform - POM - Eurotec Mühendislik Plastikleri

Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.

A search for "Tecoform" in Material Data Center leads to the following information:

Tradename: Tecoform
Family: POM
Producer: Eurotec Mühendislik Plastikleri
10 hits in the material database


Material Data Center offers information about the following products with the requested tradename. To view a datasheet, please click on the relevant product.

Datasheet Polymer
Tecoform® PO20 AR10 NL HS POM-AF10
Tecoform® PO20 GR10 NL HS POM-GF10
Tecoform® PO20 GR20 NL HS POM-GF20
Tecoform® PO20 GR25 NL HS POM-GF25
Tecoform® PO20 NL IL POM
Tecoform® PO20 NL RM POM...
Tecoform® PO20 NL RT (POM+PTFE)
Tecoform® PO20 NL RW POM
Tecoform® PO30 GB20 NL HS POM-GB20
Tecoform® PO30 GB30 NL HS POM-GB30

Additional information about this tradename, like producer contact address, etc. can be found at www.materialdatacenter.com. For access to this extra information a registration is requested. Free online registration is available.

Note: the information in Material Data Center was collected with maximum care, based on information from material producers. They are subject to short term changes at the market. There is no warranty for the correctness of this information. In no way this information can be seen as a legal advice, whether certain tradenames are protected or not.