Complete Set of CAMPUS® Data, ASTM Data, Biopolymer Database, Application Database, Tradename Database, Literature Database, Toolbox.

Material datasheets available free. Online registration at: www.materialdatacenter.com

Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.

This is the free Material Data Center Datasheet of PLEXIGLAS® Softlight zk6BR df22 - PMMA - Röhm GmbH

Material Data Center offers the following functions for PLEXIGLAS® Softlight zk6BR df22:
unit conversion, PDF datasheet print, comparison with other plastics, snap fit calculation, beam deflection calculation, parameters for material models, CAE Interfaces

Check here, which other Plexiglas datasheets, application examples or technical articles are available in Material Data Center

Use the following short links to get directly to the properties of interest in this datasheet:
Any use of this information falls under the rules of our disclaimer.
Product Texts

Productprofil:

PLEXIGLAS® Softlight zk6BR df22, based on PLEXIGLAS® Resist zk6BR, is an impact modified molding compound characterized by diffuse scattering of light.

 

Typical properties of impact modified PLEXIGLAS® molding compound are

 

  1. high break resistance and impact strength
  2. improved resistance to stress cracking
  3. good weather resistance
  4. high surface hardness and mar resistance
  5. the pleasant feel and sound of the moldings.

 

PLEXIGLAS® Softlight zk6BR df22 is characterized by the following special properties:

 

  1. very good lightdiffusion combined with excellent light transmission
  2. matte surfaces can be obtained by varying the extrusion parameters.


Application:

Used for extruding profiles and sheets, but also for injection molding items for lighting engineering applications

Example:

applications that call for light diffusion combined with optimum transmission

Processing:

PLEXIGLAS® Softlight zk6BR df22 can be processed on extruders with 3-zone general purpose screws for engineering thermoplastics.

The matte finish of profile surfaces depends very much on machine design (calibrating unit, polishing rolls) and cooling conditions. It can be enhanced by controlled temperature reduction.

Physical Form / Packaging:

PLEXIGLAS® Softlight df molding compounds are supplied as pellets of uniform size, packaged in 25kg polyethylene bags; other packaging on request.

Processing/Physical CharacteristicsValueUnitTest Standard
ISO Data
Melt volume-flow rate, MVR 1.4 cm³/10min ISO 1133
Temperature 230 °C -
Load 3.8 kg -
Mechanical propertiesValueUnitTest Standard
ISO Data
Tensile Modulus 1800 MPa ISO 527
Yield stress 45 MPa ISO 527
Yield strain 5 % ISO 527
Nominal strain at break 40 % ISO 527
Charpy impact strength, +23°C 54 kJ/m² ISO 179/1eU
Thermal propertiesValueUnitTest Standard
ISO Data
Glass transition temperature, 10°C/min 109 °C ISO 11357-1/-2
Temp. of deflection under load, 1.80 MPa 93 °C ISO 75-1/-2
Temp. of deflection under load, 0.45 MPa 99 °C ISO 75-1/-2
Vicat softening temperature, B 98 °C ISO 306
Coeff. of linear therm. expansion, parallel 90 E-6/K ISO 11359-1/-2
Burning Behav. at 1.5 mm nom. thickn. HB class IEC 60695-11-10
Electrical propertiesValueUnitTest Standard
ISO Data
Volume resistivity >1E13 Ohm*m IEC 62631-3-1
Surface resistivity 1E13 Ohm IEC 62631-3-2
Optical propertiesValueUnitTest Standard
ISO Data
Luminous transmittance 86 % ISO 13468-1, -2
Other propertiesValueUnitTest Standard
Density 1150 kg/m³ ISO 1183
Test specimen productionValueUnitTest Standard
ISO Data
Injection Molding, melt temperature 255 °C ISO 294
Injection Molding, mold temperature 58 °C ISO 294
Injection Molding, injection velocity 195 mm/s ISO 294
Diagrams
Viscosity-shear rate , PLEXIGLAS® Softlight zk6BR df22, PMMA, Röhm
Shearstress-shear rate , PLEXIGLAS® Softlight zk6BR df22, PMMA, Röhm
Dynamic Shear modulus-temperature , PLEXIGLAS® Softlight zk6BR df22, PMMA, Röhm
Stress-strain , PLEXIGLAS® Softlight zk6BR df22, PMMA, Röhm
Secant modulus-strain , PLEXIGLAS® Softlight zk6BR df22, PMMA, Röhm
Tensile modulus-temperature , PLEXIGLAS® Softlight zk6BR df22, PMMA, Röhm
Characteristics
Processing
Injection Molding, Profile Extrusion, Sheet Extrusion, Other Extrusion
Delivery form
Pellets
Additives
Release agent
Special Characteristics
High impact or impact modified, Light stabilized or stable to light, U.V. stabilized or stable to weather
Features
Light Diffusing
Chemical Resistance
Environmental Stress Crack Resistance
Regional Availability
North America, Europe, Asia Pacific, South and Central America, Near East/Africa
Other text information
Injection molding
PREPROCESSING
Predrying temperature: max. 80 °C
Predrying time in a desiccant-type drier: 2 - 3 h
PROCESSING
Melt temperature: 220 - 260°C
Mold temperature:60 - 90°C
Profile extrusion
PREPROCESSING
Predrying temperature: max. 80 °C
Predrying time in a desiccant-type drier: 2 - 3 h
PROCESSING
Melt temperature: 230 - 260 °C

Die temperature: 230 - 260 °C
Sheet extrusion
PREPROCESSING
Predrying temperature: max. 80 °C
Predrying time in a desiccant-type drier: 2 - 3 h
PROCESSING
Melt temperature: 230 - 260 °C
Die temperature: 230 - 260 °C
Disclaimer
Copyright Altair Engineering GmbH. Altair Engineering GmbH assumes no liability for the system to be free of errors. The user takes sole responsibility for the use of this data under the exclusion of every liability from Altair Engineering GmbH; this is especially valid for claims of compensation resulting from consequential damages. Altair explicitly points out that any decision about the application of materials must be double checked with the producer of this material. This includes all contents of this system. Copyright laws are applicable for the content of this system.
Created: Source: www.materialdatacenter.com


Material Data Center is provided by M-Base Engineering + Software GmbH. M-Base Engineering + Software GmbH assumes no liability for the system to be free of errors. Any decision about the application of materials must be double checked with the producer of this material.

Additional information about this material, like producer contact address, etc. can be found at www.materialdatacenter.com. For access to this extra information a registration is requested. Free online registration is available.