Complete Set of CAMPUS® Data, ASTM Data, Biopolymer Database, Application Database, Tradename Database, Literature Database, Toolbox.

Material datasheets available free. Online registration at: www.materialdatacenter.com

Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.

This is the free Material Data Center Datasheet of PLEXIGLAS® Hi-Gloss NTA-3 - PMMA - Röhm GmbH

Material Data Center offers the following functions for PLEXIGLAS® Hi-Gloss NTA-3:
unit conversion, PDF datasheet print, comparison with other plastics, snap fit calculation, beam deflection calculation, parameters for material models, CAE Interfaces

Check here, which other Plexiglas datasheets, application examples or technical articles are available in Material Data Center

Use the following short links to get directly to the properties of interest in this datasheet:
Any use of this information falls under the rules of our disclaimer.
Product Texts

Productprofil:

PLEXIGLAS® Hi-Gloss NTA-3 is an impact-modified compound with an increased heat deflection temperature based on polymethylmethacrylate (PMMA).

 

Besides the well-known properties of PLEXIGLAS® molding compound, such as

 

  • good flow
  • high mar resistance
  • good weather resistance
  • good polishability,

 

PLEXIGLAS® Hi-Gloss NTA-3 offers the added benefit of

 

  • increased heat deflection temperature under load.

 

Application:

PLEXIGLAS® Hi-Gloss NTA-3 is particularly suitable for injection molding technical components. Owing to its superior brilliance, high-gloss (Class A) surfaces can be obtained in opaque colors.

Example:

automotive body parts: window channels, pillar panels

Processing:

PLEXIGLAS® Hi-Gloss NTA-3 can be processed on machines with 3-zone general purpose screws for engineering thermoplastics.

Physical Form / Packaging:

PLEXIGLAS® Hi-Gloss NTA-3 compounds are supplied as pellets of uniform size, packaged in 25kg polyethylene bags or in 500kg boxes with PE lining; other packaging on request.

Processing/Physical CharacteristicsValueUnitTest Standard
ISO Data
Melt volume-flow rate, MVR 2 cm³/10min ISO 1133
Temperature 230 °C -
Load 3.8 kg -
Density of melt 1100 kg/m³ -
Ejection temperature 95 °C -
Mechanical propertiesValueUnitTest Standard
ISO Data
Tensile Modulus 2900 MPa ISO 527
Stress at break 60 MPa ISO 527
Strain at break 2.6 % ISO 527
Tensile creep modulus, 1h 2700 MPa ISO 899-1
Tensile creep modulus, 1000h 1700 MPa ISO 899-1
Charpy impact strength, +23°C 16 kJ/m² ISO 179/1eU
Thermal propertiesValueUnitTest Standard
ISO Data
Glass transition temperature, 10°C/min 125 °C ISO 11357-1/-2
Temp. of deflection under load, 1.80 MPa 106 °C ISO 75-1/-2
Temp. of deflection under load, 0.45 MPa 106 °C ISO 75-1/-2
Vicat softening temperature, B 116 °C ISO 306
Coeff. of linear therm. expansion, parallel 75 E-6/K ISO 11359-1/-2
Burning rate, FMVSS, Thickness 1 mm 93.4 mm/min ISO 3795 (FMVSS 302)
Electrical propertiesValueUnitTest Standard
ISO Data
Volume resistivity >1E13 Ohm*m IEC 62631-3-1
Optical propertiesValueUnitTest Standard
ISO Data
Luminous transmittance 0 % ISO 13468-1, -2
Other propertiesValueUnitTest Standard
Water absorption 3 % Sim. to ISO 62
Density 1190 kg/m³ ISO 1183
Test specimen productionValueUnitTest Standard
ISO Data
Injection Molding, melt temperature 240 °C ISO 294
Injection Molding, mold temperature 76 °C ISO 294
Injection Molding, injection velocity 195 mm/s ISO 294
Diagrams
Viscosity-shear rate , PLEXIGLAS® Hi-Gloss NTA-3, PMMA, Röhm
Shearstress-shear rate , PLEXIGLAS® Hi-Gloss NTA-3, PMMA, Röhm
Dynamic Shear modulus-temperature , PLEXIGLAS® Hi-Gloss NTA-3, PMMA, Röhm
Stress-strain , PLEXIGLAS® Hi-Gloss NTA-3, PMMA, Röhm
Secant modulus-strain , PLEXIGLAS® Hi-Gloss NTA-3, PMMA, Röhm
Stress-strain (isochronous) 23°C, PLEXIGLAS® Hi-Gloss NTA-3, PMMA, Röhm
Spec. enthalpy/mass-temp. (DSC) , PLEXIGLAS® Hi-Gloss NTA-3, PMMA, Röhm
Tensile modulus-temperature , PLEXIGLAS® Hi-Gloss NTA-3, PMMA, Röhm
Characteristics
Processing
Injection Molding
Delivery form
Pellets
Special Characteristics
High impact or impact modified, Light stabilized or stable to light, U.V. stabilized or stable to weather, Opaque
Features
High Gloss
Applications
Automotive
Regional Availability
North America, Europe, Asia Pacific, South and Central America, Near East/Africa
Other text information
Injection molding
PREPROCESSING
Predrying temperature: max. 100 °C
Predrying time in a desiccant-type drier: 2 - 3 h
PROCESSING
Melt temperature: 220 - 250°C
Mold temperature:50 - 85°C
Disclaimer
Copyright Altair Engineering GmbH. Altair Engineering GmbH assumes no liability for the system to be free of errors. The user takes sole responsibility for the use of this data under the exclusion of every liability from Altair Engineering GmbH; this is especially valid for claims of compensation resulting from consequential damages. Altair explicitly points out that any decision about the application of materials must be double checked with the producer of this material. This includes all contents of this system. Copyright laws are applicable for the content of this system.
Created: Source: www.materialdatacenter.com


Material Data Center is provided by M-Base Engineering + Software GmbH. M-Base Engineering + Software GmbH assumes no liability for the system to be free of errors. Any decision about the application of materials must be double checked with the producer of this material.

Additional information about this material, like producer contact address, etc. can be found at www.materialdatacenter.com. For access to this extra information a registration is requested. Free online registration is available.