Complete Set of CAMPUSĀ® Data, ASTM Data, Biopolymer Database, Application Database, Tradename Database, Literature Database, Toolbox.

Material datasheets available free. Online registration at: www.materialdatacenter.com

Pentamid B - PA6 - Pentac Polymer GmbH

Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.

A search for "Pentamid B" in Material Data Center leads to the following information:

Tradename: Pentamid B
Family: PA6
Producer: Pentac Polymer GmbH
43 hits in the material database


Material Data Center offers information about the following products with the requested tradename. To view a datasheet, please click on the relevant product.

Datasheet Polymer
PENTAMID B GV40 H natural PA6-GF40
PENTAMID B SK H PA6
PENTAMID B SK H RC black PA6
PENTAMID B L25 H PA6
PENTAMID B L10 H PA6
PENTAMID B E20 H black PA6
PENTAMID B E20 H natural PA6
PENTAMID B GV15 H PA6-GF15
PENTAMID B GV25 H PA6-GF25
PENTAMID B GV30 H PA6-GF30
PENTAMID B GV35 H natural PA6-GF35
PENTAMID B GV35 H black PA6-GF35
PENTAMID B GV40 H black PA6-GF40
PENTAMID B GV30 H RC black PA6-GF30
PENTAMID B S GV30 H PA6-GF30
PENTAMID B S GV50 H PA6-GF50
PENTAMID B S GV60 H PA6-GF60
PENTAMID B GV15 E H PA6-GF15
PENTAMID B GV30 E H PA6-GF30
PENTAMID B GV50 E H natural PA6-GF50
PENTAMID B GV50 E H black PA6-GF50
PENTAMID B GK30 H PA6-GB30
PENTAMID B MK30 H PA6-MX30
PENTAMID B MK40 H natural PA6-MX40
PENTAMID B MK40 H black PA6-MX40
PENTAMID B MK40 E H natural PA6-MX40
PENTAMID B MK40 E H black PA6-MX40
PENTAMID B S GV10 GK20 H black PA6-(GF+GB)30
PENTAMID B S GV10 MC20 H2 black PA6-(GF+MX)30
PENTAMID B H TF25 (PA6+PTFE)
PENTAMID B GV30 H LT black PA6-GF30
PENTAMID B GV30 H LS black PA6-GF30
PENTAMID B GV30 H LS natural PA6-GF30
PENTAMID B GK30 H LS black PA6-GF30
PENTAMID B GK30 H LS natural PA6-GF30
PENTAMID B S GV10 GK20 H LS PA6-(GF+GB)30
PENTAMID B S GV10 MC20 H2 LS black PA6-(GF+MX)30
PENTAMID B S GVB16 H2 black PA6-GB16
PENTAMID B S GV30 H black PA6-GF30
PENTAMID B S GV25 H FR black PA6-GF25
PENTAMID B S GV25 H FR natural PA6-GF25
PENTAMID B S GV30 H FR natural PA6-GF30
PENTAMID B S GV30 H FR black PA6-GF30

Additional information about this tradename, like producer contact address, etc. can be found at www.materialdatacenter.com. For access to this extra information a registration is requested. Free online registration is available.

Note: the information in Material Data Center was collected with maximum care, based on information from material producers. They are subject to short term changes at the market. There is no warranty for the correctness of this information. In no way this information can be seen as a legal advice, whether certain tradenames are protected or not.