Complete Set of CAMPUS® Data, ASTM Data, Biopolymer Database, Application Database, Tradename Database, Literature Database, Toolbox.

Material datasheets available free. Online registration at: www.materialdatacenter.com

Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.

This is the free Material Data Center Datasheet of Monprene® CP-17250 - TPE-X - Teknor Apex Co.

Material Data Center offers the following functions for Monprene® CP-17250:
unit conversion, PDF datasheet print, comparison with other plastics

Check here, which other Monprene datasheets, application examples or technical articles are available in Material Data Center

Use the following short links to get directly to the properties of interest in this datasheet:
Any use of this information falls under the rules of our disclaimer.
Product Texts
Preliminary Data

The Monprene CP-17200 Filled, High Flow Series of thermoplastic elastomer compounds, with good UV resistance, available in NAT or colors, from 40 to 80 Shore A, are designed specifically for EU consumer product applications requiring a soft, rubber-like feel. Monprene CP-17250 is a medium hardness, medium density grade that is suitable for injection molding.

Adheres to PP

PropertyValueUnitStandard
Apparent Viscosity (200 °C, 206 1/s)109
PasASTM D3835
Mechanical propertiesValueUnitTest Standard
ASTM Data
Modulus at 100% Elongation 1.3 MPa ASTM D 412
Modulus at 300% Elongation 0.63 MPa ASTM D 412
Shore A Hardness 50 - ASTM D 2240
Compression Set , 22 hr @ 73 °F 22 % ASTM D 395
Compression Set , 22 hr @ 158 °F 43 % ASTM D 395
Tensile Strength at Break 7.9 MPa ASTM D 412
Elongation at Break 900 % ASTM D 412
Other propertiesValueUnitTest Standard
Density 1050 kg/m³ ISO 1183
Processing Recommendation Injection MoldingValueUnitTest Standard
Pre-drying - Temperature 65 °C -
Pre-drying - Time 2 - 4 h -
Melt temperature 180 - 230 °C -
Mold temperature 15 - 50 °C -
Zone 1 120 - 160 °C -
Zone 2 160 - 230 °C -
Zone 3 180 - 230 °C -
Nozzle temperature 180 - 230 °C -
Screw speed 50 - 100 rpm -
Back pressure 0.5 - 1.5 MPa -
Characteristics
Processing
Injection Molding
Delivery form
Pellets
Additives
Lubricants
Special Characteristics
U.V. stabilized or stable to weather, Opaque
Features
Good Adhesion, Soft Feel
Chemical Resistance
General Chemical Resistance
Regional Availability
North America, Europe, Asia Pacific, South and Central America, Near East/Africa
Disclaimer
Copyright Altair Engineering GmbH. Altair Engineering GmbH assumes no liability for the system to be free of errors. The user takes sole responsibility for the use of this data under the exclusion of every liability from Altair Engineering GmbH; this is especially valid for claims of compensation resulting from consequential damages. Altair explicitly points out that any decision about the application of materials must be double checked with the producer of this material. This includes all contents of this system. Copyright laws are applicable for the content of this system.
Created: Source: www.materialdatacenter.com


Material Data Center is provided by M-Base Engineering + Software GmbH. M-Base Engineering + Software GmbH assumes no liability for the system to be free of errors. Any decision about the application of materials must be double checked with the producer of this material.

Additional information about this material, like producer contact address, etc. can be found at www.materialdatacenter.com. For access to this extra information a registration is requested. Free online registration is available.