Complete Set of CAMPUS® Data, ASTM Data, Biopolymer Database, Application Database, Tradename Database, Literature Database, Toolbox.

Material datasheets available free. Online registration at: www.materialdatacenter.com

Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.

This is the free Material Data Center Datasheet of EXTEM™ Filament AMHH811F - PI - Saudi Basic Industries Corporation (SABIC)

Material Data Center offers the following functions for EXTEM™ Filament AMHH811F:
unit conversion, PDF datasheet print, comparison with other plastics

Check here, which other Extem datasheets, application examples or technical articles are available in Material Data Center

Use the following short links to get directly to the properties of interest in this datasheet:
Any use of this information falls under the rules of our disclaimer.
Product Texts
EXTEM AMHH811F filament is a thermoplastic polyimide (TPI) product for additive manufacturing applications with a glass transition temperature (Tg) of 247 °C. The filament provides high heat resistance and halogen free, thin wall FR capability with a UL94 V-0 listing at 0.75 mm (Blue Cards are available on the UL IQ Database).
Thermal propertiesValueUnitTest Standard
Other Standards[S]
Glass Transition Temperature 247 °C
S: These properties are reported by the producer according standards that are different to our defaults.
Other propertiesValueUnitTest Standard
Density 1300 kg/m³ ISO 1183
Density 1300 kg/m³ ASTM D 792
3D DataValueUnitTest Standard
Other Standards[S]
Tensile modulus, flat 2180 MPa ASTM D 638
Tensile modulus, on-edge 2240 MPa ASTM D 638
Stress at break, flat 48 MPa ASTM D 638
Stress at break, on-edge 47 MPa ASTM D 638
Strain at break, flat 3 % ASTM D 638
Strain at break, on-edge 2.8 % ASTM D 638
Flexural modulus, flat 1920 MPa ASTM D 790
Flexural modulus, on-edge 2220 MPa ASTM D 790
Temp. of deflection under load, 1.80 MPa, flat 230 °C ASTM D 6484
Temp. of deflection under load, 1.80 MPa, on-edge 230 °C ASTM D 6484
Burning Behav. at thickness h, flat V-0 class UL 94
Thickness tested 0.8 mm UL 94
S: These properties are reported by the producer according standards that are different to our defaults.
Characteristics
Processing
Additive Manufacturing
Delivery form
Monofilament
Special Characteristics
Flame retardant, Halogen-free, Heat stabilized or stable to heat
Regional Availability
North America, Europe, South and Central America
Disclaimer
Copyright Altair Engineering GmbH. Altair Engineering GmbH assumes no liability for the system to be free of errors. The user takes sole responsibility for the use of this data under the exclusion of every liability from Altair Engineering GmbH; this is especially valid for claims of compensation resulting from consequential damages. Altair explicitly points out that any decision about the application of materials must be double checked with the producer of this material. This includes all contents of this system. Copyright laws are applicable for the content of this system.
Created: Source: www.materialdatacenter.com


Material Data Center is provided by M-Base Engineering + Software GmbH. M-Base Engineering + Software GmbH assumes no liability for the system to be free of errors. Any decision about the application of materials must be double checked with the producer of this material.

Additional information about this material, like producer contact address, etc. can be found at www.materialdatacenter.com. For access to this extra information a registration is requested. Free online registration is available.