Complete Set of CAMPUS® Data, ASTM Data, Biopolymer Database, Application Database, Tradename Database, Literature Database, Toolbox.

Material datasheets available free. Online registration at: www.materialdatacenter.com

Elastosil - FVMQ, VMQ - Wacker Chemie AG

Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.

A search for "Elastosil" in Material Data Center leads to the following information:

Tradename: Elastosil
Family: FVMQ, VMQ
Producer: Wacker Chemie AG
206 hits in the material database
11 hits in the literature database
3 hits in the application database


Material Data Center offers information about the following products with the requested tradename. To view a datasheet, please click on the relevant product.

Datasheet Polymer
Elastosil® C150 A/B VMQ
Elastosil® FLR 3900/40 A/B FVMQ
Elastosil® FLR 3900/60 A/B FVMQ
Elastosil® FLR 3905/40 A/B FVMQ
Elastosil® FLR 3905/60 A/B FVMQ
Elastosil® LR 3001/55 FR A/B VMQ
Elastosil® LR 3003/03 A/B VMQ
Elastosil® LR 3003/05 A/B VMQ
Elastosil® LR 3003/10 TR A/B VMQ
Elastosil® LR 3003/20 TR A/B VMQ
Elastosil® LR 3003/30 A/B VMQ
Elastosil® LR 3003/40 A/B VMQ
Elastosil® LR 3003/50 A/B VMQ
Elastosil® LR 3003/60 A/B VMQ
Elastosil® LR 3003/70 A/B VMQ
Elastosil® LR 3003/80 A/B VMQ
Elastosil® LR 3003/85 A/B VMQ
Elastosil® LR 3004/30 A/B VMQ
Elastosil® LR 3004/40 A/B VMQ
Elastosil® LR 3004/50 A/B VMQ
Elastosil® LR 3004/60 A/B VMQ
Elastosil® LR 3004/70 A/B VMQ
Elastosil® LR 3005/30 A/B VMQ
Elastosil® LR 3005/40 A/B VMQ
Elastosil® LR 3005/50 A/B VMQ
Elastosil® LR 3005/60 A/B VMQ
Elastosil® LR 3011/50 FR A/B VMQ
Elastosil® LR 3015/70 A/B VMQ
Elastosil® LR 3023/60 A/B VMQ
Elastosil® LR 3040/40 A/B VMQ
Elastosil® LR 3040/50 A/B VMQ
Elastosil® LR 3043/30 A/B VMQ
Elastosil® LR 3043/40 A/B VMQ
Elastosil® LR 3043/50 A/B VMQ
Elastosil® LR 3043/60 A/B VMQ
Elastosil® LR 3043/70 A/B VMQ
Elastosil® LR 3065/30 A/B VMQ
Elastosil® LR 3065/50 A/B VMQ
Elastosil® LR 3066/40 A/B VMQ
Elastosil® LR 3066/60 A/B VMQ
Elastosil® LR 3066/80 A/B VMQ
Elastosil® LR 3070/20 A/B VMQ
Elastosil® LR 3070/30 A/B VMQ
Elastosil® LR 3070/40 A/B VMQ
Elastosil® LR 3070/50 A/B VMQ
Elastosil® LR 3070/60 A/B VMQ
Elastosil® LR 3071/30 A/B VMQ
Elastosil® LR 3071/40 A/B VMQ
Elastosil® LR 3071/50 A/B VMQ
Elastosil® LR 3071/60 A/B VMQ
Elastosil® LR 3072/30 A/B VMQ
Elastosil® LR 3072/40 A/B VMQ
Elastosil® LR 3074/60 A/B VMQ
Elastosil® LR 3076/70 A/B VMQ
Elastosil® LR 3092/65 A/B VMQ
Elastosil® LR 3094/60 A/B VMQ
Elastosil® LR 3153 A/B VMQ
Elastosil® LR 3162 A/B VMQ
Elastosil® LR 3170/40 A/B VMQ
Elastosil® LR 3841/50 A/B VMQ
Elastosil® LR 3842/40 A/B VMQ
Elastosil® LR 3842/50 A/B VMQ
Elastosil® LR 3842/60 A/B VMQ
Elastosil® LR 3842/70 A/B VMQ
Elastosil® LR 3843/30 A/B VMQ
Elastosil® LR 3844/20 A/B VMQ
Elastosil® LR 3844/30 A/B VMQ
Elastosil® LR 3844/40 A/B VMQ
Elastosil® LR 3844/50 A/B VMQ
Elastosil® LR 3846/20 A/B VMQ
Elastosil® LR 3846/30 A/B VMQ
Elastosil® LR 3856/20 A/B VMQ
Elastosil® LR 3856/30 A/B VMQ
Elastosil® LR 6240 A/B VMQ
Elastosil® LR 6255 F VMQ
Elastosil® LR 6260 A/B VMQ
Elastosil® LR 7665 A/B VMQ
Elastosil® LR 8000/10 A/B VMQ
Elastosil® M 1470 VMQ
Elastosil® M 3502 VMQ
Elastosil® M 4370 A/B VMQ
Elastosil® M 4400 VMQ
Elastosil® M 4440 VMQ
Elastosil® M 4470 VMQ
Elastosil® M 4511 VMQ
Elastosil® M 4512 VMQ
Elastosil® M 4514 VMQ
Elastosil® M 4541 VMQ
Elastosil® M 4600 A/B VMQ
Elastosil® M 4601 A/B VMQ
Elastosil® M 4615 A/B VMQ
Elastosil® M 4630 A/B VMQ
Elastosil® M 4635 A/B VMQ
Elastosil® M 4641 A/B VMQ
Elastosil® M 4642 A/B VMQ
Elastosil® M 4643 A/B VMQ
Elastosil® M 4644 A/B VMQ
Elastosil® M 4645 A/B VMQ
Elastosil® M 4670 A/B VMQ
Elastosil® NT 75 VMQ
Elastosil® P 7600 A/B VMQ
Elastosil® P 7670 A/B VMQ
Elastosil® P 7671 A/B VMQ
Elastosil® P 7676 A/B VMQ
Elastosil® P 7684-40 A/B VMQ
Elastosil® P 7684-60 A/B VMQ
Elastosil® P 7950 A/B VMQ
Elastosil® R 101/25 VMQ
Elastosil® R 101/35 VMQ
Elastosil® R 101/45 VMQ
Elastosil® R 101/65 OH VMQ
Elastosil® R 401/30 OH VMQ
Elastosil® R 401/40 VMQ
Elastosil® R 401/50 VMQ
Elastosil® R 401/60 VMQ
Elastosil® R 401/70 VMQ
Elastosil® R 401/80 VMQ
Elastosil® R 420/40 VMQ
Elastosil® R 420/50 VMQ
Elastosil® R 420/60 VMQ
Elastosil® R 420/70 VMQ
Elastosil® R 500/60 VMQ
Elastosil® R 500/70 VMQ
Elastosil® R 501/75 VMQ
Elastosil® R 502/75 VMQ
Elastosil® R 509/65 VMQ
Elastosil® R 510/60 VMQ
Elastosil® R 510/70 VMQ
Elastosil® R 562/80 VMQ
Elastosil® R 570/50 VMQ
Elastosil® R 570/60 VMQ
Elastosil® R 570/70 VMQ
Elastosil® R 6225 Transparent VMQ
Elastosil® R 701/40 VMQ
Elastosil® R 701/50 VMQ
Elastosil® R 701/60 VMQ
Elastosil® R 701/70 VMQ
Elastosil® R 701/80 VMQ
Elastosil® R 750/60 VMQ
Elastosil® R 755/60 VMQ
Elastosil® R 760/70 VMQ
Elastosil® R 770/50 VMQ
Elastosil® R 770/60 VMQ
Elastosil® R 770/75 VMQ
Elastosil® R 805/75 VMQ
Elastosil® R 830/18 VMQ
Elastosil® R 830/45 VMQ
Elastosil® R 831/50 VMQ
Elastosil® R plus 4001/40 VMQ
Elastosil® R plus 4001/50 VMQ
Elastosil® R plus 4001/60 VMQ
Elastosil® R plus 4001/70 VMQ
Elastosil® R plus 4001/80 VMQ
Elastosil® R plus 4020/40 VMQ
Elastosil® R plus 4060/50 VMQ
Elastosil® R plus 4060/60 VMQ
Elastosil® R plus 4066/60 VMQ
Elastosil® R plus 4070/60 VMQ
Elastosil® R plus 4110/60 VP VMQ
Elastosil® R plus 4110/70 VP VMQ
Elastosil® R plus 4305/30 VMQ
Elastosil® R plus 4305/40 VMQ
Elastosil® R plus 4305/50 VMQ
Elastosil® R plus 4305/60 VMQ
Elastosil® R plus 4305/70 VMQ
Elastosil® R plus 4360/60 VMQ
Elastosil® R plus 4366/60 VMQ
Elastosil® R plus 4370/40 VMQ
Elastosil® R plus 4370/50 VMQ
Elastosil® R plus 4806/20 VMQ
Elastosil® R plus 4846/30 VMQ
Elastosil® R plus 533/60 A/B VMQ
Elastosil® R plus 573/50 A/B VMQ
Elastosil® R plus 573/70 A/B VMQ
Elastosil® RD 6600 F VMQ
Elastosil® RT 402 VMQ
Elastosil® RT 426 VMQ
Elastosil® RT 563 VMQ
Elastosil® RT 601 A/B VMQ
Elastosil® RT 602 A/B VMQ
Elastosil® RT 604 A/B VMQ
Elastosil® RT 607 A/B VMQ
Elastosil® RT 620 A/B VMQ
Elastosil® RT 622 A/B VMQ
Elastosil® RT 623 A/B VMQ
Elastosil® RT 629 A/B VMQ
Elastosil® RT 646 A/B VMQ
Elastosil® RT 675 A/B VMQ
Elastosil® RT 685 A/B VMQ
Elastosil® RT 721 A/B VMQ
Elastosil® RT 745 A/B VMQ
Elastosil® RT 772 VMQ
Elastosil® RT 773 VMQ
Elastosil® RT 774 VMQ
Elastosil® RT 778 VMQ
Elastosil® RT K VMQ
Elastosil® SC 835 A/B VMQ
Elastosil® SC 870 A/B VMQ
Elastosil® Solar 2200 A/B VMQ
Elastosil® Solar 3210 A/B VMQ
Elastosil® LR 5040/30 A/B VMQ
Elastosil® LR 5040/40 A/B VMQ
Elastosil® LR 5040/45 A/B VMQ
Elastosil® LR 5040/50 A/B VMQ
Elastosil® LR 5040/60 A/B VMQ
Elastosil® LR 5040/70 A/B VMQ

Additional information about this tradename, like producer contact address, etc. can be found at www.materialdatacenter.com. For access to this extra information a registration is requested. Free online registration is available.

Note: the information in Material Data Center was collected with maximum care, based on information from material producers. They are subject to short term changes at the market. There is no warranty for the correctness of this information. In no way this information can be seen as a legal advice, whether certain tradenames are protected or not.