Complete Set of CAMPUS® Data, ASTM Data, Biopolymer Database, Application Database, Tradename Database, Literature Database, Toolbox.

Material datasheets available free. Online registration at: www.materialdatacenter.com

Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.

This is the free Material Data Center Datasheet of DURACON® ES-5 - POM-CD5 - Polyplastics

Material Data Center offers the following functions for DURACON® ES-5:
unit conversion, PDF datasheet print, comparison with other plastics

Check here, which other Duracon datasheets, application examples or technical articles are available in Material Data Center

Use the following short links to get directly to the properties of interest in this datasheet:
Any use of this information falls under the rules of our disclaimer.
Mechanical propertiesValueUnitTest Standard
ISO Data
Tensile Strength 49 MPa ISO 527-1/-2
Strain at break 7.5 % ISO 527-1/-2
Charpy notched impact strength, +23°C 3 kJ/m² ISO 179/1eA
Flexural modulus, 23°C 2800 MPa ISO 178
Thermal propertiesValueUnitTest Standard
ISO Data
Temp. of deflection under load, 1.80 MPa 109 °C ISO 75-1/-2
Coeff. of linear therm. expansion, parallel 110 E-6/K ISO 11359-1/-2
Coeff. of linear therm. expansion, normal 110 E-6/K ISO 11359-1/-2
Burning behav. at thickness h HB class IEC 60695-11-10
Yellow Card available yes - -
Electrical propertiesValueUnitTest Standard
ISO Data
Volume resistivity 1 Ohm*m IEC 60093
Surface resistivity 500 Ohm IEC 60093
Other propertiesValueUnitTest Standard
ISO Data
Density 1410 kg/m³ ISO 1183
Characteristics
Special Characteristics
Increased electrical conductivity, Anti-static
Features
Copolymer
Regional Availability
Asia Pacific
Disclaimer
Copyright M-Base Engineering+Software GmbH. M-Base Engineering + Software GmbH assumes no liability for the system to be free of errors. The user takes sole responsibility for the use of this data under the exclusion of every liability from M-Base; this is especially valid for claims of compensation resulting from consequential damages. M-Base explicitly points out that any decision about the application of materials must be double checked with the producer of this material. This includes all contents of this system. Copyright laws are applicable for the content of this system.
Created: 2018-02-25 Source: www.materialdatacenter.com


Material Data Center is provided by M-Base Engineering + Software GmbH. M-Base Engineering + Software GmbH assumes no liability for the system to be free of errors. Any decision about the application of materials must be double checked with the producer of this material.

Additional information about this material, like producer contact address, etc. can be found at www.materialdatacenter.com. For access to this extra information a registration is requested. Free online registration is available.