Celstran - TP - Celanese

Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.

A search for "Celstran" in Material Data Center leads to the following information:

Tradename: Celstran
Family: TP
Producer: Celanese
124 hits in the material database
20 hits in the literature database
11 hits in the application database


Material Data Center offers information about the following products with the requested tradename. To view a datasheet, please click on the relevant product.

Datasheet Polymer
CELSTRAN® +PP-GF30-05CN01/10 PP-GLF30
CELSTRAN® +PP-GF30-05CN05/10 PP-GLF30
CELSTRAN® PA6-GF30-01 PA6-GLF30
CELSTRAN® PA66-GF20-02P11/12 PA66-GLF20
CELSTRAN® PA66-GF30-07 PA66-GLF30
CELSTRAN® PA66-GF40-01 PA666-GLF40
CELSTRAN® PA66-GF40-02P11/15 PA66-GLF40
CELSTRAN® PA66-GF40-07 PA66-GLF40
CELSTRAN® PA66-GF50-02 AD3007 PA66-GLF50
CELSTRAN® PA66-GF50-02 P7 PA66-GLF50
CELSTRAN® PA66-GF50-07 PA66-GLF50
CELSTRAN® PA66-GF50-20 AD3007 PA66-GLF50
CELSTRAN® PA66-SF50-02 AF3001 PA66-MEF(x)50
CELSTRAN® PBT-GF40-08 PBT-GLF40
CELSTRAN® PBT-GF50-08 PBT-GLF50
CELSTRAN® PEHD-GF40-01 (PE-HD)-GLF60
CELSTRAN® PP-GF30-0403 P10 PP-GLF30
CELSTRAN® PP-GF30-0403 P10/10 PP-GLF30
CELSTRAN® PP-GF30-0405 P10/10 PP-GLF30
CELSTRAN® PP-GF30-0453 P10/10 PP-GLF30
CELSTRAN® PP-GF30-0501 P8/13 PP-GLF30
CELSTRAN® PP-GF30-0501 P10 PP-GLF30
CELSTRAN® PP-GF30-0501P10/13 PP-GLF30
CELSTRAN® PP-GF30-0553 Black PP-GLF30
CELSTRAN® PP-GF40-0405 P10/10 PP-GLF40
CELSTRAN® PP-GF40-0414 P10 PP-GLF40
CELSTRAN® PP-GF40-0414 P7/10 PP-GLF40
CELSTRAN® PP-GF40-0414 P10/10 PP-GLF40
CELSTRAN® PP-GF50-0403 P10/10 PP-GLF50
CELSTRAN® PP-GF50-0405P10/10 PP-GLF50
CELSTRAN® PP-GF50-0453 P10/10 PP-GLF50
CELSTRAN® PP-GF50-0455 P10/10 PP-GLF50
CELSTRAN® PP-GF50-10 PP-GLF50
CELSTRAN® PP-GF60-0403 P10/10 PP-GLF60
CELSTRAN® PP-GF60-25 AD3002 Black PP-GLF60
CELSTRAN® PPS-CF40-01 PPS-CF40
CELSTRAN® PPS-SF6-01 AF3005 Natural PPS-MEF(x)6...
CELSTRAN® TPU-CF40-01 TPU-CF40
CELSTRAN® +PP-GF40-04CN15 PP-GLF40
CELSTRAN® CFR-TP HDPE GF70-01 (PE-HD)-GF70
CELSTRAN® CFR-TP PA6 CF60-03 PA6-CF60
CELSTRAN® CFR-TP PA6 GF60-03 PA6-GF60
CELSTRAN® CFR-TP PA66 CF60-02 PA66-CF60
CELSTRAN® CFR-TP PA66 GF60-02 PA66-GF60
CELSTRAN® CFR-TP PP GF60-13 PP-GF60
CELSTRAN® CFR-TP PP GF70-13 PP-GF70
CELSTRAN® CFR-TP PPS CF60-01 PPS-CF60
CELSTRAN® PA6-CF40-01 PA6-CF40
CELSTRAN® PA6-GF40-01 AD3002 Black PA6-GLF40
CELSTRAN® PA6-GF50-03 AD3019 Black PA6-GLF50
CELSTRAN® PA66-GF30-02 AD3002 Black PA66-GLF30
CELSTRAN® PA66-GF40-0101P10/11 PA666-GLF40
CELSTRAN® PA66-GF40-02 AD3002 Black PA66-GLF40
CELSTRAN® PA66-GF40-02-Natural PA66-GLF40
CELSTRAN® PA66-GF50-01 PA666-GLF50
CELSTRAN® PA66-GF50-0111P10/11 PA666-GLF50
CELSTRAN® PA66-GF50-0111P7.5/11 PA666-GLF50
CELSTRAN® PA66-GF50-0112P7,5/10 PA666-GLF50
CELSTRAN® PA66-GF50-02 AD3002 Black PA66-GLF50
CELSTRAN® PA66-GF50-02 AD3019 Black PA66-GLF50
CELSTRAN® PA66-GF50-02-Natural PA66-GLF50
CELSTRAN® PA66-GF50-28 AD3020 PA66-GLF50
CELSTRAN® PA66-GF60-0101P10 PA666-GLF60
CELSTRAN® PA66-GF60-02 AD3002 BLACK PA66-GLF60
CELSTRAN® PA66-GF60-02-Natural PA66-GLF60
CELSTRAN® PEHD-GF60-01 (PE-HD)-GLF60
CELSTRAN® POM-GF25-04 AF3001 POM-GLF25
CELSTRAN® PP-GF20-02 Black PP-GLF20
CELSTRAN® PP-GF20-02 Natural PP-GLF20
CELSTRAN® PP-GF20-0453 P10/10 PP-GLF20
CELSTRAN® PP-GF20-0501 Black PP-GLF20
CELSTRAN® PP-GF20-0553 Black PP-GLF20
CELSTRAN® +PP-GF20-05CN05 Black PP-GLF20
CELSTRAN® PP-GF30-02 AD 3002 PP-GLF30
CELSTRAN® PP-GF30-02 AD 3019 PP-GLF30
CELSTRAN® PP-GF30-02 AF 3001 PP-GLF30
CELSTRAN® PP-GF30-03-AD3002 PP-GLF30
CELSTRAN® PP-GF30-0455 P10/10 PP-GLF30
CELSTRAN® PP-GF30-0551 Black PP-GLF30
CELSTRAN® PP-GF40-02 AD3019 Black PP-GLF40
CELSTRAN® PP-GF40-02-Black PP-GLF40
CELSTRAN® PP-GF40-0453 Black PP-GLF40
CELSTRAN® PP-GF40-0455 P10/10 PP-GLF40
CELSTRAN® PP-GF40-20 AD3004 Black PP-GLF40
CELSTRAN® PP-GF50-02- Natural PP-GLF50
CELSTRAN® PP-GF50-02-Black PP-GLF50
CELSTRAN® PP-GF60-02 AD3002 Black PP-GLF60
CELSTRAN® PP-GF60-02 AD3019 PP-GLF60
CELSTRAN® PP-GF60-0403 HF Black PP-GLF60
CELSTRAN® PP-GF60-0453 HF Black PP-GLF60
CELSTRAN® PP-GF60-0453 P10/10 PP-GLF60
CELSTRAN® PPS-AF35-01- PPS-AF35
CELSTRAN® PPS-GF40-01 AD3002 Black PPS-GLF40
CELSTRAN® PPS-GF40-02 AD3002 Black PPS-GLF40
CELSTRAN® PPS-GF50-01 AD3002 Black PPS-GLF50
CELSTRAN® TPU-GF30-01 AD3002 Black TPU-GLF30
CELSTRAN® TPU-GF40-01 AD3002 Black TPU-GLF40
CELSTRAN® TPU-GF50-01 AD3002 Black TPU-GLF50
CELSTRAN®PA66-GF60-02 AD3004 Black PA66-GF60
CELSTRAN® +PP-GF30-04CN02/10 PP-GLF30
CELSTRAN® CFR-TP PPS GF60-01 PPS
CELSTRAN® PA6-GF40-01 AF3001 Natural PA6-GLF40
CELSTRAN® PA6-GF50-01 AF3001 Natural PA6-GLF50
CELSTRAN® PA6-GF60-01 AF3001 Natural PA6-GLF60
CELSTRAN® PA6-GF60-01 P11/10 PA6-GLF60
CELSTRAN® PA66-AF35-01 AF3003 Natural 6MM PA66-AF35
CELSTRAN® PA66-AF35-02 AF3003 Natural PA66-AF35
CELSTRAN® PA66-CF40-02 AF3004 Natural PA66-CF40
CELSTRAN® PA66-GF30-02 AF3001 Natural PA66-GLF30
CELSTRAN® PA66-GF50-02 AF3001 Natural PA66-GLF50
CELSTRAN® PCABS-SF6-05 AF3005 NATURAL PC-MEF(x)6
CELSTRAN® PP-GF20-0553 AD9600R BLACK PP-GLF20
CELSTRAN® PP-GF20-0553 XLE PP-GLF20
CELSTRAN® PP-GF30-0553 XLE PP-GLF30
CELSTRAN® PP-GF40-02 AF3001 NATURAL PP-GLF40
CELSTRAN® PP-GF40-0453 XVA Black PP-GLF40
CELSTRAN® PP-GF40-0455 Soul 4PK Black PP-GLF40
CELSTRAN® PP-GF40-0501 Black PP-GLF40
CELSTRAN® TPU-GF30-01 AF3001 Natural TPU-GLF30
CELSTRAN® TPU-GF40-01 AF3001 Natural TPU-GLF40
CELSTRAN® TPU-GF40-04 AF3001 Natural TPU-GLF40
CELSTRAN® TPU-GF50-01 AF3001 Natural TPU-GLF50
CELSTRAN® TPU-GF60-01 AF3001 Natural TPU-GLF60
CELSTRAN® PA6-GF30/CF20-13 AD3002 Black PA6

Additional information about this tradename, like producer contact address, etc. can be found at www.materialdatacenter.com. For access to this extra information a registration is requested. Free online registration is available.

Note: the information in Material Data Center was collected with maximum care, based on information from material producers. They are subject to short term changes at the market. There is no warranty for the correctness of this information. In no way this information can be seen as a legal advice, whether certain tradenames are protected or not.