Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.

This is the free Material Data Center Datasheet of Bio-Flex® S 5630 WH - (PLA+Copolyester)... - FKuR Kunststoff GmbH

Material Data Center offers the following functions for Bio-Flex® S 5630 WH:
unit conversion, PDF datasheet print, comparison with other plastics, snap fit calculation, beam deflection calculation, CAE Interfaces

Check here, which other Bio-Flex datasheets, application examples or technical articles are available in Material Data Center

Use the following short links to get directly to the properties of interest in this datasheet:
Any use of this information falls under the rules of our disclaimer.
Product Texts
Biodegradable compound suitable for thermoforming and injection moulding.
Processing/Physical CharacteristicsValueUnitTest Standard
ISO Data
Melt flow index, MFI 8.2 g/10min ISO 1133
Temperature 190 °C -
Load 2.16 kg -
Molding shrinkage, parallel 0.5 % ISO 294-4, 2577
Molding shrinkage, normal 0.5 % ISO 294-4, 2577
Mechanical propertiesValueUnitTest Standard
ISO Data
Tensile Modulus 2160 MPa ISO 527
Tensile Strength 32 MPa ISO 527
Yield strain 6 % ISO 527
Stress at break 29 MPa ISO 527
Strain at break 9 % ISO 527
Flexural modulus, 23°C 2400 MPa ISO 178
Charpy impact strength, +23°C 51 kJ/m² ISO 179/1eU
Charpy notched impact strength, +23°C 3 kJ/m² ISO 179/1eA
Thermal propertiesValueUnitTest Standard
ISO Data
Melting temperature, 10°C/min 150 °C ISO 11357-1/-3
Vicat softening temperature, A 105 °C ISO 306
Other propertiesValueUnitTest Standard
Density 1550 kg/m³ ISO 1183
Biobased content 60 % -
Processing Recommendation Injection MoldingValueUnitTest Standard
Pre-drying - Temperature 60 °C -
Pre-drying - Time 2 - 4 h -
Mold temperature 30 - 65 °C -
Zone 1 130 °C -
Zone 2 150 °C -
Zone 3 170 °C -
Nozzle temperature 180 °C -
Maximum residence time 5 min -
Processing Recommendation ExtrusionValueUnitTest Standard
Type of extrusion film - -
Pre-drying - Temperature 60 °C -
Pre-drying - Time 2 - 4 h -
Zone 1 150 °C -
Zone 2 170 °C -
Zone 3 180 °C -
Zone 4 185 °C -
Nozzle temperature 180 °C -
Characteristics
Processing
Injection Molding, Film Extrusion, Thermoforming
Delivery form
Pellets, White
Certifications
Contains renewable resources, Biodegradable, Food contact
Applications
Packaging, Toys
Regional Availability
North America, Europe, Asia Pacific, South and Central America, Near East/Africa
Disclaimer
Copyright Altair Engineering GmbH. Altair Engineering GmbH assumes no liability for the system to be free of errors. The user takes sole responsibility for the use of this data under the exclusion of every liability from Altair Engineering GmbH; this is especially valid for claims of compensation resulting from consequential damages. Altair explicitly points out that any decision about the application of materials must be double checked with the producer of this material. This includes all contents of this system. Copyright laws are applicable for the content of this system.
Created: Source: www.materialdatacenter.com


Material Data Center is provided by M-Base Engineering + Software GmbH. M-Base Engineering + Software GmbH assumes no liability for the system to be free of errors. Any decision about the application of materials must be double checked with the producer of this material.

Additional information about this material, like producer contact address, etc. can be found at www.materialdatacenter.com. For access to this extra information a registration is requested. Free online registration is available.