Bergamid A - PA66 - Avient Corporation

Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.

A search for "Bergamid A" in Material Data Center leads to the following information:

Tradename: Bergamid A
Family: PA66
Producer: Avient Corporation
149 hits in the material database


Material Data Center offers information about the following products with the requested tradename. To view a datasheet, please click on the relevant product.

Datasheet Polymer
BERGAMID® A65 GK15 natur PA66-GB15
BERGAMID® A65 GK15 natur SO PA66-GB15
BERGAMID® A700 PA66
BERGAMID® A700G20U-SO PA66-GF20
BERGAMID® A700G25U-SO PA66-GF25
BERGAMID® A700G30H PA66-GF30
BERGAMID® A700TM-YF PA66
BERGAMID® AB700UF PA666
Bergamid™ A70 G/GK40 H Black PA66-(GF+GB)40
Bergamid™ A70 G10 H BK032 PA66-GF10
Bergamid™ A70 G10 H NC030 PA66-GF10
Bergamid™ A70 G14 TM-X NC060 PA66-GF14
Bergamid™ A70 G15 H BK013 PA66-GF15
Bergamid™ A70 G15 H RAL9005 PA66-GF15
Bergamid™ A70 G15 HW TM-Z PA66-GF15
Bergamid™ A70 G15 U NC PA66-GF15
Bergamid™ A70 G20 H BK014 PA66-GF20
Bergamid™ A70 G25 BK062 PA66-GF25
Bergamid™ A70 G25 H BK709 PA66-GF25
Bergamid™ A70 G25 H natur TM-X PA66-GF25
Bergamid™ A70 G25 H U-SO PA66-GF25
Bergamid™ A70 G25 U-SO TM PA66-GF25
Bergamid™ A70 G30 BK076 ROHS PA66-GF30
Bergamid™ A70 G30 BK181 PA66-GF30
Bergamid™ A70 G30 H BK101 PA66-GF30
Bergamid™ A70 G30 H BL088 PA66-GF30
Bergamid™ A70 G30 H GR086 PA66-GF30
Bergamid™ A70 G30 MOS2 NC721 PA66-GF30
Bergamid™ A70 G30 NC129 PA66-GF30
Bergamid™ A70 G30 U PA66-GF30
Bergamid™ A70 G30 U-S0 BK709 PA66-GF30
Bergamid™ A70 G30 WR NC103 PA66-GF30
Bergamid™ A70 G33 MOS2 BK717 PA66-GF33
Bergamid™ A70 G33 TM-X BK079 PA66-GF33
Bergamid™ A70 G35 H NC010 PA66-GF35
Bergamid™ A70 G35 H U BK SO PA66-GF35
Bergamid™ A70 G35 U BK TM-X SO3 PA66-GF35
Bergamid™ A70 G35 UF SO PA66-GF35
Bergamid™ A70 G40 BK018 PA66-GF40
Bergamid™ A70 G5 T PA66-GF5
Bergamid™ A70 G50 H BK028 PA66-GF50
Bergamid™ A70 G50 HW SO PA66-GF50
Bergamid™ A70 GK30 BK023 PA66-GB30
Bergamid™ A70 GK30 black 13539126 PA66-GB30
Bergamid™ A70 GK30 H PA66-GB30
Bergamid™ A70 GK30 H NC132 PA66-GB30
Bergamid™ A70 H BK126 PA66
Bergamid™ A70 H NC166 PA66
Bergamid™ A70 MI40 H NC017 PA66-MX40
Bergamid™ A70 MOS2 NC062 PA66
Bergamid™ A70 TM-Y H NC121 PA66
Bergamid™ A70 TM-Z BK705 PA66
Bergamid™ A70 TM-Z UV BK171 PA66
Bergamid™ A70 UF Grey VN-3921 PA66
Bergamid™ A70 UF natur V0 PA66
Bergamid™ A70 white PA66
Bergamid™ A70 ZKW PA66
Bergamid™ A700 G10 H (f1) PA66-GF10
Bergamid™ A700 G15 H (f1) PA66-GF15
Bergamid™ A700 G15 H BK017 PA66-GF15
Bergamid™ A700 G15 H NC020 PA66-GF15
Bergamid™ A700 G15 H W UF GN046 PA66-GF15
Bergamid™ A700 G15 H W UF NC059 PA66-GF15
Bergamid™ A700 G15 HW UF PA66-GF15
Bergamid™ A700 G15 U-S0 BK035 PA66-GF15
Bergamid™ A700 G20 H (f1) PA66-GF20
Bergamid™ A700 G20 H WUF BK059 PA66-GF20
Bergamid™ A700 G20 HW UF PA66-GF20
Bergamid™ A700 G20 UF PA66-GF20
Bergamid™ A700 G25 H (f1) PA66-GF25
Bergamid™ A700 G25 HW UF PA66-GF25
Bergamid™ A700 G25 U GR037 PA66-GF25
Bergamid™ A700 G25 U-S0 S01 BK040 PA66-GF25
Bergamid™ A700 G25 U-S01 NC041 PA66-GF25
Bergamid™ A700 G30 H (f1) PA66-GF30
Bergamid™ A700 G30 H BLUE RAL 5013 (F1) PA66-GF30
Bergamid™ A700 G30 H NC121 PA66-GF30
Bergamid™ A700 G30 H RED 3000 (F1) PA66-GF30
Bergamid™ A700 G30 U-S0 BK064 PA66-GF30
Bergamid™ A700 G35 H (f1) PA66-GF35
Bergamid™ A700 G35 U-S0 NC003 PA66-GF35
Bergamid™ A700 G40 H (f1) PA66-GF40
Bergamid™ A700 G45 H (f1) PA66-GF45
Bergamid™ A700 G50 H (f1) PA66-GF50
Bergamid™ A700 G50 H NATURAL PA66-GF50
Bergamid™ A700 Mi/G30 UF PA66-(GF+MX)30
Bergamid™ A700 NC706 PA66
Bergamid™ A80 W20 H UV black SO PA66
Bergamid™ AB70 G40 H UF Natural PA666-GF40
Bergamid™ AB70 MI30 GR012 PA66-MX30
Bergamid™ AB700 UF BK138 PA666
Bergamid™ AB700 UF SO PA666
BERGAMID® A70/75/80 PA66
BERGAMID® A700/750 PA66
BERGAMID® A700G10H PA66-GF10
BERGAMID® A700G10U-SO PA66-GF10
BERGAMID® A700G15H PA66-GF15
BERGAMID® A700G15U-SO PA66-GF15
BERGAMID® A700G20H PA66-GF20
BERGAMID® A700G25H PA66-GF25
BERGAMID® A700G25U PA66-GF25
BERGAMID® A700G30U-SO PA66-GF30
BERGAMID® A700G35H PA66-GF35
BERGAMID® A700G35U-SO PA66-GF35
BERGAMID® A700G40H PA66-GF40
BERGAMID® A700G45H PA66-GF45
BERGAMID® A700G50H PA66-GF50
BERGAMID® A700GK25U-SO PA66-GB25
BERGAMID® A700MI40 PA66-MD40
BERGAMID® A700MOS2 PA66
BERGAMID® A700PM-Y PA66
BERGAMID® A70C10 PA66-CF10
BERGAMID® A70C20 PA66-CF20
BERGAMID® A70G/GK30 PA66-(GF+GB)30
BERGAMID® A70G10 PA66-GF10
BERGAMID® A70G15 PA66-GF15
BERGAMID® A70G15TM-Z PA66-GF15
BERGAMID® A70G15U PA66-GF15
BERGAMID® A70G20 PA66-GF20
BERGAMID® A70G20/GK10H PA66-(GF+GB)30
BERGAMID® A70G25 PA66-GF25
BERGAMID® A70G30 PA66-GF30
BERGAMID® A70G30MOS2 PA66-GF30
BERGAMID® A70G30TF15 PA66-GF30
BERGAMID® A70G30TM-Z PA66-GF30
BERGAMID® A70G35 PA66-GF35
BERGAMID® A70G40 PA66-GF40
BERGAMID® A70G45 PA66-GF45
BERGAMID® A70G50 PA66-GF50
BERGAMID® A70GK15TM-Z PA66-GB15
BERGAMID® A70GK20 PA66-GB20
BERGAMID® A70GK30 PA66-GB30
BERGAMID® A70GK30 MOS2 PA66-GB30
BERGAMID® A70GK35 PA66-GB35
BERGAMID® A70GK40 PA66-GB40
BERGAMID® A70MI20HWTM-X PA66-MD20
BERGAMID® A70MI30 PA66-MD30
BERGAMID® A70MI40 PA66-MD40
BERGAMID® A70MOS2 PA66
BERGAMID® A70PM-Z PA66
BERGAMID® A70TM-X PA66
BERGAMID® A70TM-Y PA66
BERGAMID® A70TM-YF PA66
BERGAMID® A70TM-Z PA66
BERGAMID® A70W25 PA66
BERGAMID® A800H PA66
BERGAMID® AB700G20U PA666-GF20
BERGAMID® AB70MI10U PA666-MD10
BERGAMID® AB70MI20UF PA666-MD20

Additional information about this tradename, like producer contact address, etc. can be found at www.materialdatacenter.com. For access to this extra information a registration is requested. Free online registration is available.

Note: the information in Material Data Center was collected with maximum care, based on information from material producers. They are subject to short term changes at the market. There is no warranty for the correctness of this information. In no way this information can be seen as a legal advice, whether certain tradenames are protected or not.