Any use of this information falls under the rules of our
disclaimer.
Product Texts
Product description:
Phenolic moulding compound, inorganically/organically filled, glass fibre reinforced, increased heat resistance, hot steam and hot water resistant (Not suitable for use of higher voltage).
Application areas:
Fittings for ovens and dishwashers, medium heat resistant cookware fittings.
Property Name |
Value |
Unit |
Standard No. |
---|
Apparent density (moulding compound) |
0.78 |
g/cm³ |
ISO 60 |
Moulding shrinkage (injection moulding, longitudinal) |
0.6 |
% |
ISO 2577 |
Post shrinkage (injection moulding, 168h/110°C) |
0.3 |
% |
ISO 2577 |
Compr. strength (test spec. flat tested) |
200 |
MPa |
ISO 604 |
Flexural strength (2mm/min) |
90 |
MPa |
ISO 178 |
Flexural modulus |
8500 |
MPa |
ISO 178 |
Ball indentation hardness (H 961/30) |
350 |
MPa |
ISO 2039/P1 |
Water absorption (24h/23°C) |
20 |
mg |
similar to ISO 62 |
Additional characteristics: |
high surface quality, resistant to high temperature, dishwasher prrof
|
Preparation of Test Specimens of Thermosetting Moulding Compound
- Compression to ISO 295
- Injection to ISO 10724
Storage capability
2 years (relative humidity of 50-60% and maximum storage temperature of approximately 20°C)
Processing/Physical Characteristics | Value | Unit | Test Standard |
ISO Data |
Molding shrinkage, parallel |
0.6 |
% |
ISO 294-4, 2577 |
Mechanical properties | Value | Unit | Test Standard |
ISO Data |
Charpy impact strength, +23°C |
6 |
kJ/m² |
ISO 179/1eU |
Charpy notched impact strength, +23°C |
1.8 |
kJ/m² |
ISO 179/1eA |
Thermal properties | Value | Unit | Test Standard |
ISO Data |
Temp. of deflection under load, 8.00 MPa |
140 |
°C |
ISO 75-1/-2 |
Electrical properties | Value | Unit | Test Standard |
ISO Data |
Relative permittivity, 100Hz |
12 |
- |
IEC 62631-2-1 |
Dissipation factor, 100Hz |
0.15 |
E-4 |
IEC 62631-2-1 |
Volume resistivity |
1E9 |
Ohm*m |
IEC 62631-3-1 |
Surface resistivity |
1E10 |
Ohm |
IEC 62631-3-2 |
Electric strength |
5 |
kV/mm |
IEC 60243-1 |
Other properties | Value | Unit | Test Standard |
Density |
1520 |
kg/m³ |
ISO 1183 |
Test specimen production | Value | Unit | Test Standard |
ISO Data |
Injection Molding, injection temperature |
115 |
°C |
ISO 10724 |
Injection Molding, injection velocity |
170 |
mm/s |
ISO 10724 |
Injection Molding, hold pressure |
100 |
MPa |
ISO 10724 |
Injection Molding, cure time |
25 |
min |
ISO 10724 |
Compression Molding, mold temperature |
160 |
°C |
ISO 295 |
Compression Molding, cure time |
1 |
min |
ISO 295 |
Characteristics
Processing
Injection Molding, Transfer Molding
Regional Availability
Other text information
Injection molding
VERARBEITUNG
Temperature of material: |
80 - 100 |
°C |
Mould temperature: |
160 - 190 |
°C |
Curing time: |
10-20 |
sec |
|
Further Information: |
Barrel temperature |
- Feed zone: |
60-75 |
°C |
- Nozzle zone: |
80-100 |
°C |
Cavity moulding pressure: |
>15 |
MPa |
Back pressure: |
0.5-2 |
MPa |
Holding pressure: |
60% of injection pressure |
Compression molding
PROCESSING
Mould temperature: | 160-190 | °C |
Curing time: | 20-40 | sec |
Cavity moulding pressure: | >15 | MPa |
Disclaimer
Copyright Altair Engineering GmbH. Altair Engineering GmbH assumes no liability for the system to be free of errors. The user takes sole responsibility for the use of this data under the exclusion of every liability from Altair Engineering GmbH; this is especially valid for claims of compensation resulting from consequential damages. Altair explicitly points out that any decision about the application of materials must be double checked with the producer of this material. This includes all contents of this system. Copyright laws are applicable for the content of this system.