Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.

A search for "Badatron" in Material Data Center leads to the following information:

Tradename: Badatron
Family: PPS
Producer: Bada AG
10 hits in the material database


Material Data Center offers information about the following products with the requested tradename. To view a datasheet, please click on the relevant product.

Datasheet Polymer
Badatron® PPS CF10 GR10 PPS-(CF+CD)20
Badatron® PPS CF20 S3 PPS-CF20
Badatron® PPS CF30 LG PPS-CF30
Badatron® PPS GF30 LG WL PPS-GF30
Badatron® PPS GF30 LG PPS-GF30
Badatron® PPS GF30 TF 20 LG (PPS+PTFE)-GF30
Badatron® PPS GF40 LG S2 PPS-GF40
Badatron® PPS GF40 TF5 (PPS+PTFE)-GF40
Badatron® PPS GF40 PPS-GF40
Badatron® PPS GF/M65 PPS-(GF+MD)65

Additional information about this tradename, like producer contact address, etc. can be found at www.materialdatacenter.com. For access to this extra information a registration is requested. Free online registration is available.

Note: the information in Material Data Center was collected with maximum care, based on information from material producers. They are subject to short term changes at the market. There is no warranty for the correctness of this information. In no way this information can be seen as a legal advice, whether certain tradenames are protected or not.