Complete Set of CAMPUS® Data, ASTM Data, Biopolymer Database, Application Database, Tradename Database, Literature Database, Toolbox.

Material datasheets available free. Online registration at: www.materialdatacenter.com

Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.

This is the free Material Data Center Datasheet of VESTAPE® PA12-CF45 20641 - PA12-CF45 - Evonik Operations GmbH

Material Data Center offers the following functions for VESTAPE® PA12-CF45 20641:
unit conversion, PDF datasheet print, comparison with other plastics

Check here, which other Vestape datasheets, application examples or technical articles are available in Material Data Center

Use the following short links to get directly to the properties of interest in this datasheet:
Any use of this information falls under the rules of our disclaimer.
材料文字说明
HT carbon fiber reinforced UD-tape made from polyamide 12 

VESTAPE® PA12-CF45 is an unidirectional carbon fiber reinforced tape made from PA12 with a fiber volume content of 45 %, that shows a high chemical resistance, low water absorption and steady mechanical properties over a wide temperature range.

VESTAPE® PA12-CF45  is supplied as a band-shaped semi-finished product showing a width of 160 mm and a thickness of 0,25 mm.


Further information about the properties and the processing of VESTAPE® can be found in our brochure „VESTAPE“.
 


FOR FURTHER INFORMATION PLEASE CONTACT US AT EVONIK-HP@EVONIK.COM OR VISIT OUR PRODUCTS AT COMPOSITES.EVONIK.COM.
热性能价值单位Test Standard
ISO数据
熔融温度, 10°C/min 178 °C ISO 11357-1/-3
玻璃化转变温度, 10°C/min 40 °C ISO 11357-1/-2
其它性能价值单位Test Standard
吸湿性 0.47 % 类似ISO 62
密度 1360 kg/m³ ISO 1183
试样制备条件价值单位Test Standard
ISO数据
模具表面温度, of test plate 220 °C -
保压时间, of test plate 5 min -
冷却速度, of test plate 20 K/min -
脱模温度, of test plate 40 °C -
成型压力, of test plate 1 MPa -
典型数据
加工方法
热成型
供货形式
Tape
特殊性能
提高导电性, 经热稳处理的/耐热的
耐化学试剂
通用耐化学性
地区供应
权利义务的法律声明
Copyright Altair Engineering GmbH. Altair Engineering GmbH assumes no liability for the system to be free of errors. The user takes sole responsibility for the use of this data under the exclusion of every liability from Altair Engineering GmbH; this is especially valid for claims of compensation resulting from consequential damages. Altair explicitly points out that any decision about the application of materials must be double checked with the producer of this material. This includes all contents of this system. Copyright laws are applicable for the content of this system.
Created: Source: www.materialdatacenter.com


Material Data Center is provided by M-Base Engineering + Software GmbH. M-Base Engineering + Software GmbH assumes no liability for the system to be free of errors. Any decision about the application of materials must be double checked with the producer of this material.

Additional information about this material, like producer contact address, etc. can be found at www.materialdatacenter.com. For access to this extra information a registration is requested. Free online registration is available.