Complete Set of CAMPUS® Data, ASTM Data, Biopolymer Database, Application Database, Tradename Database, Literature Database, Toolbox.

Material datasheets available free. Online registration at: www.materialdatacenter.com

Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.

This is the free Material Data Center Datasheet of Panlite® LV-2250Y - PC - Teijin Chemicals Ltd.

Material Data Center offers the following functions for Panlite® LV-2250Y:
unit conversion, PDF datasheet print, comparison with other plastics, snap fit calculation, beam deflection calculation, CAE Interfaces

Check here, which other Panlite datasheets, application examples or technical articles are available in Material Data Center

Use the following short links to get directly to the properties of interest in this datasheet:
Any use of this information falls under the rules of our disclaimer.
Características de processamento/físicasValorUnidadeMétodo de ensaio
ISO Dados
Índice de fluidez volumétrico, MVR 8 cm³/10min ISO 1133
Temperatura 300 °C -
Carga 1.2 kg -
ASTM Dados
Contração após a moldagem, paralelo 0.006 mm/mm ASTM D 955
Contração após a moldagem, perpendicular 0.006 mm/mm ASTM D 955
Propriedades mecânicasValorUnidadeMétodo de ensaio
ISO Dados
Módulo de tração 2400 MPa ISO 527
Tensão no escoamento 61 MPa ISO 527
Deformação no escoamento 6 % ISO 527
Deformação nominal na ruptura >50 % ISO 527
Módulo de flexão, 23°C 2300 MPa ISO 178
Resistência à flexão 91 MPa ISO 178
Resistência ao impacto Charpy, +23°C N kJ/m² ISO 179/1eU
Res. impacto Charpy c/entalhe, +23°C 76 kJ/m² ISO 179/1eA
ASTM Dados
Módulo de tração 2120 MPa ASTM D 638
Resistência à tração no escoamento 61 MPa ASTM D 638
Resistência à tração na ruptura 81 MPa ASTM D 638
Alongamento no escoamento 6 % ASTM D 638
Deformação na ruptura 140 % ASTM D 638
Resistência à compressão 76 MPa ASTM D 695
Módulo de flexão 2230 MPa ASTM D 790
Resistência à flexão 90 MPa ASTM D 790
Dureza Rockwell M 77 - ASTM D 785
Impacto Izod com entalhe, 1/8 in 880 J/m ASTM D 256
Impacto Izod com entalhe, 1/4 in 140 J/m ASTM D 256
Propriedades térmicasValorUnidadeMétodo de ensaio
ISO Dados
Temperatura de deflexão térmica, 1.80 MPa 129 °C ISO 75-1/-2
Temperatura de deflexão térmica , 0.45 MPa 142 °C ISO 75-1/-2
Temperatura de amolecimento Vicat, B 149 °C ISO 306
Coef. de expansão térmica linear, paralelo 70 E-6/K ISO 11359-1/-2
Coef. de expansão térmica linear, perpend. 70 E-6/K ISO 11359-1/-2
Flamabilidade a 1.5mm esp. nom. V-2 class IEC 60695-11-10
Espessuras do tubo de teste 1.5 mm -
Flamabilidade a espessura h V-2 class IEC 60695-11-10
Espessuras do tubo de teste 0.4 mm -
Glow Wire Flammability Index (GWFI) 875 °C IEC 60695-2-12
GWFI - thickness tested (1) 1.5 mm -
Glow Wire Flammability Index (GWFI) 960 °C IEC 60695-2-12
GWFI - thickness tested (2) 3 mm -
Glow Wire Ignition Temperature (GWIT) 850 °C IEC 60695-2-13
GWIT - thickness tested (1) 1.5 mm -
Glow Wire Ignition Temperature (GWIT) 875 °C IEC 60695-2-13
GWIT - thickness tested (2) 3 mm -
ASTM Dados
UL94 flamabilidade V-2 - UL 94
Espessuras do tubo de teste 3 mm -
Coeficiente de expansão térmica, long. 70 E-6/K ASTM D 696
Coef.de expansão térmica, trans. 70 E-6/K ASTM D 696
Propriedades elétricasValorUnidadeMétodo de ensaio
ISO Dados
Constante dielétrica, 100Hz 3.1 - IEC 62631-2-1
Constante dielétrica, 1MHz 3 - IEC 62631-2-1
Fator de dissipação dielétrica, 100Hz 10 E-4 IEC 62631-2-1
Fator de dissipação dielétrica, 1MHz 90 E-4 IEC 62631-2-1
Resistividade volumétrica específica >1E13 Ohm*m IEC 62631-3-1
Resistividade superficial específica >1E15 Ohm IEC 62631-3-2
Resistência elétrica 30 kV/mm IEC 60243-1
Índice comparativo de linha de fuga 250 - IEC 60112
ASTM Dados
Resistência elétrica, tempo curto 30 kV/mm ASTM D 149
Fator de dissipação dielétrica, 60 Hz 0.0004 - ASTM D 150
Fator de dissipação dielétrica, 1 MHz 0.009 - ASTM D 150
Constante dielétrica, 60 Hz 2.95 - ASTM D 150
Constante dielétrica, 1 MHz 2.9 - ASTM D 150
Resistividade volumétrica específica 3E16 Ohm*cm ASTM D 257
Resistência ao arco 110 s ASTM D 495
Propriedades ópticasValorUnidadeMétodo de ensaio
ASTM Dados
Transmitância luminosa 88 % ASTM D 1003
Índice de refração 1.58 - ASTM D 542
Outras propriedadesValorUnidadeMétodo de ensaio
Densidade 1200 kg/m³ ISO 1183
Absorção de água, equilíbrio 0.2 % ASTM D 570
Recomendação de processamento Moldagem por injeçãoValorUnidadeMétodo de ensaio
Pré-secagem - temperatura 120 °C -
Pré-secagem - tempo >5 h -
Temperatura da massa 270 - 320 °C -
Temperatura do molde 80 - 120 °C -
Características
Processamento
Moldagem por injeção
Forma de entrega
Granulos
Aditivos
Desmoldante
Características especiais
Transparente
Aplicaciones
Polivalente
Disponibilidade regional
América do Norte, Europa, Ásia Pacífico, America Centra e do Sul, Oriente/África
Disclaimer
Copyright Altair Engineering GmbH. Altair Engineering GmbH assumes no liability for the system to be free of errors. The user takes sole responsibility for the use of this data under the exclusion of every liability from Altair Engineering GmbH; this is especially valid for claims of compensation resulting from consequential damages. Altair explicitly points out that any decision about the application of materials must be double checked with the producer of this material. This includes all contents of this system. Copyright laws are applicable for the content of this system.
Created: Source: www.materialdatacenter.com


Material Data Center is provided by M-Base Engineering + Software GmbH. M-Base Engineering + Software GmbH assumes no liability for the system to be free of errors. Any decision about the application of materials must be double checked with the producer of this material.

Additional information about this material, like producer contact address, etc. can be found at www.materialdatacenter.com. For access to this extra information a registration is requested. Free online registration is available.