Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.

This is the free Material Data Center Datasheet of SABIC® PC Resin PC1803R - PC - Saudi Basic Industries Corporation (SABIC)

Material Data Center offers the following functions for SABIC® PC Resin PC1803R:
unit conversion, PDF datasheet print, comparison with other plastics, snap fit calculation, beam deflection calculation, CAE Interfaces

Check here, which other Sabic datasheets, application examples or technical articles are available in Material Data Center

Use the following short links to get directly to the properties of interest in this datasheet:
Any use of this information falls under the rules of our disclaimer.
제품 설명서
PC1803R resin is a medium-high flow (MFR = 18 at 300?C/1.2kg), heat and UV stabilized, polycarbonate product with mold release designed for use in the general purpose molding market.
Processing/Physical Characteristics단위시험규격
ISO 데이터
용융 부피 - 흐름 속도, MVR 17 cm³/10min ISO 1133
온도 300 °C -
하중 1.2 kg -
ASTM 데이터
용융 흐름성, MFI 18 g/10min ASTM D 1238
온도 300 °C -
하중 1.2 kg -
기계적 특성단위시험규격
ISO 데이터
인장탄성률 2350 MPa ISO 527
항복강도 63 MPa ISO 527
항복변형률 6 % ISO 527
파단시 신율 50 % ISO 527
굴곡 계수 2300 MPa ISO 178
로크웰 경도 R 120 - ISO 2039-2
ASTM 데이터
인장탄성률 2350 MPa ASTM D 638
항복강도 63 MPa ASTM D 638
항복변형률 6 % ASTM D 638
파단시 신율 70 % ASTM D 638
굴곡 계수 2300 MPa ASTM D 790
로크웰 경도 R 120 - ASTM D 785
아이조드 충격은 노치, 1/8 in 700 J/m ASTM D 256
Izod충격강도, 1/8 in N J/m ASTM D 256
열적 특성단위시험규격
ISO 데이터
하중하에서의 변형온도, 1.80 MPa 124 °C ISO 75-1/-2
하중하에서의 변형온도, 0.45 MPa 135 °C ISO 75-1/-2
비카트 연화 온도, B 141 °C ISO 306
1.5mm 평균두께에서의 난연성 V-2 class IEC 60695-11-10
테스트 두께 1.6 mm -
열전도율 0.2 W/(m K) DIN 52616
ASTM 데이터
DTUL @ 66 psi 135 °C ASTM D 648
DTUL @ 264 psi 124 °C ASTM D 648
비카트 연화 온도 141 °C ASTM D 1525
열전도율, 솔리드 0.0288 W/(m K) ASTM C 177
전기적 특성단위시험규격
ISO 데이터
상대 유전뮬, 1MHz 3 - IEC 62631-2-1
소산 인자, 100Hz 10 E-4 IEC 62631-2-1
소산 인자, 1MHz 100 E-4 IEC 62631-2-1
부피 저항 >1E13 Ohm*m IEC 62631-3-1
전기 압력 27 kV/mm IEC 60243-1
ASTM 데이터
전기 압력, 단기간의 27 kV/mm ASTM D 149
소산 인자, 60 Hz 0.001 - ASTM D 150
소산 인자, 1 MHz 0.01 - ASTM D 150
상대 유전율, 60 Hz 3 - ASTM D 150
상대 유전율, 1 MHz 3 - ASTM D 150
부피 저항 1E15 Ohm*cm ASTM D 257
광학 특성단위시험규격
ASTM 데이터
탁도 0.8 % ASTM D 1003
광선 투겠淅 90 % ASTM D 1003
굴절 지수 1.59 - ASTM D 542
기타 특성단위시험규격
물에서의 흡수성 0.35 % ISO 62와 유사
물에서의 흡수성, 평형 0.35 % ASTM D 570
밀도 1200 kg/m³ ASTM D 792
Bulk Density 1.2 kg/m³ -
Processing Recommendation Injection Molding단위시험규격
Pre-drying - Temperature ≤120 °C -
Pre-drying - Time 2 - 4 h -
용융수지온도 280 - 300 °C -
성형온도 80 - 100 °C -
Zone 1 260 - 280 °C -
Zone 2 270 - 290 °C -
Zone 3 280 - 300 °C -
Nozzle temperature 270 - 290 °C -
특징
특별 특성
U.V. 안정성 또는 기후 안정성
Disclaimer
Copyright Altair Engineering GmbH. Altair Engineering GmbH assumes no liability for the system to be free of errors. The user takes sole responsibility for the use of this data under the exclusion of every liability from Altair Engineering GmbH; this is especially valid for claims of compensation resulting from consequential damages. Altair explicitly points out that any decision about the application of materials must be double checked with the producer of this material. This includes all contents of this system. Copyright laws are applicable for the content of this system.
Created: Source: www.materialdatacenter.com


Material Data Center is provided by M-Base Engineering + Software GmbH. M-Base Engineering + Software GmbH assumes no liability for the system to be free of errors. Any decision about the application of materials must be double checked with the producer of this material.

Additional information about this material, like producer contact address, etc. can be found at www.materialdatacenter.com. For access to this extra information a registration is requested. Free online registration is available.