Complete Set of CAMPUS® Data, ASTM Data, Biopolymer Database, Application Database, Tradename Database, Literature Database, Toolbox.

Material datasheets available free. Online registration at: www.materialdatacenter.com

Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.

This is the free Material Data Center Datasheet of Delrin® 500AL NC010 - POM-Z - DuPont Engineering Polymers

Material Data Center offers the following functions for Delrin® 500AL NC010:
unit conversion, PDF datasheet print, comparison with other plastics, snap fit calculation, beam deflection calculation, parameters for material models, CAE Interfaces

Check here, which other Delrin datasheets, application examples or technical articles are available in Material Data Center

Use the following short links to get directly to the properties of interest in this datasheet:
Any use of this information falls under the rules of our disclaimer.
제품 설명서
Common features of Delrin® acetal resins include mechanical and physical properties such as high mechanical strength and rigidity, excellent fatigue and impact resistance, as well as resistance to moisture, gasoline, lubricants, solvents, and many other neutral chemicals. Delrin® acetal resins also have excellent dimensional stability and good electrical insulating characteristics. They are naturally resilient, self-lubricating, and available in a variety of colors and speciality grades.

Delrin® acetal resin typically is used in demanding applications in the automotive, domestic appliances, sports, industrial engineering, electronics, and consumer goods industries.

Delrin® 500AL is a medium viscosity acetal homopolymer containing an advanced system of lubrication designed for low wear, low friction, and low noise against metals and plastics.
Processing/Physical Characteristics단위시험규격
ISO 데이터
용융 부피 - 흐름 속도, MVR 12 cm³/10min ISO 1133
온도 190 °C -
하중 2.16 kg -
성형 수축률, 평행 1.8 % ISO 294-4, 2577
성형 수축률, 수직 1.7 % ISO 294-4, 2577
ASTM 데이터
용융 흐름성, MFI 6 g/10min ASTM D 1238
온도 190 °C -
하중 1.05 kg -
성형 수축률, 평행 0.0185 mm/mm ASTM D 955
성형 수축률, 수직 0.0185 mm/mm ASTM D 955
기계적 특성단위시험규격
ISO 데이터
인장탄성률 3100 MPa ISO 527
항복강도 66 MPa ISO 527
항복변형률 11 % ISO 527
파단시 평균신율 23 % ISO 527
탄성변형률, 1h 2400 MPa ISO 899-1
탄성변형률, 1000h 1600 MPa ISO 899-1
챠피 충격 강도 , +23°C 160 kJ/m² ISO 179/1eU
챠피 충격 강도, -30°C 130 kJ/m² ISO 179/1eU
챠피 노치드 충격 강도, +23°C 7 kJ/m² ISO 179/1eA
챠피 노치드 충격 강도, -30°C 6 kJ/m² ISO 179/1eA
ASTM 데이터
인장탄성률 3170 MPa ASTM D 638
인장 강도 66 MPa ASTM D 638
항복강도 66 MPa ASTM D 638
항복변형률 10 % ASTM D 638
파단시 신율 30 % ASTM D 638
굴곡 계수 2970 MPa ASTM D 790
굴곡 강도 88 MPa ASTM D 790
아이조드 충격은 노치, 1/8 in 58 J/m ASTM D 256
열적 특성단위시험규격
ISO 데이터
녹는점, 10°C/min 178 °C ISO 11357-1/-3
하중하에서의 변형온도, 1.80 MPa 97 °C ISO 75-1/-2
하중하에서의 변형온도, 0.45 MPa 164 °C ISO 75-1/-2
선형 열팽창 계수, 평행 120 E-6/K ISO 11359-1/-2
선형 열팽창 계수, 수직 120 E-6/K ISO 11359-1/-2
1.5mm 평균두께에서의 난연성 HB class IEC 60695-11-10
테스트 두께 1.5 mm -
Yellow Card 유효한 - -
두께 H인 제품의 난연성 HB class IEC 60695-11-10
테스트 두께 0.8 mm -
Yellow Card 유효한 - -
ASTM 데이터
UL94 난연성 HB - UL 94
테스트 두께 1.5 mm -
열팽창 계수, 평행 118 E-6/K ASTM D 696
열팽창 계수, 수직 116 E-6/K ASTM D 696
DTUL @ 66 psi 169 °C ASTM D 648
DTUL @ 264 psi 108 °C ASTM D 648
녹는점 178 °C ASTM D 3418
전기적 특성단위시험규격
ASTM 데이터
전기 압력, 단기간의 17.7 kV/mm ASTM D 149
소산 인자, 1 MHz 0.006 - ASTM D 150
상대 유전율, 1 MHz 3.6 - ASTM D 150
표면 저항 >1E15 Ohm ASTM D 257
부피 저항 7E14 Ohm*cm ASTM D 257
기타 특성단위시험규격
조건에서의 흡습성 0.3 % ISO 62와 유사
밀도 1390 kg/m³ ISO 1183
밀도 1390 kg/m³ ASTM D 792
도표
점도-변형률 , Delrin® 500AL NC010, POM-Z, DuPont
전단-변형률 , Delrin® 500AL NC010, POM-Z, DuPont
응력-신율 , Delrin® 500AL NC010, POM-Z, DuPont
시컨트탄성율-신율 , Delrin® 500AL NC010, POM-Z, DuPont
특징
생산 공정
사출 성형
인도 유형
펠렛 (입자,알갱이), 자연 색상
부가물
윤활제, 이형제
특성
Creep Resistance, Tribologic Grade, Weldable, Homopolymer
지역별 검색
기타 정보
사E성
Drying is recommended, but not necessary for newly opened packaging stored in a dry location.
Follow the drying guidelines above in the following cases:

·         If moisture is above the Processing Moisture Content recommendation,

·         When a resin container is damaged,

·         When the material is not properly stored in a dry place at room temperature, or

·         When packaging stays open for a significant time.

화학적 매체에 대한 저항력
에서의 아세트산 (질량 5%) (23°C)
23 °C에서의 시트르산 용액 (질량 10%) (23°C)
23 °C에서의 락트산 (질량 10%) (23°C)
에서의 염산 (질량 36%) (23°C)
23 °C에서의 질산 (질량 40%) (23°C)
에서의 황산 (질량 38%) (23°C)
에서의 황산 (질량 5%) (23°C)
에서의 크롬산 용액 (질량 40%) (23°C)
염기
에서의 수산화나트륨 용액 (질량 35%) (23°C)
에서의 수산화나트륨 용액 (질량 1%) (23°C)
에서의 수산화암모늄 용액 (질량 10%) (23°C)
알코올
23 °C에서의 이소프로필 알코올 (23°C)
23 °C에서의 메탄올 (23°C)
23 °C에서의 에탄올 (23°C)
탄화수소
에서의 n-헥산 (23°C)
에서의 톨루엔 (23°C)
에서의 이소옥탄 (23°C)
케톤
에서의 아세톤 (23°C)
에테르
에서의 디에틸 에테르 (23°C)
광유
에서의 SAE 10W40 멀티그레이드 모터 오일 (23°C)
에서의 SAE 10W40 멀티그레이드 모터 오일 (130°C)
에서의 SAE 80/90 하이포이드 기어 오일 (130°C)
에서의 절연유 (23°C)
표준 연료
에서의 ISO 1817 액체 1 (60°C)
에서의 ISO 1817 액체 2 (60°C)
60 °C에서의 ISO 1817 액체 3 (60°C)
에서의 ISO 1817 액체 4 (60°C)
에서의 무알코올 표준 연료 (ISO 1817 액체 C 참조) (23°C)
에서의 알코올성 표준 연료 (ISO 1817 액체 4 참조) (23°C)
에서의 디젤 연료 (ISO 1817 액체 F 참조) (23°C)
에서의 디젤 연료 (ISO 1817 액체 F 참조) (90°C)
에서의 디젤 연료 (ISO 1817 액체 F 참조) (>90°C)
염액
에서의 염화나트륨 용액 (질량 10%) (23°C)
에서의 차아염소산나트륨 용액 (질량 10%) (23°C)
에서의 탄산나트륨 용액 (질량 20%) (23°C)
에서의 탄산나트륨 용액 (질량 2%) (23°C)
에서의 염화아연 용액 (질량 50%) (23°C)
기타
에서의 초산 에틸 (23°C)
에서의 과산화수소 (23°C)
에서의 DOT No. 4 브레이크 오일 (130°C)
에서의 에틸렌 글리콜 수용액 (질량 50%) (108°C)
에서의 노닐페녹시-폴리에틸레녹시 에탄올 1% 수용액 (23°C)
에서의 50% 올레산 + 50% 올리브 오일 (23°C)
에서의 물 (23°C)
에서의 탈이온수 (90°C)
에서의 페놀 용액 (질량 5%) (23°C)
Disclaimer
Copyright Altair Engineering GmbH. Altair Engineering GmbH assumes no liability for the system to be free of errors. The user takes sole responsibility for the use of this data under the exclusion of every liability from Altair Engineering GmbH; this is especially valid for claims of compensation resulting from consequential damages. Altair explicitly points out that any decision about the application of materials must be double checked with the producer of this material. This includes all contents of this system. Copyright laws are applicable for the content of this system.
Created: Source: www.materialdatacenter.com


Material Data Center is provided by M-Base Engineering + Software GmbH. M-Base Engineering + Software GmbH assumes no liability for the system to be free of errors. Any decision about the application of materials must be double checked with the producer of this material.

Additional information about this material, like producer contact address, etc. can be found at www.materialdatacenter.com. For access to this extra information a registration is requested. Free online registration is available.