Complete Set of CAMPUS® Data, ASTM Data, Biopolymer Database, Application Database, Tradename Database, Literature Database, Toolbox.

Material datasheets available free. Online registration at: www.materialdatacenter.com

Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.

This is the free Material Data Center Datasheet of VALOX™ FR Resin ENH4530 - Americas - PBT-GF15 - Saudi Basic Industries Corporation (SABIC)

Material Data Center offers the following functions for VALOX™ FR Resin ENH4530 - Americas:
unit conversion, PDF datasheet print, comparison with other plastics, snap fit calculation, beam deflection calculation, CAE Interfaces

Check here, which other Valox datasheets, application examples or technical articles are available in Material Data Center

Use the following short links to get directly to the properties of interest in this datasheet:
Any use of this information falls under the rules of our disclaimer.
商品の説明文
VALOX ENH4530 is a 15% glass reinforced, non-chlorinated/brominated flame retardant Polybutylene Terephthalate (PBT) injection moldable grade with excellent chemical resistance. It has a UL94V0@0.80mm flame rating. This is a good candidate for a variety of applications needing a sustainable FR PBT solution.
Processing/Physical Characteristics単位テスト基準
ISO データ
メルトボリュームレイト, MVR 18 cm³/10min ISO 1133
温度 265 °C -
荷重 5 kg -
ASTM数据
メルトフローレイト, MFI 24 g/10min ASTM D 1238
温度 265 °C -
荷重 5 kg -
機械的特性単位テスト基準
ISO データ
引張弾性率 7500 MPa ISO 527
降伏応力 80 MPa ISO 527
降伏ひずみ 2 % ISO 527
破壊応力 80 MPa ISO 527
破壊ひずみ 3 % ISO 527
曲げ弾性率 6400 MPa ISO 178
ノッチ付きシャルピー衝撃強さ, +23°C 4 kJ/m² ISO 179/1eA
Izod impact strength, +23°C, 4mm 30 kJ/m² ISO 180/1U
Izod impact strength, -30°C, 4mm 23 kJ/m² ISO 180/1U
ノッチ付きアイゾット衝撃強さ, +23°C, 4mm 6 kJ/m² ISO 180/1A
ノッチ付きアイゾット衝撃強さ, -30°C, 4mm 6 kJ/m² ISO 180/1A
ロックウェル硬度 R 98 - ISO 2039-2
Ball indentation hardness 128 MPa ISO 2039-1
ASTM数据
引張弾性率 7300 MPa ASTM D 638
降伏応力 80 MPa ASTM D 638
破壊応力 80 MPa ASTM D 638
降伏点伸び 2 % ASTM D 638
破断伸び 3 % ASTM D 638
曲げ弾性率 5800 MPa ASTM D 790
ノッチ付きIzod衝撃強さ, 1/8 in 50 J/m ASTM D 256
ノッチ付きIzod衝撃強さ, Low-Temperature 50 J/m ASTM D 256
温度 -30 °C -
アイゾット衝撃試験, 1/8 in 400 J/m ASTM D 256
熱的特性単位テスト基準
ISO データ
荷重たわみ温度, 1.80 MPa 200 °C ISO 75-1/-2
荷重たわみ温度, 0.45 MPa 220 °C ISO 75-1/-2
ビカット軟化温度, A 220 °C ISO 306
ビカット軟化温度, B 205 °C ISO 306
ビカット軟化温度, 120°C/h 50N 205 °C ISO 306
ASTM数据
DTUL @ 66 psi 220 °C ASTM D 648
DTUL @ 264 psi 200 °C ASTM D 648
ビカット軟化温度 205 °C ASTM D 1525
電気的特性.単位テスト基準
ISO データ
比誘電率, 1MHz 3.7 - IEC 62631-2-1
誘電正接, 1MHz 1500 E-4 IEC 62631-2-1
体積抵抗率 1E13 Ohm*m IEC 62631-3-1
表面抵抗率 >1E15 Ohm IEC 62631-3-2
耐電圧 28 kV/mm IEC 60243-1
ASTM数据
耐電圧, 短い時間 17 kV/mm ASTM D 149
誘電正接, 1 MHz 0.15 - ASTM D 150
比誘電率, 1 MHz 3.7 - ASTM D 150
体積抵抗率 1E15 Ohm*cm ASTM D 257
その他の特性.単位テスト基準
吸水率. 0.15 % Sim. to ISO 62
吸湿率 0.07 % Sim. to ISO 62
密度. 1450 kg/m³ ISO 1183
吸水率, 24hr 0.07 % ASTM D 570
密度 1450 kg/m³ ASTM D 792
Processing Recommendation Injection Molding単位テスト基準
Pre-drying - Temperature 110 - 120 °C -
Pre-drying - Time 2 - 4 h -
Processing humidity ≤0.02 % -
樹脂温度 245 - 260 °C -
金型温度 40 - 100 °C -
Feed temperature 40 - 60 °C -
Zone 1 230 - 240 °C -
Zone 2 235 - 250 °C -
Zone 3 240 - 260 °C -
特殊な特性
成形加工法.
射出成形.
添加剤.
難燃剤.
特殊な特性.
難燃.
耐薬品性
General Chemical Resistance
領域別の利用可能性
北アメリカ.
Disclaimer
Copyright Altair Engineering GmbH. Altair Engineering GmbH assumes no liability for the system to be free of errors. The user takes sole responsibility for the use of this data under the exclusion of every liability from Altair Engineering GmbH; this is especially valid for claims of compensation resulting from consequential damages. Altair explicitly points out that any decision about the application of materials must be double checked with the producer of this material. This includes all contents of this system. Copyright laws are applicable for the content of this system.
Created: Source: www.materialdatacenter.com


Material Data Center is provided by M-Base Engineering + Software GmbH. M-Base Engineering + Software GmbH assumes no liability for the system to be free of errors. Any decision about the application of materials must be double checked with the producer of this material.

Additional information about this material, like producer contact address, etc. can be found at www.materialdatacenter.com. For access to this extra information a registration is requested. Free online registration is available.