Complete Set of CAMPUS® Data, ASTM Data, Biopolymer Database, Application Database, Tradename Database, Literature Database, Toolbox.

Material datasheets available free. Online registration at: www.materialdatacenter.com

Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.

This is the free Material Data Center Datasheet of Sarlink® 5740DB - TPV - Teknor Apex Co.

Material Data Center offers the following functions for Sarlink® 5740DB:
unit conversion, PDF datasheet print, comparison with other plastics

Check here, which other Sarlink datasheets, application examples or technical articles are available in Material Data Center

Use the following short links to get directly to the properties of interest in this datasheet:
Any use of this information falls under the rules of our disclaimer.
商品の説明文

The Sarlink TPV 5700B series are highly engineered extrusion-grade thermoplastic vulcanizates with outstanding UV stability designed for demanding automotive interior and exterior sealing applications, including glass run channels, waistbelts, weather strips, seals and other profiles. Sarlink TPV X5740DB is a high hardness, medium density, high performance grade with low fogging and excellent color retention and elastic properties.



PropertyValueUnitStandard
Tensile properties (Cross Flow Direction)

ISO 37
   Tensile strength at break      19 MPa
   Modulus at 100% elongation        9 MPa
   Elongation at break    640 %
Hot air aging (168h/150°C, Cross Flow Direction)

ISO 188
   Change in hardness       3 points
   Change in tensile strength at break    -22 %
   Change in modulus at 100% elongation       5 %
   Change in elongation at break    -25 %
Hot air aging (1000h/135°C, Cross Flow Direction)

ISO 188
   Change in hardness       3 points
   Change in tensile strength at break    -20 %
   Change in modulus at 100% elongation       9
%
   Change in elongation at break    -25
%
Volume swell (70h/125°C in IRM 903 oil)     47 % ISO 1817
Apparent shear viscosity @ 206 1/s, 200°C   400 Pa.s ISO 11443 Capillary
機械的特性単位テスト基準
ISO データ
圧縮永久ひずみ 23℃, 24h 46 % ISO 815
圧縮永久ひずみ 70℃, 24h 58 % ISO 815
ショア硬さD 40 - ISO 7619-1
Other Standards[S]
伸び率100%時の応力 13.3 MPa ISO 37
破壊応力 TPE 18 MPa ISO 37
破壊ひずみ TPE 490 % ISO 37
S: These properties are reported by the producer according standards that are different to our defaults.
その他の特性.単位テスト基準
密度. 960 kg/m³ ISO 1183
特殊な特性
成形加工法.
射出成形., 異形押出成形., その他の押出成形., ブロー成形.
特殊な特性.
紫外線安定化., 熱安定化.
耐薬品性
General Chemical Resistance
アプリケーション
自動車
領域別の利用可能性
北アメリカ., ヨーロッパ., アジア/太平洋地域., 南・中央アメリカ.
Disclaimer
Copyright Altair Engineering GmbH. Altair Engineering GmbH assumes no liability for the system to be free of errors. The user takes sole responsibility for the use of this data under the exclusion of every liability from Altair Engineering GmbH; this is especially valid for claims of compensation resulting from consequential damages. Altair explicitly points out that any decision about the application of materials must be double checked with the producer of this material. This includes all contents of this system. Copyright laws are applicable for the content of this system.
Created: Source: www.materialdatacenter.com


Material Data Center is provided by M-Base Engineering + Software GmbH. M-Base Engineering + Software GmbH assumes no liability for the system to be free of errors. Any decision about the application of materials must be double checked with the producer of this material.

Additional information about this material, like producer contact address, etc. can be found at www.materialdatacenter.com. For access to this extra information a registration is requested. Free online registration is available.