Complete Set of CAMPUS® Data, ASTM Data, Biopolymer Database, Application Database, Tradename Database, Literature Database, Toolbox.

Material datasheets available free. Online registration at: www.materialdatacenter.com

Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.

This is the free Material Data Center Datasheet of TPE ProvaMed® 1060 - TPE - ACTEGA DS GmbH

Material Data Center offers the following functions for TPE ProvaMed® 1060:
unit conversion, PDF datasheet print, comparison with other plastics, application examples, CAE Interfaces

Check here, which other Provamed datasheets, application examples or technical articles are available in Material Data Center

Use the following short links to get directly to the properties of interest in this datasheet:
Any use of this information falls under the rules of our disclaimer.
Processing/Physical Characteristics単位テスト基準
ISO データ
メルトフローレート, MFI 8 g/10min ISO 1133
温度 230 °C -
荷重 2.16 kg -
機械的特性単位テスト基準
ISO データ
伸び率100%時の応力 1.7 MPa ISO 527
破壊ひずみ TPE >300 % ISO 527
圧縮永久ひずみ 23℃, 24h 18 % ISO 815
圧縮永久ひずみ 70℃, 24h 91 % ISO 815
ASTM数据
ショア硬さA 60 - ASTM D 2240
ショア硬さD 15 - ASTM D 2240
熱的特性単位テスト基準
ISO データ
溶融温度, 10゚C/min 162 °C ISO 11357-1/-3
ガラス転移点, 10゚C/min -40 °C ISO 11357-1/-2
その他の特性.単位テスト基準
密度. 890 kg/m³ ISO 1183
Processing Recommendation Injection Molding単位テスト基準
金型温度 20 - 60 °C -
Feed temperature 20 - 30 °C -
Zone 1 140 - 230 °C -
Nozzle temperature 190 - 230 °C -
特殊な特性
成形加工法.
射出成形., その他の押出成形.
納入形状.
ペレット.
特殊な特性.
透明., 滅菌可能, エチレンオキシド滅菌(EtO), 蒸気滅菌, Gamma irradiation sterilization
耐薬品性
Oxidation Resistance, Radiation Resistance
Certifications
Medical Grade, Biocompatibility ISO 10993
アプリケーション
医療の
領域別の利用可能性
北アメリカ., ヨーロッパ., アジア/太平洋地域., 南・中央アメリカ., 近東/アフリカ
Disclaimer
Copyright Altair Engineering GmbH. Altair Engineering GmbH assumes no liability for the system to be free of errors. The user takes sole responsibility for the use of this data under the exclusion of every liability from Altair Engineering GmbH; this is especially valid for claims of compensation resulting from consequential damages. Altair explicitly points out that any decision about the application of materials must be double checked with the producer of this material. This includes all contents of this system. Copyright laws are applicable for the content of this system.
Created: Source: www.materialdatacenter.com


Material Data Center is provided by M-Base Engineering + Software GmbH. M-Base Engineering + Software GmbH assumes no liability for the system to be free of errors. Any decision about the application of materials must be double checked with the producer of this material.

Additional information about this material, like producer contact address, etc. can be found at www.materialdatacenter.com. For access to this extra information a registration is requested. Free online registration is available.