Complete Set of CAMPUS® Data, ASTM Data, Biopolymer Database, Application Database, Tradename Database, Literature Database, Toolbox.

Material datasheets available free. Online registration at: www.materialdatacenter.com

Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.

This is the free Material Data Center Datasheet of Panlite® L-1250Z 100 - PC - Teijin Chemicals Ltd.

Material Data Center offers the following functions for Panlite® L-1250Z 100:
unit conversion, PDF datasheet print, comparison with other plastics, snap fit calculation, beam deflection calculation, CAE Interfaces

Check here, which other Panlite datasheets, application examples or technical articles are available in Material Data Center

Use the following short links to get directly to the properties of interest in this datasheet:
Any use of this information falls under the rules of our disclaimer.
Processing/Physical Characteristics単位テスト基準
ISO データ
メルトボリュームレイト, MVR 8 cm³/10min ISO 1133
温度 300 °C -
荷重 1.2 kg -
ASTM数据
成形収縮率., 平行 0.006 mm/mm ASTM D 955
成形収縮率, 直角 0.006 mm/mm ASTM D 955
機械的特性単位テスト基準
ISO データ
引張弾性率 2400 MPa ISO 527
降伏応力 61 MPa ISO 527
降伏ひずみ 6 % ISO 527
破壊呼びひずみ >50 % ISO 527
曲げ弾性率, 23°C 2350 MPa ISO 178
曲げ強さ 93 MPa ISO 178
シャルピー衝撃強さ, +23°C N kJ/m² ISO 179/1eU
ノッチ付きシャルピー衝撃強さ, +23°C 76 kJ/m² ISO 179/1eA
ASTM数据
引張弾性率 2120 MPa ASTM D 638
降伏応力 62 MPa ASTM D 638
破壊応力 80 MPa ASTM D 638
降伏点伸び 6 % ASTM D 638
破断伸び 140 % ASTM D 638
圧縮強度 76 MPa ASTM D 695
曲げ弾性率 2230 MPa ASTM D 790
曲げ強さ 92 MPa ASTM D 790
ロックウェル硬度 M 77 - ASTM D 785
ノッチ付きIzod衝撃強さ, 1/8 in 880 J/m ASTM D 256
ノッチ付きIzod衝撃強さ, 1/4 in 140 J/m ASTM D 256
熱的特性単位テスト基準
ISO データ
荷重たわみ温度, 1.80 MPa 129 °C ISO 75-1/-2
荷重たわみ温度, 0.45 MPa 142 °C ISO 75-1/-2
ビカット軟化温度, B 149 °C ISO 306
線膨張係数, 平行 70 E-6/K ISO 11359-1/-2
線膨張係数, 直角 70 E-6/K ISO 11359-1/-2
1.5mm厚さでの燃焼性 HB class IEC 60695-11-10
試験片の厚さ 1.5 mm -
厚さhでの燃焼性 V-2 class IEC 60695-11-10
試験片の厚さ 0.4 mm -
グローワイヤ燃焼性指数 (GWFI) 825 °C IEC 60695-2-12
GWFI - 試験片の厚さ 1.5 mm -
グローワイヤ燃焼性指数 (GWFI) 875 °C IEC 60695-2-12
GWFI - 試験片の厚さ 3 mm -
グローワイヤ着火温度 (GWIT) 850 °C IEC 60695-2-13
GWIT - 試験片の厚さ 1.5 mm -
グローワイヤ着火温度 (GWIT) 850 °C IEC 60695-2-13
GWIT - 試験片の厚さ 3 mm -
ASTM数据
線膨張係数, 平行 70 E-6/K ASTM D 696
線膨張係数, 直角 70 E-6/K ASTM D 696
電気的特性.単位テスト基準
ISO データ
比誘電率, 100Hz 3.1 - IEC 62631-2-1
比誘電率, 1MHz 3 - IEC 62631-2-1
誘電正接, 100Hz 10 E-4 IEC 62631-2-1
誘電正接, 1MHz 90 E-4 IEC 62631-2-1
体積抵抗率 >1E13 Ohm*m IEC 62631-3-1
表面抵抗率 >1E15 Ohm IEC 62631-3-2
耐電圧 30 kV/mm IEC 60243-1
耐トラッキング性 250 - IEC 60112
ASTM数据
耐電圧, 短い時間 30 kV/mm ASTM D 149
誘電正接, 60 Hz 0.0004 - ASTM D 150
誘電正接, 1 MHz 0.009 - ASTM D 150
比誘電率, 60 Hz 2.95 - ASTM D 150
比誘電率, 1 MHz 2.9 - ASTM D 150
体積抵抗率 3E16 Ohm*cm ASTM D 257
耐アーク 100 s ASTM D 495
光学特性単位テスト基準
ASTM数据
視感透過率 88 % ASTM D 1003
くっせつりつ 1.58 - ASTM D 542
その他の特性.単位テスト基準
密度. 1200 kg/m³ ISO 1183
吸水率, 平衡 0.2 % ASTM D 570
Processing Recommendation Injection Molding単位テスト基準
Pre-drying - Temperature 120 °C -
Pre-drying - Time >5 h -
樹脂温度 270 - 320 °C -
金型温度 80 - 120 °C -
特殊な特性
成形加工法.
射出成形.
納入形状.
ペレット.
添加剤.
離型剤.
特殊な特性.
紫外線安定化., 透明.
アプリケーション
自動車, 汎用
領域別の利用可能性
北アメリカ., ヨーロッパ., アジア/太平洋地域., 南・中央アメリカ., 近東/アフリカ
Disclaimer
Copyright Altair Engineering GmbH. Altair Engineering GmbH assumes no liability for the system to be free of errors. The user takes sole responsibility for the use of this data under the exclusion of every liability from Altair Engineering GmbH; this is especially valid for claims of compensation resulting from consequential damages. Altair explicitly points out that any decision about the application of materials must be double checked with the producer of this material. This includes all contents of this system. Copyright laws are applicable for the content of this system.
Created: Source: www.materialdatacenter.com


Material Data Center is provided by M-Base Engineering + Software GmbH. M-Base Engineering + Software GmbH assumes no liability for the system to be free of errors. Any decision about the application of materials must be double checked with the producer of this material.

Additional information about this material, like producer contact address, etc. can be found at www.materialdatacenter.com. For access to this extra information a registration is requested. Free online registration is available.