Complete Set of CAMPUS® Data, ASTM Data, Biopolymer Database, Application Database, Tradename Database, Literature Database, Toolbox.

Material datasheets available free. Online registration at: www.materialdatacenter.com

Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.

This is the free Material Data Center Datasheet of NORYL GTX™ Resin GTX674PC - Americas - (PPE+PA*) - Saudi Basic Industries Corporation (SABIC)

Material Data Center offers the following functions for NORYL GTX™ Resin GTX674PC - Americas:
unit conversion, PDF datasheet print, comparison with other plastics, snap fit calculation, beam deflection calculation, cooling time calculation, parameters for material models, CAE Interfaces

Check here, which other Noryl datasheets, application examples or technical articles are available in Material Data Center

Use the following short links to get directly to the properties of interest in this datasheet:
Any use of this information falls under the rules of our disclaimer.
商品の説明文
NORYL GTX™ 674PC resin is a conductive, non-reinforced alloy of Polyphenylene Ether (PPE) + Polyamide (PA). This injection moldable grade is optimized to allow for in- or on-line primer-less powder coat painting around corners and holes with a Class A Surface. NORYL GTX674PC resin exhibits high heat resistance, improved surface appearance and is an excellent candidate for automotive applications such as mirror housings and brackets. This material is only available in black.

UL Yellow Card Link E121562-549484
Processing/Physical Characteristics単位テスト基準
ISO データ
溶融時の密度 967 kg/m³ -
溶融時の熱伝導率 0.19 W/(m K) -
溶融時の比熱 3760 J/(kg K) -
突き出し時の時の温度 156 °C -
ASTM数据
メルトフローレイト, MFI 25 g/10min ASTM D 1238
温度 300 °C -
荷重 5 kg -
機械的特性単位テスト基準
ISO データ
引張弾性率 2320 MPa ISO 527
降伏ひずみ 3 % ISO 527
破壊応力 60 MPa ISO 527
破壊ひずみ 4 % ISO 527
曲げ弾性率 2480 MPa ISO 178
ASTM数据
引張弾性率 2810 MPa ASTM D 638
降伏応力 65 MPa ASTM D 638
破壊応力 64 MPa ASTM D 638
降伏点伸び 3 % ASTM D 638
破断伸び 4 % ASTM D 638
曲げ弾性率 2890 MPa ASTM D 790
ノッチ付きIzod衝撃強さ, 1/8 in 74 J/m ASTM D 256
ノッチ付きIzod衝撃強さ, Low-Temperature 50 J/m ASTM D 256
温度 -30 °C -
熱的特性単位テスト基準
ISO データ
荷重たわみ温度, 0.45 MPa 185 °C ISO 75-1/-2
ビカット軟化温度, B 197 °C ISO 306
ビカット軟化温度, 120°C/h 50N 196 °C ISO 306
線膨張係数, 平行 122 E-6/K ISO 11359-1/-2
線膨張係数, 直角 134 E-6/K ISO 11359-1/-2
1.5mm厚さでの燃焼性 HB class IEC 60695-11-10
試験片の厚さ 1.5 mm -
ASTM数据
DTUL @ 66 psi 188 °C ASTM D 648
ビカット軟化温度 197 °C ASTM D 1525
その他の特性.単位テスト基準
密度. 1110 kg/m³ ISO 1183
密度 1110 kg/m³ ASTM D 792
Processing Recommendation Injection Molding単位テスト基準
Pre-drying - Temperature 95 - 105 °C -
Pre-drying - Time 3 - 4 h -
Processing humidity ≤0.07 % -
樹脂温度 280 - 305 °C -
金型温度 75 - 120 °C -
Zone 1 265 - 305 °C -
Zone 2 270 - 305 °C -
Zone 3 275 - 305 °C -
Screw speed 20 - 100 rpm -
Back pressure 0.3 - 1.4 MPa -
機能
 粘度せん断速度. , NORYL GTX™  Resin GTX674PC - Americas, (PPE+PA*), SABIC
 せん断応力-せん断速度. , NORYL GTX™  Resin GTX674PC - Americas, (PPE+PA*), SABIC
 pvT , NORYL GTX™  Resin GTX674PC - Americas, (PPE+PA*), SABIC
特殊な特性
成形加工法.
射出成形.
領域別の利用可能性
北アメリカ.
Disclaimer
Copyright Altair Engineering GmbH. Altair Engineering GmbH assumes no liability for the system to be free of errors. The user takes sole responsibility for the use of this data under the exclusion of every liability from Altair Engineering GmbH; this is especially valid for claims of compensation resulting from consequential damages. Altair explicitly points out that any decision about the application of materials must be double checked with the producer of this material. This includes all contents of this system. Copyright laws are applicable for the content of this system.
Created: Source: www.materialdatacenter.com


Material Data Center is provided by M-Base Engineering + Software GmbH. M-Base Engineering + Software GmbH assumes no liability for the system to be free of errors. Any decision about the application of materials must be double checked with the producer of this material.

Additional information about this material, like producer contact address, etc. can be found at www.materialdatacenter.com. For access to this extra information a registration is requested. Free online registration is available.